BATTERIES, FUEL CELLS, AND ENERGY CONVERSION
A493
G. A. Roberts, E. J. Cairns and J. A. Reimer
A497
Shanwen Tao and John T. S. Irvine
Electrochemical current-potential and impedance measurement techniques have been applied to a ceramic anode based on the mixed electronic and oxide ion conductor
(ScYZT). Significantly better performance is obtained with this anode using a platinum current collector than for platinum on its own or platinum applied to a porous yttria-stabilized zirconia interlayer. Indeed the polarization resistance of ScYZT is 5.66 Ω cm2 at open circuit-voltage at 900°C in wet 5%
which is ten times lower than for platinum under the same conditions. Impedance spectroscopic measurements show a number of phenomena attributed to a combination of the electronic resistance through the anode, the oxide ionic current exchange between anode and electrolyte, and noncharge chemical processes at the anode. It was found that interface and chemical impedances change with changes in the electronic conductivity of ScYZT when different bias potentials are applied, although the overall chemical impedance was not observed to change significantly. These measurements suggest that ScYZT is a promising anode material for use with an appropriate current collector. © 2004 The Electrochemical Society. All rights reserved.
A504
Yucheng Sun, Chuying Ouyang, Zhaoxiang Wang, Xuejie Huang and Liquan Chen
A509
Karen E. Thomas-Alyea, John Newman, Guoying Chen and Thomas J. Richardson
A continuum-scale model is presented to explain how electroactive polymers such as polythiophene can be used to provide overcharge protection for lithium-ion batteries. The model shows how the cell is transformed upon overcharge from a battery to a resistor with a resistivity that varies with position across the separator. Upon discharge or open circuit, self discharge transforms the resistor back into a battery, and normal cycling can be resumed. A simplified model yields a design equation that shows how the potential at which the cell shorts depends on the current density, separator thickness, and the variation of the electronic conductivity and the oxidation potential of the polymer with a degree of oxidation. The effect of these parameters on the transient and steady-state behavior of the short is explored. The shorting voltage is independent of the choice of positive electrode and scales with the potential of the charged negative electrode. Kinetic effects on the transient behavior and thermal effects are also considered. © 2004 The Electrochemical Society. All rights reserved.
A522
Robert Kostecki, Laura Norin, Xiangyun Song and Frank McLarnon
The decrease of ionic conductivity of polymeric separators in high-power Li-ion cells, which were cycled or stored at elevated temperatures, was accompanied by dramatic changes in separator surface morphology. The source and nature of polymer separator degradation in high-power Li-ion batteries have been studied. We attributed the observed porosity loss to a deposit, which precipitated onto the separator surface from the electrolyte and clogged separator pores. This deposit resulted from a homogenous decomposition process of the
-ethylene carbonate-ethyl-methyl carbonate electrolyte, which was significantly accelerated at elevated temperatures. The electrolyte decomposition products consisted of lithium halophosphates and displayed very strong fluorescence. They contributed to the solid electrolyte interphase layers on both cathode and anode where they underwent further oxidation or reduction reactions, respectively. © 2004 The Electrochemical Society. All rights reserved.
A527
Hiroyasu Furukawa, Mitsuhiro Hibino and Itaru Honma
Amorphous titanium oxide was prepared by a sol-gel route employing Ti(IV) alkoxide as a starting agent. The average size of the primary particles was about 4 nm, and the Brunauer-Emmett-Teller specific surface area was 390 m2 g−1. Addition of acetylene black in synthesis allowed us to obtain the composite of titania and carbon materials. The composite materials could be galvanostaticly discharged and charged around 2 V vs.
After thermal treatment at 330°C the composite showed specific capacity above 125 mA h g−1, even under large discharge current of 10 A g−1. Based on the relationship between specific capacity and current density, the chemical diffusion coefficient of lithium was estimated to be
© 2004 The Electrochemical Society. All rights reserved.
A532
K. Honda, M. Yoshimura, K. Kawakita, A. Fujishima, Y. Sakamoto, K. Yasui, N. Nishio and H. Masuda
A542
H. H. Lee, C. C. Wan and Y. Y. Wang
A548
Pei-Wen Li and Kenjiro Suzuki
A quasi-2D model was proposed and made available for numerical studies on the performance of a single tubular solid oxide fuel cell (SOFC) under practical operating conditions. The model takes account of the air and fuel flow velocity fields, ohmic and thermodynamic heat generation, convective heat-transfer, mass transfer of participating chemical species including the electrochemical processes, and the electric potential and electric current in the electrodes and electrolyte. Numerical computation was carried out to test the proposed model for a single unit cell having a specific geometry being operated at a few different thermal and composition conditions for the inlet fuel and air flows. Obtained numerical results show that the quasi-two-dimensional approximation adopted in the model to mitigate the computational cost effectively can work reasonably well. At low electric current density, the cell terminal voltage was overpredicted. In order to improve the model on this point, the simple treatment adopted for the activation and concentration polarization in the model must be replaced by a more sophisticated approach in future studies. Discussions were further given concerning the obtained results for the overall cell performance and the detailed features of the velocity, thermal, and mass-transfer fields in the cell in addition to the local electrochemical characteristics. It is suggested that the air flow convective heat-transfer is important as a cooling means and that overpotential due to concentration polarization is more serious for the cathode side than for the anode side. All the presented results including the electricity conversion efficiency were observed to agree reasonably well with the popularly accepted cell performance. © 2004 The Electrochemical Society. All rights reserved.
A558
D. Bahadur, N. Lahl, K. Singh, L. Singheiser and K. Hilpert
A563
Yong Wang, Jim Yang Lee and Bing-Hung Chen
A571
Jong H. Jang and Seung M. Oh
A new analytical methodology, complex capacitance analysis, is developed for porous carbons that are employed as electric double-layer capacitor (EDLC) electrodes. Based on the transmission line model, the imaginary capacitance profiles
vs.
are theoretically derived for a cylindrical pore and further extended to multiple pore systems. The theoretical derivation illustrates that two important electrochemical parameters in EDLCs can be estimated from the peak-shaped imaginary capacitance plots: total capacitance from the peak area and rate capability from the peak position. The usefulness of this analysis in estimating EDLC parameters is demonstrated by applying to two sets of practical porous carbon electrodes. In addition, the penetrability distribution curves that are derived from the experimental imaginary capacitance data using the log-normal assumption and discrete Fourier transform allow us to estimate the pore structure of carbon electrodes. © 2004 The Electrochemical Society. All rights reserved.
A578
S. Passerini, M. Lisi, T. Momma, H. Ito, T. Shimizu and T. Osaka
In this work, the co-continuous polymer blend was synthesized for use as the electrolyte in lithium batteries. Such electrolytes were characterized by a co-continuous morphology consisting of two three-dimensionally interpenetrated polymer networks simply formed by hot-mixing two nonmiscible polymers. A preliminary electrochemical characterization of the gelified co-continuous polymer blend as electrolyte for lithium batteries is also reported. © 2004 The Electrochemical Society. All rights reserved.
A583
Jingtian Yin, Masashi Wada, Shigeo Tanase and Tetsuo Sakai
A590
Calvin J. Curtis, Jiaxiong Wang and Douglas L. Schulz
A599
Z. R. Zhang, H. S. Liu, Z. L. Gong and Y. Yang
The electrochemical behaviors of native and
-coated
electrodes which were cycled in different potential regions (i.e., 3.0-4.3 and 3.0-4.6 V) were investigated by the powder microelectrode technique. The surface species on the electrodes were also studied by Fourier transform infrared and temperature-programmed desorption-mass spectroscopy (TPD-MS) techniques. Different oxidation products were formed on the bare and coated electrodes, respectively. The results indicated that the improved cyclic stability of the coated electrodes may be attributed to formation of different surface oxide films through an electro-oxidation mechanism of the solvents on the electrodes. A possible electro-oxidation mechanism has been proposed based on the results. © 2004 The Electrochemical Society. All rights reserved.
A604
Steven McIntosh, Hongpeng He, Shung-Ik Lee, Olga Costa-Nunes, Venkatesan V. Krishnan, John M. Vohs and Raymond J. Gorte
The deposition, stability, and function of carbonaceous films formed by exposing porous yttria-stabilized zirconia (YSZ) anodes in YSZ-based solid oxide fuel cells (SOFCs) to n-butane at elevated temperatures was studied using a combination of four-probe conductivity, impedance spectroscopy, and cell polarization measurements. The carbonaceous deposits were found to have high electronic conductivity and to be relatively stable for steam-to-carbon ratios as high as 3.75. Comparison of the performance of cells in which carbon films were used as the sole current collector in the anode with anodes containing both Cu and carbon films indicated that in the latter case, the carbon layer plays an important role in providing electronic conductivity near the three-phase boundary. © 2004 The Electrochemical Society. All rights reserved.
A609
Junwei Jiang, Hubert Fortier, J. N. Reimers and J. R. Dahn
A614
Thierry Brousse, Mathieu Toupin and Daniel Bélanger
A623
Yongchao Si, H. Russell Kunz and James M. Fenton
A632
Wu Xu, Alan J. Shusterman, Robert Marzke and C. Austen Angell
Synthesis, characterization, ionic conductivity, electrochemical stability, and lithium-ion transport number of an asymmetric version of the successful orthoborate lithium salt lithium bis(oxalato)borate (LiBOB), are described. The salt, lithium (malonato oxalato) borate (LiMOB), is thermally stable up to 273°C. It is poorly soluble in common organic solvents such as 1,2-dimethoxyethane, tetrahydrofuran, acetonitrile, dimethyl carbonate, and propylene carbonate, but has moderate solubility in γ-butyrolactone (GBL) and N,N-dimethylformamide (DMF), and high solubility in dimethyl sulfoxide (DMSO). The 0.5 M solutions of LiMOB in GBL, DMSO, and DMF show high conductivities 


and 
at 25°C, respectively) relative to most 0.5 M nonaqueous solutions. Even the room temperature conductivity of the 0.08 M LiMOB-PC solution is close to 
The conductivities of LiMOB solutions are close to those of LiBOB solutions, which has been demonstrated in recent studies to be a successful substitute for
in lithium-ion batteries. The cyclic voltammograms show that LiMOB solutions in PC and GBL have electrochemical stability as high as 4.3 V vs.
The lithium-ion transport number at room temperature for 0.5 M LiMOB in
was 0.36, obtained from self-diffusivity measurement by the pulsed field gradient spin echo nuclear magnetic resonance technique. The highest occupied molecular orbital energy, which is usually correlated with electrochemical stability has been calculated, and electrostatic potential maps for the new anion and its fluorinated derivatives are presented. They suggest that the fluorinated analogue of LiMOB should be more stable and more soluble, and may have unique properties. © 2004 The Electrochemical Society. All rights reserved.
A639
Kunchan Lee, Akimitsu Ishihara, Shigenori Mitsushima, Nobuyuki Kamiya and Ken-ichiro Ota
We have investigated the effect of the recast temperature, i.e., heat-treatment of a polymer electrolyte, on the diffusion coefficient and solubility of oxygen in the electrolyte and also on the morphological properties of recast ion-exchange membranes for improving the cathode activity in polymer electrolyte fuel cells. Based on chronoamperometric measurements, the diffusion coefficient and solubility of oxygen were found to be deeply affected by the recast temperature. The diffusion coefficient increased with the decreasing recast temperature, while the solubility had the opposite tendency. The water uptakes and ionic cluster size also varied with the recast temperature. Based on the X-ray measurements, it is considered that the differences in the mass transport parameters, the cluster sizes, and water uptakes are due to the growth of the clusters and the crystallinity in the electrolyte. © 2004 The Electrochemical Society. All rights reserved.
A646
Yingyi Huang, John M. Vohs and Raymond J. Gorte
A652
B. V. Ratnakumar, M. C. Smart, L. D. Whitcanack, E. D. Davies, K. B. Chin, F. Deligiannis and S. Surampudi
Planetary exploration missions to Jupiter and its moons require that the power system components, including batteries, be tolerant to high intensities, about 4 Mrad, of γ-radiation. In view of the several polymeric materials used as separators and binders and the use of organic electrolyte solutions in Li-ion cells, it is difficult to predict their response to such radiation environments. Therefore, a detailed experimental evaluation was undertaken to determine the performance of Li-ion cells after exposure to various levels of cumulative radiation levels up to 25 Mrad, at different levels of intensities. Prototype cells, obtained from two domestic sources for aerospace lithium-ion batteries and consisting of two different chemistries, were used as test articles. Discharge performances, at ambient and low temperatures, as well as, electrical impedance spectroscopy responses were determined after each exposure, and analyses were made for the impedance characteristics and their changes upon irradiation. Postradiation cycling tests were carried out on these cells to assess their cyclability subsequent to radiation exposure. Although control measurements were not made on cells without radiation, these studies reveal that the lithium-ion cells display good tolerance to radiation, with only marginal decline in their capacity, and with no significant change in capacity fade rate during subsequent cycling. © 2004 The Electrochemical Society. All rights reserved.
CORROSION, PASSIVATION, AND ANODIC FILMS
B207
E. Cano, E. M. Mora, H. Azcaray and J. M. Bastidas
Copper corrosion initiated by butyric acid vapors
ranging from 0.1 to 100 ppm at 100% relative humidity was studied. The copper corrosion rate at 0.1 and 100 ppm pollutant levels was 8.5 and 630 mg m−2 d−2, respectively. Corrosion products were characterized using X-ray diffraction and X-ray photoelectron spectroscopy analyses and their morphology was observed by scanning electron microscopy (SEM). The main compounds identified were cuprite and a copper butyrate compound. The amount of cuprite decreased as the pollution level increased. Copper butyrate was observed from the lowest concentrations, and its amount increased with the butyric acid vapor concentration. The patina formed was very porous and provided little protection to the underlying copper. © 2004 The Electrochemical Society. All rights reserved.
B214
Xueming Chen and Guohua Chen
B220
W. S. Li, S. Q. Cai and J. L. Luo
B227
Renchun Huang, Kurt R. Hebert, Thomas Gessmann and Kelvin G. Lynn
The effect of impurities on formation of interfacial metallic voids, during uniform dissolution of aluminum in 1 M NaOH, was investigated. These voids are thought to act as initiation sites for pitting corrosion, and were previously shown to be formed by NaOH dissolution. Samples of three different bulk purities were compared: 99.98, 99.997, and 99.9995%. Positron annihilation spectroscopy and atomic force microscopy revealed that nanometer-scale voids were formed by dissolution in each foil. For each sample, the void volume fraction interpreted from these measurements increased to a maximum during dissolution, and then declined. As the purity increased, more extensive dissolution was required to produce voids. Accumulation of near-surface Cu and Fe impurities during dissolution was characterized using Rutherford backscattering spectrometry. The results suggested a possible general correlation of void volume fraction with copper surface concentration. Processes involving near-surface copper impurities may then at least partly control the formation of voids. © 2004 The Electrochemical Society. All rights reserved.
B233
N. D. Budiansky, J. L. Hudson and J. R. Scully
The origins of persistent interactions among localized corrosion sites were investigated using multielectrode arrays (MEA). MEAs consisted of one hundred 250 μm diam AISI 316 stainless steel wires configured into
close-packed rectangle and
far-spaced configurations. Experiments were conducted in dilute chloride solutions and elevated temperatures to accentuate interactions. Interactions between early dominating pits and the adjacent electrode surface were found to develop as regions of enhanced or suppressed pitting susceptibility triggered by concentration and potential fields developed during growth of large pits, respectively. Transient aggressive species accumulation around active pits was also found to cause “surface damage” to electrodes that persisted for long periods after primary pits were repassivated and solutions extensively stirred. Oxide film alteration, mixed metal sulfide inclusion damage, and surface contamination were all considered to be possible origins of persistent interactions. Mn(Fe,Cr)S inclusions were implicated to be the origin of such persistent interactions. Persistent interactions were completely suppressed by nitric acid treatment, which is believed to remove or modify susceptible Mn(Fe,Cr)S inclusions. © 2004 The Electrochemical Society. All rights reserved.
ELECTROCHEMICAL/CHEMICAL DEPOSITION AND ETCHING
C229
B. Vuillemin, R. Oltra, H. Perrot, C. Sauvage and O. Néel
The ability of the channel flow double electrode (CFDE) technique and electrochemical quartz crystal microbalance (EQCM) for studying in situ chromate phosphate conversion coating on 5182 aluminum alloys was explored. It was first demonstrated that aqueous Cr(VI) can be analyzed quantitatively with the CFDE technique by reduction into Cr(III) on a graphite electrode. Samples used for EQCM were quartz plated by physical vapor deposition using a 5182 alloy target, allowing thin layers of aluminum alloys with a similar chemical composition to be obtained. EQCM was adapted in order to account for the hydrodynamic conditions in an industrial process, by placing the quartz in a flow cell. In order to be able to control, and then study, the early stage of the coating, the aluminum electrode used for the CFDE technique was covered with a mask (a thin layer of varnish) that was removed in situ by a laser pulse. With EQCM the triggering of the coating was performed by injecting the required amount of hydrofluoric acid. Since the time duration of the transient responses was different in both techniques, we focused our discussion on the steady state. Measurements of the electroacoustic impedance of the aluminum-alloy-coated quartz in the conversion solution showed that the chromate phosphate film can be considered as acoustically thin, allowing the use of the Sauerbrey’s equation to calculate mass variations. Combining in the steady state the rate of mass variation measured by EQCM, and the rate of Cr(VI) reduction by CFDE as functions of the bath composition, it was possible to calculate a chemical yield for the film growth. The results in agreement with the literature indicate strong synergetic effect between chemical species present in the solution. © 2004 The Electrochemical Society. All rights reserved.
C236
Stéphanie de Persis, Francis Teyssandier, Dominique Thévenin and Nasser Darabiha
The intrinsic low dimensional manifold method (ILDM), which is a reduction method of large gaseous chemical systems, is applied to the gas-phase chemistry used to deposit 4H or 6H silicon carbide (SiC). The 1-dimensional (1-D) manifold corresponding to the relaxation of all the fast reaction modes of the complex gaseous chemical system is calculated and represented according to different projections in the state space. The ILDM method is also used to compare trajectories corresponding to various initial gas-phase compositions. These initial gas-phase mixtures, which include different carbon precursors, all converge towards the same thermodynamic equilibrium. Long before thermodynamic equilibrium is reached, the trajectories are attracted by the 1-D manifold. © 2004 The Electrochemical Society. All rights reserved.
C245
Sophie Pagani Lakard, Guillaume Herlem, Boris Lakard, Michel Herlem, Tijani Gharbi and Bernard Fahys
C250
Kazuo Kondo, Toshiaki Matsumoto and Keiji Watanabe
C256
W. R. A. Meuleman, S. Roy, L. Péter and I. Bakonyi
In a previous paper [W. R. A. Meuleman, S. Roy, L. Peter, and I. Varga, J. Electrochem. Soc., 149, C479 (2002)], the electrodeposition of Ni(Cu)/Cu multilayers from a citrate electrolyte has been discussed. In the present work, an X-ray diffraction (XRD) study and the magnetoresistance characteristics of the same multilayers are described. For Cu layer thicknesses above about 2 nm, satellite reflections due to multilayer periodicity could be observed. The grain sizes as deduced from the broadening of the XRD lines were between 10 and 15 nm. A clear giant magnetoresistance (GMR) behavior was observed at Cu thicknesses above 2 nm for the constant current/constant potential series where galvanostatic and potentiostatic control was used for the deposition of the magnetic and nonmagnetic layer, respectively. However, the maximum GMR at 8 kOe was around −0.3% only. For the constant current/relaxation/constant current series in which both layers were deposited under galvanostatic control with a zero current interval in between, only a very weak indication for the GMR contribution could be detected besides the dominating anisotropic magnetoresistance. Interface intermixing due to the Ni vs. Cu exchange reaction, electrolyte pH, (111) orientation of the deposit, and very small crystallite sizes have been considered as possible sources leading to the poor GMR. © 2004 The Electrochemical Society. All rights reserved.
C262
T. P. Moffat, D. Wheeler and D. Josell
C272
Soo-Hyun Kim, Su Suk Oh, Hyun-Mi Kim, Dae-Hwan Kang, Ki-Bum Kim, Wei-Min Li, Suvi Haukka and Marko Tuominen
The properties of
films deposited by atomic layer deposition (ALD) using 
and triethyl boron were characterized as diffusion barriers for copper metallization. The films deposited at 313°C showed resistivity of about 350 μΩ cm with a density of
The film composition measured by Rutherford backscattering spectrometry showed W, C, and N of approximately 48, 32, and 20 atom %, respectively. Transmission electron microscopy analyses showed that the as-deposited film was composed of a face-centered-cubic phase with a lattice parameter similar to both
and
with an equiaxed microstructure. The film kept its nanocrystalline microstructure until annealing at 700°C, although some amount of simple hexagonal α-WC was identified to be formed and the
phase disappeared. As the annealing temperature increased to 800°C, relatively larger grains of body-centered-cubic W were newly formed with smaller grains of hexagonal-close-packed
or α-WC. All the phenomena are related to nitrogen release after annealing at 700 and 800°C. The results of diffusion barrier performance between Cu and Si analyzed by X-ray diffractometry showed that
film (12 nm) failed only after annealing at 700°C for 30 min by the formation of copper silicide, while the sputter-deposited Ta (12 nm) and ALD-TiN (20 nm) films failed at 650 and 600°C annealing, respectively. It is thought that the superior diffusion barrier performance of
film is the consequence of both the formation of equiaxed microstructure and the high-density nature of the film. © 2004 The Electrochemical Society. All rights reserved.
ELECTROCHEMICAL SYNTHESIS AND ENGINEERING
D31
Dun Zhang, Takeyoshi Okajima, Futoshi Matsumoto and Takeo Ohsaka
The electrode reaction of the molecular oxygen
ion
redox couple at glassy carbon (GC), gold (Au), and platinum (Pt) electrodes in three 1-n-alkyl-3-methylimidazolium tetrafluoroborate
room-temperature ionic liquids (RTILs), 1-ethyl-3-methylimidazolium tetrafluoroborate, 1-n-propyl-3-methylimidazolium tetrafluoroborate, and 1-n-butyl-3-methylimidazolium tetrafluoroborate, has been analyzed quantitatively using cyclic voltammetry, normal pulse voltammetry, and hydrodynamic chronocoulometry (HCC). Cyclic voltammetric measurements showed that the redox reaction of the
couple in these RTILs is a quasi-reversible process and that the resulting
is stable. The relevant thermodynamic and kinetic parameters [the formal potential
the standard rate constant
and the cathodic transfer coefficient
of the
redox couple were evaluated using cyclic and normal pulse voltammetry: (i) the
values are almost the same irrespective of the media and electrode materials examined, i.e., ca. −1.0 V vs. an internal standard potential of the ferrocene (Fc)/ferricinium ion
redox couple, (ii) the
value is dependent on the electrode material and increases in the order
and (iii) the values of
are in the range of 0.35-0.47. The diffusion coefficients
and saturated concentrations
of
in three
RTILs were also determined by HCC. © 2004 The Electrochemical Society. All rights reserved.
PHYSICAL AND ANALYTICAL ELECTROCHEMISTRY
E119
Tomas Johansson, Nils-Krister Persson and Olle Inganäs
The propagation speed of the front of electrochemical conversion, from semiconductor to highly doped polymer, in films of regioregular poly(3-hexylthiophene) spin cast on insulating substrates was analyzed. Propagation of the p-doped zone in polymer electrochromic devices was imaged simultaneously with recording of electrochemical data. The current is proportional to the propagation speed and has a Tafel-like behavior when taking the resistive drop in the film into account. The resistivity in the film, which gradually lowers the propagation speed, was used for determination of the conductivity of the p-doped polymer. By combining these values with the doping charge injected into the film during front migration we estimated the hole carrier mobility for different doping levels. © 2004 The Electrochemical Society. All rights reserved.
E125
K. H. Kangasniemi, D. A. Condit and T. D. Jarvi
Electrochemical surface oxidation of Vulcan XC-72, a carbon black commonly used in proton exchange membrane (PEM) fuel cells, was studied following potentiostatic treatments up to 120 h at potentials from 0.6 to 1.2 V at room temperature and 65°C. Surface oxidation was followed using cyclic voltammetry (CV), thermal gravimetric analysis coupled to on-line mass spectrometry (TGA-MS), X-ray photoelectron spectroscopy (XPS), and contact angle measurements. The analytical techniques all indicate significant surface oxidation occurred during the first 16 h of 1.2 V potential holds at room temperature and a slow increase in surface oxide formation thereafter. An identification of ether, carbonyl, and carboxyl surface oxide species was made by deconvolution of XPS spectra and assigning these functional groups to the observed TGA-MS
evolution peaks (150-750°C). An increase in CO evolution (>800°C) determined by TGA-MS was consistent with electrochemical CV data, which detected electroactive hydroquinone/quinone species; these electrochemically detected species were a minor fraction of the electrochemically generated surface oxides. Potential holds at 1.0 V at room temperature only resulted in slight oxidation of Vulcan XC-72. However, experiments at 65°C showed clear signs of surface oxidation after only 16 h at potentials ⩾0.8 V, verifying that surface oxides can be generated under simulated PEM fuel cell conditions. Overall, these results suggest that changes in component hydrophobicity, driven by carbon surface oxidation, are an important factor in determining long-term PEM performance instability and decay. © 2004 The Electrochemical Society. All rights reserved.
E133
Qingzhi Guo and Ralph E. White
A model for the simulation of the steady-state impedance response of a polymer electrolyte membrane fuel cell (PEMFC) cathode is presented. The catalyst layer of the electrode is assumed to consist of many flooded spherical agglomerate particles surrounded by a small volume fraction of gas pores. Stefan-Maxwell equations are used to describe the multicomponent gas-phase transport occurring in both the gas diffusion layer and the catalyst layer of the electrode. Liquid-phase diffusion of
is assumed to take place in the flooded agglomerate particles. Newman’s porous electrode theory is applied to determine over-potential distributions. © 2004 The Electrochemical Society. All rights reserved.
E150
A. Šurca Vuk, M. Gaberšček, B. Orel and Philippe Colomban
E162
Ying Wang, Zheng-Wen Fu, Xiao-Li Yue and Qi-Zong Qin
An attempt to extend the application of the electrochemical mechanism on nanosized transition metal in the range 1-5 nm to drive formation and decomposition of
was made for other transition metal compounds. Using reactive pulsed laser deposition and dc discharge methods in a nitrogen ambient, a transition compound of
thin film has been fabricated successfully. The lithium electrochemical reaction of
thin-film electrode was first investigated by scanning electron microscopy (SEM), X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS), the discharge and charge, cyclic voltammetry (CV), the in situ spectroelectrochemical measurements. An irreversible process in the lithium electrochemical reaction of
thin-film electrode was confirmed by spectroelectrochemical, CV, ex situ XRD, and XPS measurement. However, irreversible capacity loss between the first two cycles is only 5% of the first discharge. The observed diffraction peaks from metal nickel in the lithiated thin films showed good crystallinity with crystal size more than 5 nm confirmed by transmission electron microscopy (TEM) and selected area electron diffraction (SEAD). So the oxidation/reduction of nanosized metal may not be used for an explanation for the electrochemical behavior of
thin film. Another reaction mechanism involves rich transition metals dispersed into a lithium containing matrix, two kinds of roles of metallic nickel are revealed, one part of metallic nickel is nitrided and reduced in the lithium electrochemical reaction, another part of nickel seems to act as an active spectator to drive the formation and decomposition of
© 2004 The Electrochemical Society. All rights reserved.
E168
Shen-Ming Chen and Sheh-Hung Hsueh
DIELECTRIC SCIENCE AND MATERIALS
F69
Marko Vehkamäki, Mikko Ritala, Markku Leskelä, Anthony C. Jones, Hywel O. Davies, Timo Sajavaara and Eero Rauhala
F73
Y. H. Wang and R. Kumar
F77
S. Van Elshocht, M. Caymax, S. De Gendt, T. Conard, J. Pétry, L. Daté, D. Pique and M. M. Heyns
F81
Norio Tokuda, Shingo Nishiguchi, Satoshi Yamasaki, Kazushi Miki and Kikuo Yamabe
F87
Y. K. Wang, C. H. Huang, T. Y. Tseng and Pang Lin
(PZT) thin films with a (110) preferred orientation were prepared on
substrates using a sol-gel method. The oxide bottom electrode, BSR, was fabricated at various temperatures on
substrates by rf sputtering. The annealed PZT films on
substrates exhibited improved crystallinity. The electrical properties of PZT films, such as the electric field
induced variations of the leakage current density, the dielectric constant, and the polarization were strongly dependent on the processing temperatures of the PZT films as well as the bottom oxide electrode. A typical PZT thin film annealed at 650°C on the BSR electrode, which was deposited at 450°C on the
substrate by a sputtering technique, has a leakage current of 
at an applied electric field of 500 kV/cm and a dielectric constant of 968. From the polarization-electric field characteristics, the remanent polarization and coercive field of the PZT were found to be
and
respectively, at an applied voltage of 5 V. The PZT films exhibited fatigue-free characteristics up to
switching cycles under 5 V bipolar pulses. © 2004 The Electrochemical Society. All rights reserved.
SEMICONDUCTOR DEVICES, MATERIALS, AND PROCESSING
G217
Jian-Bin Chiu, An-Jhih Su, Cheng-Ching Yu and Shih-Haur Shen
The simple analytical model of Boning and co-workers is extended by taking variable removal rate (RR) into account. The advantage of rapid process characterization is retained and model parameters can be obtained from experimental data, and more importantly, analytical solutions are available to provide necessary analysis. The result shows that tradeoff between electrochemically plated copper thickness and throughput exists when the conventional constant RR strategy is applied. At the low RR extreme, minimal Cu thickness is obtained while low throughput is also experienced as a result of low polish rate. At the high RR end, however, highest throughput can be achieved but extremely thick Cu layer should be plated in order to meet planarization specifications. This results in additional operating cost for post-CMP waste water treatment. Therefore, an optimal control problem is formulated for CMP planarization and an analytical solution for optimal RR trajectory is derived. The optimal trajectory achieves the highest throughput with minimal amount of copper thickness (47% less than the conventional practice). In addition to the variable RR strategy to carry out optimal process control, stepwise implementation is also proposed and it can readily be practiced on present CMP stations with little extra engineering effort. © 2004 The Electrochemical Society. All rights reserved.
G223
Han-Ki Kim, I. Adesida, K.-K. Kim, S.-J. Park and T.-Y. Seong
We have investigated Al/Pt (20/50 nm) ohmic contacts on a n-type zinc oxide (ZnO:Al) epitaxial layer. The samples were annealed at temperatures of 300°C and 600°C for 1 min in nitrogen ambient. Current-voltage measurements indicated that the as-deposited sample was ohmic with a specific contact resistivity of
However, the annealing at 300°C resulted in a significantly better ohmic behavior, with a contact resistivity of
A further increase in the annealing temperature to 600°C led to a decrease in specific contact resistivity due to extensive interfacial reactions between Al and ZnO. Both Auger electron spectroscopy and glancing angle X-ray diffraction were employed to investigate the nature of the interfacial reaction between the Al/Pt and ZnO layer with increasing annealing temperature. Possible explanation is given to describe the temperature dependence of the specific contact resistivity. © 2004 The Electrochemical Society. All rights reserved.
G227
Nak-Jin Seong and Soon-Gil Yoon
G230
T. Du, D. Tamboli, V. Desai and S. Seal
G236
Y. Ein-Eli, E. Abelev and D. Starosvetsky
G241
J. Lu, C. Rogers, V. P. Manno, A. Philipossian, S. Anjur and M. Moinpour
Chemical mechanical planarization (CMP) is a process widely used for the manufacture of silicon integrated circuits. In this work, we measured the thickness of the slurry film between the wafer and the pad during polish while simultaneously measuring the frictional drag. All experiments are performed on a 1:2 scale laboratory tabletop rotary polisher with variable pad speed and wafer downforce control. Dual emission laser-induced fluorescence techniques optically measured the slurry film thickness through a dual-camera imaging system. The resulting data are discussed for wafers polished with a 3.1 wt % abrasive concentration slurry solution on Freudenberg’s FX-9 polishing pads. It was found that the degree of surface curvature of the wafer substrate significantly influences the slurry film thickness and wafer drag, and therefore, the polish. The convex wafer shows the expected behavior of increased downforce reduces the slurry film thickness and increases the coefficient of friction. Further, as the pad speeds up, the slurry thickness increases and the friction decreases. The concave wafer shows no change in slurry film thickness and a decrease in the frictional coefficient with increasing downforce. Both the film thickness and frictional coefficient appear to decrease slightly with increasing pad speed. This difference between the two wafer shapes reflects the different fluid mechanics in each case. © 2004 The Electrochemical Society. All rights reserved.
G248
D. Cavalcoli, A. Cavallini and M. Rossi
Scanning Kelvin probe and surface photovoltage methods have been implemented in a single tool to obtain information on surface, as well as on bulk, electronic properties of mono- and multicrystalline Si wafers. The two combined methods allow for the measurement, in a noncontacting and nondestructive way, of three parameters: minority carrier diffusion length, majority carrier distribution in the near-surface region, and work function difference over the whole wafer area. Examples of the application of these methods to the characterization of crystalline wafers are presented. © 2004 The Electrochemical Society. All rights reserved.
G252
Jae Kyeong Jeong, Ho Keun Song, Myung Yoon Um, Hoon Joo Na, In Bok Song, Dae Hwan Kim and Hyeong Joon Kim
G257
Kyosuke Oshima, Sorin Cristoloveanu, Bernard Guillaumot, Simon Deleonibus and Hiroshi Iwai
To improve thermal dissipation in silicon-on-insulator metal-oxide-semiconductor field-effect transistors (SOI MOSFETs), we recently proposed replacing the buried oxide with buried alumina, which offers higher thermal conductivity. However, because alumina is a high-k insulator, there is also a definite impact on the electrical properties, namely, coupling and short-channel effects. Our simulations show that the role of fringing fields is accentuated, leading to more severe drain-induced barrier lowering (DIBL)-like problems. The trade-off between the thermal merit and the electrical performance of very advanced SOI transistors is examined by comparing various MOS architectures. We conclude on the usefulness of a ground plane located underneath a relatively thin buried alumina. © 2004 The Electrochemical Society. All rights reserved.
G262
Kyu-Jeong Choi, Jeon-Ho Kim and Soon-Gil Yoon
G266
A. F. Saavedra, K. S. Jones, M. E. Law and K. K. Chan
G271
D. Castillo-Mejia, J. Kelchner and S. Beaudoin
Polishing pad surface morphology has been demonstrated to be an important parameter in the optimization of chemical mechanical planarization (CMP) processes. In this work, the mechanical behavior of the asperity layer of a polishing pad and its effect on CMP is modeled. A Greenwood-Williamson microcontact model describes the asperity contact with the wafer. The local strain fields on individual asperities are calculated and then averaged, and an average elastic modulus is extracted to describe the asperity layer. The asperities are assumed to behave as an effective layer subject to this average strain field. The model is implemented on a previously developed locally relevant removal rate model for CMP. Comparison of the modeling results with polishing results obtained using a commercial CMP system shows important improvements in removal rate and uniformity prediction on the wafer-scale. © 2004 The Electrochemical Society. All rights reserved.
G279
S. Ohmi, M. Takeda, H. Ishiwara and H. Iwai
SENSORS AND DISPLAYS: PRINCIPLES, MATERIALS, AND PROCESSING
H75
Sheng Yao and Joseph R. Stetter
H81
Keekeun Lee and Keith E. Holbert
A deflected edge emission field effect transistor (DEEFET), a hybrid solid-state and vacuum microelectronics device, was constructed with electron-beam lithography to measure magnetic fields. The fabricated DEEFET device employs an extremely sharp emitter tip, a pair of gate electrodes, and a pair of split anodes. Field emission currents were observed around an anode bias of 40 V without gate bias. As the gate potential was increased, a lower turn-on voltage (around 25 V) and a higher field emission current were observed. A comparison of the anode and gate currents showed that most of the emitted electrons are collected by the anode, and only a few electrons are lost to the gate electrode. When forward and reverse magnetic fields were applied, an emission current imbalance was measured due to electron deflection by the Lorentz force. The calculated magnetic sensitivity was 98%/tesla for a forward magnetic field of 0.5 T and 92%/tesla for the reverse magnetic field. These magnetic sensitivities are up to six or seven times higher than those from a conventional silicon-based magnetic sensor with a split drain. © 2004 The Electrochemical Society. All rights reserved.
H86
Yasuo Shimomura and Naoto Kijima
We obtained a high-luminance
red phosphor by spray pyrolysis without postheating treatment using a high-temperature furnace with a long residence time and the addition of alkali metal salts to the precursor solution. The luminance under UV and vacuum UV radiation was about 100 and 90% that of the conventional phosphor made by solid-state reaction. The phosphor with the highest luminance was synthesized from a precursor solution that contained a lithium salt at 1.6 times the total of the yttrium and europium molar quantity. Optimum pyrolysis conditions were 1600°C temperature and 12 s residence time. The median particle diameter of the phosphor was 1.0 μm, which is much smaller and less agglomerated than the commercial phosphor made by solid-state reaction, whose median diameter was 3.5 μm. Compared with the phosphor having 1.5 μm median particle diameter by the solid-state reaction, the luminance of the phosphor in this study was 125%. An X-ray diffraction study indicated that the highest luminance phosphor obtained by the addition of a lithium salt had little strain in the crystal and that crystal growth was promoted by the additive. © 2004 The Electrochemical Society. All rights reserved.
H93
G. Baldacchini, T. Baldacchini, A. Pace and R. B. Pode
Recent annealing experiments have shown that
films are highly susceptible to various atmospheres, going to their destruction in particular environments well below 200°C. Moreover, before this abrupt transition a sizable increase in photoluminescence has been observed especially by annealing in humid air. This property, which hints at a new phase of the material with some analogies to the recently discovered δ-phase except for a much lower temperature, displays a remarkable stability in ambient air, a result with important implications both for the development of environmentally stable organic light-emitting diodes devices and for basic understanding of the morphological structure of
systems. © 2004 The Electrochemical Society. All rights reserved.