Anatase Equation or symbol description not availableTi1−xCoxO2 thin films onto Equation or symbol description not availableSiO2/Si substrates at 400°C using liquid-delivery metallorganic chemical vapor deposition (MOCVD) were successfully prepared and the ferromagnetic properties investigated through microstructural analysis by transmission electron microscopy and high-resolution scanning Auger microscopy as a function of Co-doping concentration. Ferromagnetic behaviors of polycrystalline films were observed at room temperature and the magnetic and structural properties depend critically on the Co distribution, which varies widely with Co-doping concentration. Annealed Equation or symbol description not availableTi1−xCoxO2 thin films with Equation or symbol description not availablex⩽0.05 showed a homogeneous structure without any clusters, and pure ferromagnetic properties of thin films are attributed only to the Equation or symbol description not availableTi1−xCoxO2 phases. In the case of thin films above Equation or symbol description not availablex=0.05,10­150 nm Co-rich Equation or symbol description not availableCo1−xTix clusters are formed in homogeneous Equation or symbol description not availableTi1−xCoxO2 phases. The solid solubility of Co was approximately 5 atom % in Equation or symbol description not availableMOCVD­Ti1−xCoxO2 polycrystalline thin films. Equation or symbol description not availableCo1−xTix clusters with a c axis preferred orientation decrease the value of Equation or symbol description not availableHc (coercive field) and increase the saturation magnetic field. The polycrystalline anatase Equation or symbol description not availableTi1−xCoxO2 thin films prepared by liquid-delivery MOCVD have an advantage for high-density device application in ferromagnetic semiconductor fields. © 2004 The Electrochemical Society. All rights reserved.