Equation or symbol description not availablePb(Zr0.53Ti0.47)O3 (PZT) thin films with a (110) preferred orientation were prepared on Equation or symbol description not availableBa0.5Sr0.5RuO3 (BSR)/Ru/SiO2/Si substrates using a sol-gel method. The oxide bottom electrode, BSR, was fabricated at various temperatures on Equation or symbol description not availableRu/SiO2/Si substrates by rf sputtering. The annealed PZT films on Equation or symbol description not availableBSR/Ru/SiO2/Si substrates exhibited improved crystallinity. The electrical properties of PZT films, such as the electric field Equation or symbol description not available(E) induced variations of the leakage current density, the dielectric constant, and the polarization were strongly dependent on the processing temperatures of the PZT films as well as the bottom oxide electrode. A typical PZT thin film annealed at 650°C on the BSR electrode, which was deposited at 450°C on the Equation or symbol description not availableRu/SiO2/Si substrate by a sputtering technique, has a leakage current of Equation or symbol description not available2.7×10−7 Equation or symbol description not availableA/cm2 at an applied electric field of 500 kV/cm and a dielectric constant of 968. From the polarization-electric field characteristics, the remanent polarization and coercive field of the PZT were found to be Equation or symbol description not available38.9 μC/cm2 and Equation or symbol description not available59.6 kV/cm, respectively, at an applied voltage of 5 V. The PZT films exhibited fatigue-free characteristics up to Equation or symbol description not available∼1.0×1012 switching cycles under 5 V bipolar pulses. © 2004 The Electrochemical Society. All rights reserved.