Abstract
The origins of persistent interactions among localized corrosion sites were investigated using multielectrode arrays (MEA). MEAs consisted of one hundred 250 μm diam AISI 316 stainless steel wires configured into
close-packed rectangle and
far-spaced configurations. Experiments were conducted in dilute chloride solutions and elevated temperatures to accentuate interactions. Interactions between early dominating pits and the adjacent electrode surface were found to develop as regions of enhanced or suppressed pitting susceptibility triggered by concentration and potential fields developed during growth of large pits, respectively. Transient aggressive species accumulation around active pits was also found to cause “surface damage” to electrodes that persisted for long periods after primary pits were repassivated and solutions extensively stirred. Oxide film alteration, mixed metal sulfide inclusion damage, and surface contamination were all considered to be possible origins of persistent interactions. Mn(Fe,Cr)S inclusions were implicated to be the origin of such persistent interactions. Persistent interactions were completely suppressed by nitric acid treatment, which is believed to remove or modify susceptible Mn(Fe,Cr)S inclusions. © 2004 The Electrochemical Society. All rights reserved.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.

concentrations even though
reached a maximum and began to decrease at
concentrations above 20%. The increase in Cr:Fe ratios, despite a corresponding decrease in pitting potential, strongly suggests that Cr:Fe ratios have secondary effects on the pitting potential.