Abstract
Amorphous titanium oxide was prepared by a sol-gel route employing Ti(IV) alkoxide as a starting agent. The average size of the primary particles was about 4 nm, and the Brunauer-Emmett-Teller specific surface area was 390 m2 g−1. Addition of acetylene black in synthesis allowed us to obtain the composite of titania and carbon materials. The composite materials could be galvanostaticly discharged and charged around 2 V vs.
After thermal treatment at 330°C the composite showed specific capacity above 125 mA h g−1, even under large discharge current of 10 A g−1. Based on the relationship between specific capacity and current density, the chemical diffusion coefficient of lithium was estimated to be
© 2004 The Electrochemical Society. All rights reserved.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.

and
respectively, from ICP measurements. This is in good agreement with the estimation by use of specific capacity
for initial discharge,
for initial charge).