A0: Macroscopic Modeling
3
Xuhai Wang and Trung V. Nguyen
In this study, a model was developed to evaluate the role of the micro-porous layer (MPL) and the effects of its properties on the liquid water saturation levels in the cathode porous media and the performance of a proton exchange membrane (PEM) fuel cell. The results validated that the fuel cell performance was improved by adding an MPL between the macro-porous gas diffusion layer (GDL) and the catalyst layer (CL) in the cathode side. The MPL, due to its high hydrophobicity, increases the liquid water pressure in the cathode to the levels much higher than those in the anode resulting in an increased back-transport rate of liquid water from the cathode to the anode. The more hydrophobic the MPL is, the higher liquid pressure increases, and, consequently, the higher driving force is created across the membrane to drive water from the cathode to the anode.
13
Nobuaki Nonoyama and Yoshihiro Ikogi
We have developed mathematical models of PEMFC to design MEA. For quantitative simulations, a model is required to reflect the effects of the physical properties of each component and the operating conditions of a cell accurately. Therefore, the model was constructed with as many principal physical equations as possible and was validated with experimental data from a wide range of conditions. Here, we examined the effect of some physical parameters of membrane for low-humidity operation. The importance of water diffusion as well as proton conductivity was shown. The orders of performance for small-size cells with high gas stoichiometry are often different from that of large-size cells with the same parameters. The reason for this discrepancy is explained.
23
Torsten Berning
This research focuses on the analysis of multi-phase flow through the porous media of the cathode side of a PEM Fuel Cell using a three-dimensional, multi-fluid model based on computational fluid dynamics (CFD). In a first step, it is assumed that all product water exists and leaves the cell in the liquid phase, and its flow through the catalyst layer, micro-porous layer, and gas diffusion medium is investigated as function of in- and through plane hydraulic permeability, effective contact angles, and irreducible saturation of each layer. The effect of under-the-land compression on the predicted water saturation level will be discussed. Finally, the important role of the pore size distribution of the porous media on the liquid water transport and predicted saturation level ("flooding") is highlighted, and a qualitative approach to obtain the capillary pressure curve as function of liquid saturation for different types of porous media will be outlined.
35
Andrew J. Desouza, Radu Bradean, Virginia Branzea, Stephen Hamada, Joerg Kleemann, Herwig Haas, Joy Roberts and Emerson Gallagher
Membrane electrode assemblies (MEAs) that were initially adhered at the cathode-catalyst-layer/cathode-porous-electrode (CCL/CPE) interface can become unadhered at this interface because of operational stressors. Unadhered MEAs may have an additional electrical contact resistance between the CCL and the CPE that was not present for adhered MEAs. This paper investigates the impact of an electrical contact resistance between the CCL and the CPE on fuel cell performance. Model predictions and experimental results are compared for adhered and un-adhered MEA designs operating in plates with different gas distribution channel geometries for a wide range of operating conditions. Model and experiment indicate that the effect of an electrical contact resistance between the CCL and the CPE can lead to significant performance loss.
45
Kunal Jain, James Vernon Cole, Sanjiv Kumar, Ashok Gidwani and N. Vaidya
A finite volume based computational method for predicting two-phase flows in fuel cells is presented. The model formulation and numerical algorithms are selected to provide robustness and accuracy, while allowing the treatment of important phenomena relevant to fuel cell water management such as segregation of the phases to form films and slugs in gas channels. Variations in the algorithms for computing pressure corrections and phase fractions are assessed using water-air flows in fuel cell channel geometries. The accuracy of the model is evaluated by comparison to benchmark simulations, measured pressure drop data for air-water flows, and analytical solutions for capillary pressure in porous media. The results indicate that the selected formulation is sufficiently stable and accurate to serve as the basis for a detailed model of water transport in fuel cells.
57
Michihisa Koyama, Donghyun Kim, Boyeong Kim, Tatsuya Hattori, Ai Suzuki, Riadh Sahnoun, Hideyuki Tsuboi, Nozomu Hatakeyama, Akira Endou, Hiromitsu Takaba et al
Toawrd rational design of polymer electrolyte fuel cell (PEFC), understandings of both atomistic scale and systems characteristics are important. Multi-scale simulation can contribute to bridging microscopic and macroscopic understandings effectively. In this manuscript, we described a multi-scale simulation approach based on an original porous structure simulator and computational chemistry methods. Proton conductivity was estimated by molecular dynamics method and structures of porous catalyst layer were modeled by the porous structure simulator. Multi-scale simulations for macroscopic current-voltage characteristics of PEFC were performed considering both atomistic-scale properties and porous microstructure. Influences of atomistic properties and microstructure of porous catalyst layer on macroscopic current-voltage characteristics were successfully studied. Effectiveness of the developed multi-scale simulation approach was confirmed from the simulation results.
67
Shiladitya Mukherjee, James Vernon Cole, Kunal Jain and Ashok Gidwani
The lattice Boltzmann (LB) method is employed to simulate single and multiphase flow through porous gas-diffusion-layer (GDL) of a Proton Exchange Membrane Fuel Cell (PEMFC). The porous layer is composed of layers of fibers. The structure is reconstructed numerically and validated by other published data on porosity and pore-size distributions. The in-plane gas-permeability is greater than the through-plane values and has greater sensitivity to fiber orientations. The permeability decreases as the GDL is compressed. When liquid is introduced, multiple droplets emerge from the other side of the GDL through surface pores. On hydrophobic GDL, the liquid advancing inside the GDL is in the form of several interconnected streams leading to surface openings. As the hydrophobicity is increased the liquid break-through occurs at lower saturation.
79
Etim U. Ubong, Zhongying Shi and Xia Wang
This paper is to investigate the performance of a high temperature proton exchange membrane fuel cell. Both experimental work and numerical simulation are conducted. The high temperature proton exchange membrane (HT-PEM) is based on polybenzimidazole (PBI) doped with phosphoric acid. A single cell with triple serpentine flow channels was operated at steady state at various levels of temperature, pressure and air stoichiometry. A three dimensional model based on COMSOL Multiphysics software was used to simulate the cell performance and polarization curves were used to validate the experimental values. The theoretical model accurately predicts the experimental results. A sound knowledge of the impact of various variables, at various levels of the cell operation is necessary for unraveling the parametric influence and can prove extremely useful for optimizing the cell operation.
C0.1: Non@–Pt Catalyst
93
Jinli Qiao, Jun Sheng Zheng, Bing Li and Jianxin Ma
Binary IrCo alloy as a novel substitute for platinum has been viewed as the anode catalyst in hydrogen-air fuel cells. The resulting IrCo/C of 50/50 ratio, heat treated at 800{degree sign}C in argon atmosphere, shows promising catalytic performance in terms of hydrogen oxidation reaction. Results of electrochemical characterization, which was performed using a rotating disc electrode (RDE) by cyclic voltammetry (CV) and liner sweep voltammetry (LSV), with emphasis on the activity of the catalyst are presented.
99
Pahiyamattom J. Sebastian, Edgar Valenzuela, Shine Joseph and Joel Moreira
The authors studied no-platinic and low-platinum containing electrocatalysts for fuel cell application. The electrocatalysts were based on Pt, Ru, Mo, W, Pd and Au. In some cases Pt was alloyed with these elements and in others without Pt and also alloyed among the non-platinic catalysts. The Pt-M (M represents the non-platinic element) and no-platinic catalysts exhibited better characteristics for oxidation of fuels other than hydrogen. All the catalysts showed suitable characteristics for oxygen reduction reaction. The catalysts were synthesized by a thermal pyrolysis of the carbonyl compounds or by a chemical reduction of the chlorides of the corresponding elements. The catalyst performance depended on the particle size, distribution on the gas diffusion electrode, type of catalyst support, the alloy composition etc. The nanostructured catalysts were characterized by high resolution transmission electron microscope (TEM), x-ray diffraction (XRD) and the electrochemical techniques.
109
Xiaoping Wang, Nancy Kariuki, Suhas Niyogi, Matt C. Smith, Deborah J. Myers, Timo Hofmann, Yufeng Zhang, Marcus Bär and Clemens Heske
Bimetallic palladium-base metal nanoparticle catalysts are being investigated as alternatives to platinum-based catalysts for the oxygen reduction reaction (ORR) in polymer electrolyte fuel cells. We report here our results on the palladium-copper, palladium-nickel, and palladium-iron systems. We are studying the effect of synthetic procedure, palladium to base metal ratio, heat treatment temperature, and heat treatment atmosphere on the ORR activity as well as on the valence band structure of these systems. Palladium-copper nanoparticle catalysts synthesized by the colloidal technique with a composition of 75 mol% copper are the most active investigated thus far. This catalyst shows an ORR activity which is approximately 75% that of platinum (per gram of platinum-group metal). The corresponding valence band structure is strongly modified compared to that of Pd and Cu alone and resembles that of Pt, which is believed to be the reason for its superior performance among the other investigated platinum-free alternatives.
C0.2: Non–Pt and Non-Precious Catalyst
123
Vito Di Noto, Enrico Negro, Sandra Lavina, Nicola Boaretto and Matteo Piga
This report describes two new synthesis protocols for the preparation of "core-shell" platinum-free electrocatalysts consisting of graphite cores covered by carbon nitride shells embedding the active sites. The resulting systems are characterized by a well-controlled chemical composition with different wt% of nitrogen in their supports. The protocols rely on the thermal decomposition of precursors obtained by networking suitable metal coordination complexes with an organic binder over active carbon nanoparticles. The resulting electrocatalysts showed a higher thermal stability in oxidizing conditions with respect to a reference system. The materials provided a remarkable performance in the oxygen reduction reaction (ORR), even if a lower selectivity towards the desired 4-electron pathway is observed. Membrane electrode assemblies (MEAs) tested in operative conditions with the proposed materials applied at the cathode required a lower mass of noble metal (up to 0.46 g/kW) to achieve the same electrical power as the platinum-based reference (1.1 g/kW).
139
Arnd Garsuch, Xavier Michaud, Catherine O'Neill, Ping Li and Jeff Dahn
Mesoporous Ru- and RuSe-based catalysts for proton exchange membrane fuel cells were prepared using an amorphous silica gel as a template. Impregnation with sucrose (carbon source), ruthenium(III)-chloride and selenium dioxide was employed to infiltrate the catalyst precursors in the mesopores of the template. After carbonization in argon and reduction in hydrogen atmosphere, the catalyst materials were liberated by dissolving the template framework with hydrofluoric acid. Nitrogen adsorption, X-ray diffraction and transmission electron microscopy were used in order to investigate the structural properties of the prepared catalyst samples. The catalytic activity towards the reduction of oxygen was tested using the rotating-ring-disk-electrode technique. It was observed that RuSe-containing carbon samples possess a higher catalytic activity for oxygen reduction than Ru-containing carbon samples.
147
Eric J. Rees, Kenji Essaki, Connor Brady and G. T. Burstein
Microwave-induction heating has been used to synthesise tungsten and tantalum carbides, from precursor mixtures of the metal oxides and graphitic carbon. The electrocatalytic tungsten carbide is considered to be a possible alternative to platinum-based materials, on fuel cell anodes. It is shown that the phase composition of the products of microwave heating is similar to that produced by conventional furnace heating. However the more rapid microwave technique leads to the production of smaller nanoparticles, and concomitantly higher electrocatalytic activity. A number of admixants have been investigated for the carbide synthesis, including iron, nickel, potassium chloride, and manganese. These additives had various significant influences on the syntheses. When an admixant exhibited an effect on the furnace-synthesized carbide products, a similar effect was found following microwave-syntheses. In particular, KCl promoted the reduction of tungsten oxide to the metal and carbide phases, and nickel led to grain coarsening of the product.
159
Gang Wu, Zhongwei Chen, Kateryna Artyushkova, Fernando H. Garzon and Piotr Zelenay
This paper focuses on a new polyaniline-derived non-precious cathode catalyst with high oxygen-reduction activity, verified in electrochemical and fuel cell testing. The rotating disk (RDE) onset and half-wave potential of oxygen reduction were measured at 0.90 V and 0.77 V, respectively. Rotating ring-disk electrode (RRDE) study revealed very good selectivity in the four-electron reduction, with peroxide yields below 1% (0.4% at 0.4 V). Similarly, the catalyst showed good performance in the hydrogen-air fuel cell, even at high cell operating voltages, yielding 0.04 A cm-2 at 0.80 V and 0.21 A cm-2 at 0.6 V. Fuel cell life test at a constant voltage of 0.4 V demonstrated promising stability up to 450 hours, generating a current density of approximately 0.32 A cm-2, a respectable performance for a non-precious cathode catalysts operated on air rather than oxygen. Ex situ characterization pointed to pyridine- and pyrrole-like metal species as likely active ORR sites.
Morning Plenary Session
173
Keith B. Wipke, Sam Sprik, Jennifer Kurtz and John Garbak
The "Controlled Hydrogen Fleet and Infrastructure Demonstration and Validation Project," is a five-year U.S. Department of Energy (DOE) project started in 2004. The purpose of this project is to conduct an integrated field validation that examines the performance of fuel cell vehicles and the supporting hydrogen infrastructure. NREL has analyzed data from almost three years of the five-year project. During this time, 92 vehicles have been deployed, 15 project refueling stations were placed in use, and no fundamental safety issues have been identified. We've analyzed data from over 200,000 individual vehicle trips covering 1,100,000 miles traveled and over 40,000 kg hydrogen produced or dispensed. Public analytical results for this project are in the form of composite data products, which aggregate individual performance into a range that protects the intellectual property and the identity of each company, while still publishing overall status and progress.
185
Koichi Kojima and Toru Morita
Concerns surrounding the timing of peak oil for conventional fossil fuels (i.e., the point at which the maximum global production rate will be reached) and the growing need to reduce CO2 emissions are increasing the importance of energy source diversification. For vehicles, this can be accomplished by more efficient internal combustion engines (ICE), the use of bioethanol, more widespread application of ICE-hybrid systems, and the development of technologies that use electricity and hydrogen, such as plug-in hybrid vehicles (PHV) and fuel cell hybrid vehicles (FCHV). Since Toyota started limited lease of the Toyota FCHV, the world's first market-ready fuel cell vehicle, in 2002, Toyota has steadily improved the technology, and has succeeded in significantly extending the vehicle's cruising range in actual driving conditions and enhancing its cold start capabilities. For the next step, Toyota aims to work toward the commercialization and popularization of fuel cell vehicles by focusing on reducing costs and improving durability, and by cooperating with governments and energy companies to establish hydrogen infrastructure.
199
Masahiro Watanabe, Mitsuru Wakisaka, Hiroshi Yano and H. Uchida
We first reported that enhanced activities in oxygen reduction reaction (ORR) are obtained at Pt skin-layer formed on the surfaces of alloyed Pt with non-precious metals such as Fe, Co, Ni, etc. and also that a positive core level shift in Pt4f7/2 was observed at the Pt skins, due to the modification of the Pt electronic structures. It was also found that such an enhancement is induced without changing the activation energy but the corresponding frequency factor value Z from that of pure Pt. The enhancement mechanism is discussed with the experimental data obtained by using electrochemical-XPS system on adsorbed O-containing species at the Pt skin-layers in comparison with pure Pt. The enhancement, or increased Z values, can be correlated to the increase in Oads formed by dissociative adsorption of O2, resulting in the enhanced activity.
Afternoon Plenary Session
209
Jeffrey Greeley
Three case studies of the use of Density Functional Theory calculations to model electrochemical phenomena are presented. These studies range from fundamental investigations of electrocatalytic reaction mechanisms to detailed atomistic analyses of dissolution and dealloying phenomena. The studies are intended to illustrate how first principles calculations are beginning to complement and enhance well-established experimental results in electrochemistry.
225
Masanobu Uchimura, Seiho Sugawara, Yosuke Suzuki, Jianbo Zhang and Shyam S. Kocha
Proton Exchange membrane fuel cells (PEMFCs) for automotive applications are subject to hundreds of thousands of potential or load cycles during normal operation of the vehicle. Pt dissolves under such cycling and is a major contributing factor to the lowered durability of PEMFCs. This paper details the effect of various simplified potential-cycle profiles, the effect of operating conditions such as temperature, relative humidity, reactant gases etc., as well as different catalyst materials under normal fuel cell operating voltage ranges (0.95-0.60V) in fuel cells. Results on Pt dissolution utilizing complementary ex-situ methods are also presented. The fundamental and practical implications of varying the operating parameters as well as a possible hypothesis for Pt dissolution are reported.
235
Frank D. Coms
A detailed thermochemical and kinetic analysis of PFSA ionomers and the reactive oxygen species formed in an operating fuel cell is reported. The analysis reveals that hydroxyl radical is the only oxygen species capable of abstracting a hydrogen atom from carboxylic acid intermediates, thereby propagating the PFSA main chain unzipping process. Two chemically specific, main chain scission mechanisms are proposed. The first involves formation of sulfonyl radicals under dry conditions and the second invokes the action of hydrogen atoms formed from hydrogen gas and hydroxyl radical. The thermochemical analysis provides a strong basis from which to rationalize the results from a broad range of in-situ and ex-situ fuel cell degradation studies.
257
Hiroyuki Yanagi and Kenji Fukuta
We newly developed the anion exchange membranes and ionomers for alkaline membrane fuel cell system. The AEMs consist of hydrocarbon type main chain and quaternary ammonium groups as ion exchanging site, and they show sufficient OH- conductivity and thermal durability. The ionomer also consists of hydrocarbon type main chain and quaternary ammonium groups. It shows applicable OH- conductivity for the catalyst layer of fuel cells. We evaluated the cell performance based on the developed membrane and ionomer . It shows sufficient cell output even if the ambient air was used as the oxidant.
263
Thomas J. Schmidt and Jochen Baurmeister
This paper describes some detailed information on the development and properties of high temperature polybenzimidazole based Celtec MEAs. Specifically, insight is given on anode behavior for the oxidation of CO containing reformates as well as on the development of corrosion stable cathodes.
A1.1: Water and Thermal Management
273
Jixin Chen, Yun Wang and Partha P. Mukherjee
This paper investigates interaction of the electrochemical kinetics, oxygen transport and solid water formation within polymer electrolyte fuel cell (PEFC) electrode during cold start. Followed by the analysis of Wang [1], we simplify the one-dimensional model of electrode processes, which allows solving the profiles of important quantities and directly relating the ice impact mechanisms to surface overpotential. The key parameters that govern these profiles are evaluated in the range of the relevant factors for a typical fuel cell. We also decouple the mechanisms of solid water impacts and compare their importance. This study is valuable for studying the characteristics of cold-start for PEFCs.
285
Ryan J. Balliet, Karen E. Thomas-Alyea and John Newman
A two-dimensional, transient model of the full-cell sandwich has been developed in order to predict water redistribution during the freezing process. Critical factors affecting the magnitude and direction of water movement are found to be the location of the cell within the stack, the permeability of the porous media of the cell, and the high thermal conductivity of the rib relative to the gas channel.
297
Kevin G. Gallagher, Bryan S. Pivovar and Thomas F. Fuller
Measurements of the electro-osmotic drag coefficient for Nafion® and both random and multi-block co-polymer sulfonated poly(arylene ether sulfone) (BPSH) chemistries are reported for vapor equilibrated samples below 0 {degree sign}C. No significant change in the drag coefficient behavior for Nafion from that reported above 0 {degree sign}C is found. However BPSH is found to have a drag coefficient of 0.4. The implication of a drag coefficient less than unity in the interpretation of conduction mechanisms is discussed. Measurements of water sorption isotherms below 0 {degree sign}C are also presented. A significant reduction in the capacity of polymer electrolytes to store water below 0 {degree sign}C is found. This reduced water content is a result of the lower vapor pressure of ice compared to supercooled liquid.
309
William Braff and Cortney K. Mittelsteadt
A novel technique for measuring the electroosmotic drag coefficient (EODC) of proton exchange membranes using a non flow through, or "dead-ended" hydrogen pump is presented here over a full range of non-condensing humidification. This experiment is conducted in situ under "fuel cell like" conditions, so the transport phenomena observed are directly applicable to an operating fuel cell without any extrapolation. Experiments were conducted on 50 μm and 500 μm Nafion® 1100 EW membranes. The measurements consistently demonstrated that for low to medium humidification, the EODC observed is below unity. This observation confirms that the vehicular proton transport mechanism cannot be the sole source of proton transport at low relative humidity, leading one to conclude that the Grotthus "hopping" mechanism is active even at low levels of humidification.
317
Irfan Hussaini and Chao-Yang Wang
Response of PEM fuel cells to a step-change in load is investigated experimentally in this work. Voltage undershoot, a characteristic feature of such transient response, is shown to be due to transients of water distribution in membrane phase occurring at sub-second time scales. Use of humidified reactants as a means to control magnitude of voltage undershoot has been demonstrated. Constant stoichiometry operation under certain current-step conditions is found to result in reactant starvation, potentially leading to cell shut down. Further, response under step decrease in current density has been explored to determine existence of hysteresis. Under sufficiently humidified conditions, response under forward and reverse step changes are found to be symmetric, but under low RH conditions, voltage undershoot is found to be twice as large as the overshoot.
329
John Davey, R. Mukundan, Jacob Spendelow, Daniel S. Hussey, David Jacobson, Muhammad Arif and Rodney L. Borup
The water dynamics of the membrane electrode assembly (MEA) of a 50 cm2 polymer electrolyte membrane (PEM) fuel cell was studied in response to current and humidity step transients as a function of inlet relative humidity (RH) and cell operating temperature. MEA water content change was monitored by high frequency resistance (HFR) and in situ neutron imaging. The MEA "wetting" response was significantly faster (10-30 seconds) than the reciprocal "drying" response (several minutes). The wetting response to increasing current appears faster than that to increasing gas inlet RH. Wetting and drying responses to gas inlet RH transients are greater at low current densities showing the dominating effect of current wetting over gas inlet humidity effects. Operating the fuel cell at 40oC with no inlet gas humidification, a current wetting response was observed and 34 amps of current sustained. This showed that reaction water produced at the cathode is sufficient to support high current density if the drying effect of inlet gases is low. It also suggests that back diffusion of reaction water to the MEA is sufficient to account for the fast drop in HFR. In situ neutron imaging results show that GDL wetting is also faster than drying but on a slower time scale than that for the MEA. However, MEA and GDL drying are on a similar slow time scale and are coupled because water diffusing out of the MEA must move through the GDLs.
341
Koichiro Aotani, Shin-ichi Miyazaki, Norio Kubo and Masafumi Katsuta
Water transport resistance through the polymer electrolyte membrane was evaluated by measuring the water permeability of it. From the results of a thickness sensitivity evaluation, two types of water transport resistance were found. One was "internal diffusion resistance," which was proportional to the membrane thickness, and the other was "interfacial transport resistance," which was independent of thickness. This interfacial resistance was found not to be negligible. Furthermore, both resistances showed sensitivity to temperature and relative humidity. The internal diffusion coefficient estimated from the results of water permeation experiments correlated well with the results obtained by the pulse field gradient nuclear magnetic resonance (PFG-NMR) method. And, the electro-osmotic drag coefficient was also measured by the proton pump balance method based on the water permeation test system. It was concluded that water permeation experiments are helpful for obtaining a better fundamental understanding of water transport mechanism through the membrane.
B1.1: Catalyst Degradation I
355
Yunlong Gu, Jean St-Pierre, Ronald S. Goeke, Abhaya Datye and P. Atanassov
A model Pt catalyst nano-array on planar glassy carbon was synthesized and subjected to a potential cycle aging procedure. Preliminary experimental data suggest a similar degradation behavior as gas diffusion electrodes with an observed decrease in surface area (decrease in H2 and CO oxidation peak areas as determined by cyclic voltammetry). Atomic force microscopy topography images support this conclusion.
361
Yuyan Shao, Rong Kou, Jun Wang, Ja Hun Kwak, Vish Viswanathan, Yong Wang, Jun Liu and Yuehe Lin
ETek Pt/C catalyst was used as standard materials to develop a new test protocol for fast screening durable catalyst for PEM fuel cells. Potential step (Pstep) method with the upper potential of 1.4V and the potential-static (Pstat) holding at 1.4 V or 1.2V are used to degrade the catalyst. The degradation in the electrochemical surface area (ESA) for Pt/C under Pstep conditions is greatly accelerated as compared with that under other conditions. The durability of Pt/Vulcan and Pt/CNT were studied using the new protocol with the electrochemical stressing of Pstep(1.4V/0.6V), which provided the same results as those tested using conventional protocols: Pt/CNT is more durable than Pt/Vulcan. This confirms that the new protocol works well in screening catalyst in terms of durability. The new protocol can differentiate the durability of electrocatalysts by shortening the test time to several hours.
367
Tomohiro Takeshita, Hajime Murata, Tatsuya Hatanaka and Yu Morimoto
Pt particle size distributions at various positions in a cathode catalyst layer were evaluated by transmission electron microscopy (TEM) observation before and after a potential cycling test and by simple 1D macro model simulation to describe the degradation phenomena. Both the results showed similar tendencies: at the position near the membrane, the number of Pt particles for all sizes decreased with time; in contrast, at the position near the gas diffusion layer (GDL), the number of large Pt particles increased. The validity of this model is not verified yet because the precision of parameters is not confirmed. This model, however, can be used as a tool for deeper understanding of Pt degradation.
C1.1: Non–Precious Catalyst
377
Haixia Li, Hengyi Li and Xuan Cheng
The cobalt-polypyrrole (Co-PPy) composites adsorbed on the multiwall-carbon nanotubes (MWCNTs) were prepared by three methods. The structural, chemical and electrochemical properties of Co-PPy-MWCNTs samples were characterized by using XRD, SEM/EDX, element analysis, TG, FTIR, XPS, and cyclic voltammetry (CV). The results revealed that the Co-PPy was deposited on the MWCNTs surface and the ratios of Co/N for the three samples prepared differently varied. The conductivities and electrochemical catalytic activities of Co-PPy-MWCNTs samples were also affected by the different interactions between Co and PPy presented when using three preparation methods.
385
Hoon T. Chung, Christina M. Johnston, Fernando H. Garzon and Piotr Zelenay
An active, non-precious catalyst for electrochemical oxygen reduction was made by heat-treating simple precursors. The current density obtained in an H2/O2 PEM fuel cell was as high as 0.34 A/cm2MEA at 0.65 V. The oxygen-reduction activities of catalysts prepared at different temperatures over the range 800-1050{degree sign}C were shown to be equivalent by the Rotating Ring Disk Electrode (RRDE) method. The nitrogen content, however, was observed by XPS to be highly variable with preparation temperature. Thus, in contrast to some reports in the literature, the surface nitrogen content was not strongly correlated to performance. The nature of the active site(s) is currently under investigation.
393
Eric Proietti and Jean-Pol Dodelet
The effect of ballmilling three carbon black supports on the ORR activity of Fe-based electrocatalysts was investigated. Catalysts were prepared by acid-washing these ballmilled carbon supports, then impregnating them with iron(II) acetate and pyrolyzing in NH3 at 950{degree sign}C. It was found that ballmilling the carbon support improved the ORR activity for catalysts made with Black Pearls 2000 (Cabot), but decreased it for those made with N650 and left it relatively unchanged for those made with N234 (both low surface area commercial furnace carbon blacks from Sid Richardson Carbon Corporation). For catalysts made with ballmilled Black Pearls 2000, it was found that ORR activity increases as i) degree of disorder increases, ii) the change in micropore surface area due to pyrolysis increases, iii) nitrogen content increases and iv) crystallite size (La) approaches 24 Aå. No compelling trends were found for catalysts made with ballmilled N234 and N650.
405
Vijayadurga Nallathambi, Xuguang Li, Jong Won Lee and Branko N. Popov
Carbon-based catalysts for oxygen reduction reaction (ORR) were synthesized by modifying the carbon surface with nitrogen-containing precursors. The electrocatalytic properties were studied as a function of surface treatment, nitrogen and oxygen concentrations, and heattreatment temperature. The catalysts showed an onset potential for ORR close to 0.83 V and the amount of H2O2 generated was about 1 % at 0.5 V under our experimental conditions. The current transient in fuel cell at 0.4 V exhibited an initial increase of current density to approximately 0.12 A cm-2 and then a steady-state current profile for up to 200 h. The characterizations indicated that pyridinic and graphitic nitrogen acts as catalytic sites for ORR.
419
Michael A. Kostowskyj, Donald W. Kirk and Steven J. Thorpe
This work investigated the synthesis and characterization of a Ag-Mn bifunctional catalyst for the oxygen reduction reaction at the cathode of a fuel cell system. A template-base electroless deposition method was developed to deposit Ag as a model system and then to co-deposit Ag-Mn and synthesize the nanowire catalysts. Scanning electron microscopy showed that Mn altered the growth mechanism of the pure Ag deposit. Scanning transmission electron microscopy confirmed that small amounts of Mn co-deposited with Ag using the novel procedure developed. Current work is ongoing to determine the chemical form and amount of Mn present in the nanowires.
431
Juan Herranz, Michel Lefe`vre and Jean-Pol Dodelet
The adsorption of iron II acetate over two microporous carbon blacks of different surface properties was studied in order to determine if this factor limits the activity of Fe/N/C catalysts for ORR made with these carbon supports. Whereas one of these carbons only had oxygen-derived functionalities over its surface, the other one contained both oxygen and nitrogen bearing functionalities. Their points of zero charge (PZC) were first determined to be 3.9 and 8.8, respectively. Adsorption curves showing the evolution of the metallic uptake with the pH revealed that both carbon supports are able to adsorb 100% of the positive Fe ions in solution at pH>4, and this up to 0.8 wt% Fe. Therefore, the adsorption of iron is not the factor responsible for the limited site density of Fe/N/C catalysts having a Fe content {less than or equal to} 0.8 wt% loaded either by adsorption or by wet-impregnation of the carbon supports.
443
Ruizhi Yang, Tara Dahn and Jeff Dahn
Fe-N-C catalysts were prepared by impregnating FeCl3 within two kinds of activated carbon (Kuraray GC and Nuchar) that had been previously burned-off at 500oC in air to vary their pore sizes in a controlled way. The impregnated samples were subsequently heated at 850oC in NH3. The average pore size of the samples was determined by small-angle X-Ray scattering (SAXS) measurements and quantified by the radius of gyration (Rg) of the pores. The catalytic activities of the samples vary with the pore size of the activated carbon, which depends on the burn-off time. The results support suggestions from the Dodelet group about the importance of the pore size in determining catalytic activity.
449
Akimitsu Ishihara, Motoko Tamura, Youta Maekawa, Yoshiro Ohgi, Koichi Matsuzawa, Shigenori Mitsushima and Ken-ichiro Ota
A partially oxidized TaC0.58N0.42 has been investigated as a new cathode for polymer electrolyte fuel cells. The catalytic activity for oxygen reduction reaction (ORR) significantly depended on an oxidation state of the TaC0.58N0.42. TaC0.58N0.42 and Ta2O5 had a poor catalytic activity for the ORR. The onset potential on the partially oxidized TaC0.58N0.42 for the ORR had a maximum value of 0.9 V vs. RHE in 0.1 mol dm-3 H2SO4 at 30oC. Hard X-ray PhotoElectron Spectroscopy and XRD analyses indicated that the surfaces of the partially oxidized TaC0.58N0.42 were oxidized, although the inner parts of the partially oxidized TaC0.58N0.42 remained tantalum carbonitride. This result indicated that an appropriate oxidation of the TaC0.58N0.42 was essential to enhance the catalytic activity for the ORR.
459
Hirohisa Tanaka, Koichiro Asazawa, Tomokazu Sakamoto, Takeshi Kato, Mitsuru Kai, Susumu Yamaguchi, Koji Yamada and Hirotoshi Fujikawa
In order to overcome the barriers against the FCVs, a platinum-free anionic fuel cell has been developed. The platinum-free fuel cell, by using liquid hydrazine hydrate (N2H4·H2O) for fuel, comprises cobalt or nickel for the anode and cobalt for the cathode, can demonstrate a high performance, and achieves zero CO2 emissions. For vehicle application, a detoxification method, which repeatedly fixes and releases hydrazine hydrate, has also been developed. In this paper, the fuel cell performance using nickel, cobalt and platinum as an anode catalyst was compared. It was shown clearly that nickel and cobalt have the superior catalytic activity to platinum. The influence of fuel concentration and KOH addition is also discussed. This new fuel cell technology can conquer the conventional subject, and is expected to spread widely. Moreover, this technology was exhibited and attracted attention in Environmental Showcase of G8 Hokkaido Toyako Summit held in July, 2008.
D1.1: DMFC Anode Catalysts
467
Sanping Jiang, Shuangyin Wang and Xin Wang
A new synthesis method for the preparation of high performance PtRu electrocatalysts on multi-walled carbon nanotubes (MWCNTs) is reported. In this method, bimetallic Pt-Ru electrocatalysts are deposited onto 1-aminopyrene (1-AP)-functionalized MWCNTs by a microwave-assisted polyol process. The non-covalent functionalization of MWCNTs by 1-AP is simple and can be carried out at room temperature without the use of expensive chemicals or corrosive acids, thus preserving the integrity and the electronic structure of MWCNTs. PtRu electrocatalysts on 1-AP functionalized MWCNTs show much better distribution with no formation of aggregates, higher electrochemically active surface area and higher electrocatalytic activity for the electrooxidation of methanol in direct methanol fuel cells as compared to that on conventional acid treated MWCNTs and carbon black supported PtRu electrocatalysts.
473
Yu-Chi Hsieh, Yung-Jean Lu, Pu-Wei Wu, Yun-Min Chang and Yu-Fan Chiu
A galvanostatic pulse electrodeposition technique of preparing nanoparticulate PtRu electrocatalyst for direct methanol fuel cells has been demonstrated. After extensive cyclic voltammetric analysis, we determined the optimized parameters for the methanol oxidation to be current on-time on 50 ms, current off-time of 400 ms, current density of 50 mA/cm2, and total charge of 8.0 C/cm2. In addition, the catalyst loading was measured at 68 μg/cm2, resulting in a mass activity of 213 mA/Pt.mg. The composition for the nanoparticles was confirmed as Pt65Ru35. High-magnification images on the specimen indicated fine particles in 4-20 nm with uniform distributions.
483
Noelia Cabello-Moreno, Eleanor Crabb, Janet Fisher, Andrea E. Russell and David Thompsett
This paper reports an 'MEA based' accelerated ageing test designed primarily to investigate stability of anode catalysts for DMFCs. The effect of potential cycling on the anode with increasing number of cycles is investigated. Methanol stripping voltammetry is used to characterize changes at both the anode and cathode catalysts and the changes observed are related to quantitative changes in performance of the MEA polarization data. Changes in catalyst morphology and surface composition are characterized by TEM. In particular, comparisons between unsupported PtRu ('black') and carbon supported PtRu catalysts are made.
497
Moitrayee Chatterjee, Susanta Ghosh and Indra N. Basumallick
Nanosized platinum catalysts were deposited onto graphite and carbon felt surface by both chemical and electrochemical techniques. The controlled potentiostatic condition was used for electrodeposition using cationic surfactant, CTAB, at pre-CMC concentration in electrolytic bath. Electrocatalytic activity of such electrodes for methanol oxidation were studied and compared. The parameters like peak potential (Ep), peak current (ip), apparent diffusion coefficient for methanol (Dapp), Tafel slope and apparent rate constant (k) were obtained from cyclic voltammograms of methanol oxidation in acid medium. The morphology and crystal structure of these electrodes were analyzed by SEM and XRD. Electrokinetic parameters of these systems clearly indicate that methanol oxidation rates are almost comparable onto these electrodes. It is thus suggested to follow electrochemical route using surfactant as capping agent. Graphites are found to be better substrate than felt material. SEM pictures clearly indicate formation of highly dispersed catalytic particles (Pt) via electrochemical route.
B1.2: Catalyst Degradation II
509
Kenneth C. Neyerlin, Ratndeep Srivastava and Peter Strasser
Pt25Cu75 and Pt20Cu20Co60 electrochemically dealloyed electrocatalysts were shown to possess improved resistance to electrochemical surface area (ECSA) loss relative to commercially available Pt/HSC and Pt/Vu catalysts. The difference in ECSA loss was shown to be directly related to the temperature at which the alloy catalysts were prepared (i.e. reduced/annealed), with higher temperatures resulting in greater resistance to ECSA loss. To normalize for preparation conditions, commercially available catalysts were exposed to a heat treatment process mimicking the annealing/reducing procedure for the Pt alloys.
515
Peter Strasser, Zengcai Liu and Shirlaine Koh
Voltammetrically dealloyed Pt-Cu alloy nanoparticles show significantly improved Pt-mass and specific activities for the oxygen reduction reaction in acidic media in both RDE and MEA configurations. The active phase of the catalyst is prepared from very Cu-rich precursor materials which are formulated into catalyst inks and electrode layers. The high Cu content of the precursor materials raises fundamental and practical questions as to the molecular stability / oxidation state of the Cu rich catalyst surface and the shelf-life of precursor powders, inks and electrode layers. Here we present aging studies of a carbon-supported Pt25Cu75 nanoparticle catalyst precursor. We monitored how the surface area (ECSA) and the oxygen electroreduction (ORR) reactivity of dealloyed precursors (active form of catalyst) change as a function of the exposure time to air of the Pt25Cu75 precursor at room temperature. Similarly, we aimed to investigate how ECSA and ORR of the active catalyst changed with the time the liquid catalyst ink was exposed to air. We find little detrimental effect of air aging of the precursor on ORR activity over the time scales investigated. The effect of air aging of the catalyst inks is more complex, however. Initially, aged inks show increased ORR reactivity, that is, aged inks result in more active catalyst layers. After about 4-5 days of aging of the inks in air, however, we observed a drop in ORR activity of the resulting catalyst layers. This complex aging behavior of the inks seems independent of prior air aging of the dry powder precursor.
523
Lihong Huang, Jian Xie, Rongrong Chen, Deryn Chu and Andew Hsu
Nickel-based catalysts with iron promotion were prepared by impregnation, tested in auto-thermal reforming (ATR) of ethanol for hydrogen production. The reaction results show a remarkable improved durability in catalytic activity as well as selectivity to hydrogen in ATR is obtained: Over the 10 wt.% iron-loading nickel catalyst, conversion of ethanol at 99.61 % and selectivity of hydrogen around 115 % are kept at 600 C during a 30-hour test, while that of iron-free sample decreases sharply from 85.10 % to 19.71 % on hydrogen selectivity within a 26-hour test. The improved durability is attributed to the synergistic effect of the NiAl2O4-FeAl2O4 mixed crystals that are more resistant to sintering and oxidation in the oxidative atmosphere of ATR.
A1.2: Water and Thermal Management
535
Ivan Tolj, Mayssa Abdallah and Frano Barbir
Thermal behavior of a 1 kW, air cooled PEM fuel cell stack was analyzed and simulated. Operation of the stack under various scenarios was simulated such as start-up from room temperature, steady state at full and half load and sudden changes of load (from full to half load and reverse), under constant or variable flow rate of the cooling air. In variable power load operation, the stack temperature is not constant. One interesting finding of this analysis is that liquid water occurs at the outlet whenever the stack temperature falls below 60{degree sign}C, although the nominal operating conditions were selected such that there is no liquid water at the outlet at steady state operation. The results also indicate that this particular stack has insufficient heat exchange area with cooling air resulting in relatively large cooling air flow rates and low temperatures.
543
Aboubakr M. Abdullah, Takeyoshi Okajima, F. Kitamura and Takeo Ohsaka
The pH of the water drained out from the cathode and the anode sides was measured using a flow pH meter connected to the exits of the anode and cathode compartments and was found to depend mainly on the cell's operating conditions and the MEA's aging condition. Aged MEA operating at low temperature - low RH condition led to a significant increase in the acidity of the water drained out from the cathode side (pH 1.8). On the other hand, the water drained out from the anode side has a pH value of 4.8 on average. Reactions that might affect the pH of the water drained out from the PEM fuel cell were studied. Membrane degradation via hydroxyl radicals (⋅OH) was found to be the most influencing reaction that lowers the pH of water within PEM fuel cells.
551
Ahmet Kusoglu, Anette Karlsson, Michael Santare, Simon Cleghorn and William B. Johnson
Investigation into the durability of fuel cells is a challenging issue due to the large number of parameters affecting membrane electrode assembly (MEA) integrity. The mechanical stresses induced in the membrane due to swelling associated with water absorption play an important role in the long-term failure of the MEA. Thus, the stresses and the water distribution in the MEA are coupled. To better understand the relationship between mechanical stresses and water absorption, we introduce a numerical model to simultaneously determine the swelling-induced stresses and the water distribution in the MEA under various cell operating conditions. Preliminary results suggest that open-circuit voltage (OCV) operations lead to the most severe environment for the mechanical response, whereas under current load, the stresses and the permanent deformation are on average lower and localized at the cathode side of the MEA. The results suggest that the mechanical behavior of the MEA must be taken into account in the investigations of MEA degradation to establish a complete understanding on the failure mechanisms and durability.
563
Motoaki Kawase, Tatsuya Inagaki and Kouichi Miura
A nonisothermal model of the proton exchange membrane (PEM) fuel cell is developed with taking the through-plane heat and water transport into consideration. Local vapor-liquid equilibrium of water in the gas diffusion layer (GDL) is assumed. The steam pressure is determined only by temperature in the presence of condensed water. Only 1 oC temperature rise in GDL creates a steam flux corresponding to water generation at the current density of 0.74 A/cm2. Using stacked four PEM sheets, between which 20 μm thick thermocouples were inserted, the PEM temperature was measured in a cell having carbon paper GDLs, operated at 80 oC with hydrogen and oxygen supplied. About 1 oC rise in the PEM temperature was observed at a current density of 0.6 A/cm2. The effective thermal conductivity of the GDL was estimated from the experimental results. The temperature rise calculated by the one-dimensional numerical simulation well represents the experimental results.
575
Soowhan Kim and Matthew Mench
The objective of this work is to investigate water transport of polymer electrolyte fuel cell (PEFC) materials subjected to a temperature gradient. Experiments on different fuel cell materials (Nafion®, reinforced membrane, reinforced membrane electrode assembly (MEA), non-reinforced MEA, hydrophilic and hydrophobic diffusion media) were performed using an in-house fuel cell fixture with an imposed temperature gradient between the anode and cathode. Contrary to thermo-osmotic flow in fuel cell membranes (17, 18), a net flux of water was found to flow from the hot to cold side of the fuel cell. The key to this is the existence of some gas phase in the catalyst layer or other porous media. This mode of transport can be explained by a phase-change driven flow, also known as a heat pipe effect. The measured water transport through the membrane electrode assembly is the net effect of mass diffusion as well as thermo-osmosis in the membrane, which moves counter to the direction of the phase-change driven flow. The net flux of water was fit by Arrhenius functions that are dependent on material set, temperature gradient, and average temperature across the materials. In addition to direct quantification, the phase-change driven flow was visualized and confirmed using high resolution neutron radiography.
587
Felix N. Buechi, Reto Flückiger, Denis Tehlar, Federica Marone and Marco Stampanoni
The local saturation in porous transport layers (PTL) has been determined using synchrotron-based x-ray micro-tomography. The water distribution inside the porous structure could be resolved on the scale of the pores. After phase segmentation of the image data, the measurement of the liquid saturation as function of the through plane coordinate of the PTL and the capillary pressure was possible. For verification, first experiments with complete cells are also shown.
C1.2: In–situ Structure and Morphology
595
Mike Toney, Shirlaine Koh, Chengfei Yu and Peter Strasser
X-ray diffraction (XRD) and small angle X-ray scattering (SAXS) are methods that are used to characterize the atomic structure and particle size of nanoparticle electrocatalysts. These methods do not inherently provide element specific information on structure and particle size. However, with the use of an anomalous scattering approach, one can obtain element specificity. This contribution describes these methods and applies these to fuel cell nanoparticle catalysts.
D1.2: Catalysts for Acidic Direct–Fuel Fuel Cells
605
Xirong Jiang, Friedrich Prinz and Stacey Bent
Using rf co-sputtering, we have successfully deposited Pt-Ru catalysts of well controlled Ru content over a wide range of compositions. The surface morphology of the films, acquired from scanning electron microscopy studies, is very rough and nanoporous. The structure of the films has been verified as polycrystalline by x-ray diffraction analysis. The electrochemical behavior of the electrodes has been characterized using chronoamperometry with methanol oxidation as the probe reaction in a H2SO4/MeOH electrolyte at room temperature. The results indicate that the optimal stoichiometry of the alloys measured in 1 M MeOH and 16.6 M MeOH is Ru0.24Pt0.76 and Ru0.46Pt0.54, respectively. These alloys have an onset potential 0.2 volt lower than pure Pt.
613
Wenming M. Wang, Zhilin L. Li, Zhiqing Zou, Hui Yang and Songlin Feng
We report one-step synthesis of Pd-rich carbon-supported Pd-Pt alloy electrocatalysts of different Pd/Pt atomic ratios with and without the addition of trisodium citrate as the complexing agent and stabilizer. An activity comparison of the oxygen reduction reaction (ORR) on the Pd-Pt/C catalysts with the same fcc structure and a similar particle size has been investigated. The Pd3Pt1/C catalyst exhibits the highest ORR activity among all the alloy catalysts prepared with the addition of trisodium citrate and a comparative ORR activity with the Pt/C. However, the Pd3Pt1/C catalyst prepared without the addition of trisodium citrate shows an enhanced ORR activity in comparison with the Pt/C. All the bimetallic catalysts exhibited much higher methanol tolerance during the ORR than the Pt/C catalyst. The high methanol tolerance of the Pd-Pt/C alloy catalysts during the ORR may be ascribed to a composition effect and to the formation of Pd-based alloys.
621
Liney Arnadottir, Hannes Jo´nsson and Eric M. Stuve
Two forms of the reaction intermediate with H:C:O stoichiometry were studied on Pt(111) using density functional theory. Three cases were studied: the intermediate on a clean surface, the intermediate and one water molecule on the surface and the intermediate with a water bilayer. Both the H-C=O (formyl) and C-OH (hydroxmethylidyne) configurations were found to be stable on clean Pt(111) and when coadsorbed with a water molecule. Interconversion between the two configurations was studied using the nudged elastic band method. On the clean surface interconversion between the two forms goes through COads and Hads intermediates, meaning that, although both HCO and COH are stable on the clean surface, they will not interconvert. In the presence of a single coadsorbed water molecule the activation barrier for interconversion from HCO to COH was found to be 0.62 eV. The HCO configuration is stable in the presence of a water bilayer, but the COH configuration dissociates to COads and Hads. These results suggest that, in the presence of water, the HCO form will be the only stable form of the reaction intermediate of H:C:O stoichiometry.
627
John L. Haan and Richard I. Masel
Recent progress in studies on the direct formic acid fuel cell reported here includes improvements to the anode catalyst and analysis of the impact of pH on reaction rate. We demonstrate that several adatoms can be underpotentially deposited to the surface of the palladium anode catalyst to improve the oxidation of formic acid. Antimony and lead adatoms show strong improvement to operation of the fuel cell. We also demonstrate that the solution pH has a strong effect on the reaction rate in a nearly irreversible reaction (formic acid oxidation). We eliminate the effects of adsorbed surface species and conclude that the change in pH results in a change in thermodynamic driving force that is evidenced by a remarkable increase in reaction rate with increase in pH.
639
Kristian Noel and Xin Wang
Highly active Pt-decorated Au nanoparticles on carbon support was successfully synthesized based on successive reduction strategy. The electrocatalytic activity of this decorated structure toward formic acid oxidation unexpectedly increases despite the low amount of Pt being used. The enhancement is attributed to the less Pt ensemble sites that the decorated structure possesses (ensemble effect) and the increase in the Pt atom reactivity on Au nanocrystal (electronic effect).
647
Régis Chenitz and Jean-Pol Dodelet
Single MEA direct formic acid fuel cells were assembled using various anode diffusion electrodes and various Nafion/Pd black ratios for the catalyst layers. Power densities above 100 mW cm-2 were obtained at room temperature with 10 M formic acid fed to the anode and O2 at atmospheric pressure fed to the cathode. The best results were obtained when untreated carbon cloth was used as the anode diffusion layer and with a catalyst layer composed of equal volumes of Nafion and Pd black electrocatalyst. We have also observed increased performance of the MEA when the flow of formic acid is drastically reduced, probably due to a better evacuation of CO2; the gas produced at the anode due to the oxidation of formic acid.
B1.3: Catalyst Contamination I
659
Susanne Dorn, Guido Bender, Keith Bethune, Michael Angelo and Rick Rocheleau
The impact of fuel impurities toluene (C7H8) and carbon monoxide (CO) on the performance of polymer electrolyte membrane fuel cells (PEMFCs) was investigated. Single and mixed impurities were injected into the fuel cell via the anode feed stream. Experiments were accompanied by gas chromatography analysis to determine the conversion and reaction processes occurring during contaminant exposure. Impurity injections of 2 and 20 ppm C7H8 caused an insignificant overpotential change of 2 and 8 mV respectively. An almost complete conversion of C7H8 to methylcyclohexane (C7H14) was observed. Impurity injections of 2 ppm CO caused a significant overpotential change of 247 mV. At steady state conditions more than 60% of the injected CO was converted to CO2 in the fuel cell. When the impurities were injected into the anode feed stream as a mixture the overpotential change was 100 mV greater than the sum of the overpotential changes the single impurities caused .Hydrogenation of C7H8 to C7H14 was observed but in contrast to the single C7H8 impurity experiment it stopped when a certain CO coverage was reached. The strong adsorption of CO caused a competition between the hydrogen reduction reaction and the hydrogenation of C7H8 for the available reaction sites.
669
Michael Angelo, Guido Bender, Susanne Dorn, Keith Bethune, Tim Hossain, Dan Posey, Jerzy Gazda, Amiya Ghatak-roy and Rick Rocheleau
In this paper, we report the effects on cell performance and durability of repeatedly poisoning the anode catalyst of a proton exchange membrane fuel cell (PEMFC) to 2 ppm carbon monoxide (CO) in the hydrogen fuel. The experiments were designed to simulate repeated exposure to low level impurities as may be experienced in a dynamically operated PEMFC. Experiments were conducted over a period of 1000 hours and accompanied by weekly diagnostics to characterize detailed changes in performance. Results for the repeatedly poisoned cell were compared to those of a control cell which was operated identically but without CO in the anode feed stream. Two effects were observed: the electro-chemically active area (ECA) of the test cell anode decreased significantly during the initial 300 hours of the experiment and the hydrogen crossover rates increased by a factor of 67 by the end of the experiment. Both effects contributed to performance losses, while the latter also indicated the end of life for the membrane electrode assembly (MEA). The results of the experiments emphasize the impact low level CO contaminant may have on MEA lifetime and cell performance under dynamic conditions.
677
Jean St-Pierre
A mathematical model is derived describing the effect of an electroactive contaminant on the catalyst surface. Two cases are considered and characterized by different rate determining steps: contaminant reaction and contaminant product desorption. Each case leads to a closed form solution for the transient and scaled current density either during the contamination or recovery process. The model was partially validated using proton exchange membrane fuel cell (PEMFC) data obtained by operating with hydrogen contaminated with small amounts of CO. Results suggest the use of well designed experiments to minimize artifacts and additional model validation using a wider range of operating conditions.
C1.3: Hydrocarbon Membranes
689
Hossein Ghassemi, Ram Subbaraman, Christopher Brockman, Brandon Pyle and Thomas Zawodzinski
Sulfonated poly(ether sulfone) (SPES) copolymers with a degree of sulfonation higher than 30% show high proton conductivity (> 60 mS/cm) as well as a high extent of swelling. Two methods were considered to decrease the swelling and improve dimensional stability. First, composite membranes were prepared by blending SPES and polyacrylonitrile (PAN) and annealing under nitrogen at 280 oC. In a second approach, SPES was blended with polysulfone (PSU) and heated at 260-280 oC to form sulfone crosslinks in the membrane. The membranes prepared by these methods showed significantly lower swelling in water and methanol with minor decreases in conductivity.
699
Andrew M. Herring, James L, Horan, Mei-Chen Kuo, Steven F. Dec, Matthew H. Frey, Anitha Genupur, Lucy Ren, Mike A. Yandrasits and Stephen J. Hamrock
The heteropoly acids (HPAs) are a class of inorganic oxides that have some of the highest solid state proton conductivities known at room temperature. At elevated temperatures proton diffusion coefficients in these crystalline materials increase, but, not all the protons are mobile resulting in a decrease of the observed proton conductivity. The proton conductivity in these materials is heavily dependant on the hydration state of the HPA. In order to develop new PEMs based on the HPAs for elevated temperature, dry operation, it will be necessary to both immobilize the HPA and ensure that all of the protons are mobile all of the time. If both these objectives can be obtained a new class of PEMs will be developed that could facilitate the use of PEM fuel cells in automotive applications. We have created a new class of PEM by polymerizing HPA monomers with appropriate co-monomers to produce films with unique proton conducting properties.
705
Clovis A. Linkous, Stephen L. Rhoden, William G. Linkous, Benjamin P. Pearman and Nahid Mohajeri
Water uptake is an important attribute of all membrane electrolytes, as it is related to mechanical strength, creep, and dimensional stability. Thus some means of controlling water uptake by a hydrophilic sulfonic acid polymer is desirable. This is particularly important for SPEEK, which at high degrees of sulfonation (i.e., low equivalent weight) has demonstrated substantial water uptake, on order of 10's of water molecules per sulfonic acid unit. We have attempted to control water uptake in SPEEK membranes by performing cross-linking reactions on the finished polymer. Water-soluble SPEEK (85% degree of sulfonation, or 418 g/eq EW), 1,4-benzenedimethanol, and various transition metal chloride catalysts were cast together to form a membrane that was heated at 200 oC for 10 min. The resulting insoluble membrane was shown to have conductivity comparable to an uncross-linked SPEEK membrane over a range of relative humidities.
C1.4: Pt Catalysts I
713
Tatsuya Takeguchi, Guoxiong Wang, Ernee Muhamad and Wataru Ueda
PtRuSnO2/C catalyst was prepared by the ethylene glycol method to improve the CO tolerance for polymer electrolyte membrane fuel cell. The prepared catalysts were characterized by X-ray diffraction (XRD), scanning transmission electron microscopy (STEM), CO stripping voltammetry and single cell performance measurements. Based on XRD and STEM results, PtRuSnO2/C catalyst exhibited a slightly smaller particle size than PtRu/C catalyst due to the addition of SnO2. CO stripping voltammetry showed that SnO2 promoted CO electro-oxidation on PtRuSnO2/C catalyst at low potential. And PtRuSnO2/C catalyst gave a better single cell performance under 500 ppm CO-contaminated H2. These results suggested that the performance improvement was due to the combined promotional effect of SnO2 and Ru species on Pt for CO tolerance.
Poster Session
719
Haolin Tang and Sanping Jiang
A novel conception of inorganic proton exchange membrane for elevated temperature PEM fuel cell was proposed in this research. The inorganic electrolyte was approached by trapping heteropolyacid (HPA) molecules inside mesoporous silica structure via a self-assembly route assisted with a structure-directing surfactant, and then construct an inorganic membrane based on mesoporous silica matrix and HPA proton conducting sites. Such mesoporous HPA/silica significantly enhance the stability of HPA molecules, and provided continuous proton transfer channels with diameter of 3~4 nm, resulting high proton conductivity of about 0.05 S/cm at 300oC. A PEMFC based on the mesoporous HPA/silica inorganic PEM and a non-platinum cathode catalyst achieved a power density of 102 mW/cm2 at 300oC, closing to the performance of the cell with Pt catalyst at temperature of 80 oC.
729
P.S. Pa
The purpose of this research is to apply proton membrane fuel cells to toys, and assess its feasibility. The study uses Taguchi Methods to analyze the "Proton Exchange Membrane Fuel Cell Power Supply and Work Module for Toys". The study assembled the proton exchange membrane fuel cell power supply module in the "Toy of Hydrogen-based Energy Module-Ship of Hydrogen-based Energy" and observes its operation state. It finds that the ship moved forward smoothly, and indicates that hydrogen can be used for this toy. This study uses renewable "Solar Energy" matching "the Proton Exchange Membrane" to design the "Hydrogen and Oxygen Fuel Module", which creates the hydrogen and oxygen fuel supply for the "Proton Exchange Membrane Fuel Cell Power Supply and Work Module" for toys using hydrogen-based energy. "Hydrogen-based Energy" will become applied extensive to the toy field in the future by way of this study.
741
Yuichi Tamura, Kento Taneda, Mikito Ueda and Toshiaki Ohtsuka
PtCo and PdCo alloy electrodes were investigated in a 0.5 M sulfuric acid solution by electrochemistry, ellipsometry, laser Raman scattering spectroscopy, XPS, and GD-OES. The corrosion resistibility of Pt-Co and Pd-Co alloys decreased with increase of Co addition. The increase of Co addition, however, enhanced the catalytic efficiency on the ORR. The alloy surfaces may be covered by CoOOH and Pt or Pd oxide 2-3nm thick. At the potential of 1.2V vs. Ag/ AgCl/ sat. KCl, the thickness of oxide film increased with the Co addition. The presence of the oxide film on the alloy electrodes increases the overvoltage for the ORR. The effect of the oxide thickness on the ORR was discussed.
751
Masashi Matsumoto, Takashi Manako and Hideto Imai
The corrosion of highly oriented pyrolytic graphite (HOPG) model electrodes' surfaces with platinum nanoparticles and oxygen molecules in an aqueous solution was investigated using electrochemical scanning tunneling microscopy in order to understand the degradation of carbon supports found in polymer electrolyte fuel cells (PEFCs) cathode electrode. Structural changes of HOPG surfaces with platinum nanoparticles and oxygen due to the corrosion were observed directly at atomic levels under the real conditions at which PEFCs operate. The STM observations revealed that the graphite surface oxide formation due to corrosion of the HOPG surfaces with platinum nanoparticles occurred initially at step edge sites, i.e., at defect sites and then grew toward terraces. This indicates that platinum particles and oxygen on the HOPG surface accelerated the corrosion. Surface oxygen species formed through the partial oxidation of water and the dissociative adsorption of oxygen molecules likely enhance the oxidation rate of graphitic oxide species.
761
S. Fraire Luna, F.J. Rodriguez Varela, R. Dabek and O. Savadogo
We studied the performance of carbon-supported Pd cathode electrocatalysts in O2-saturated acid solution containing ethanol. The Pd/C electrocatalysts showed an important selectivity toward the Oxygen Reduction Reaction (ORR), and a very high degree of tolerance to poisoning due to the presence of the alcohol. A negative shift in onset potential for the ORR of only 10 mV for a 20% Pd/C electrocatalyst in 0.5M H2SO4 + 0.125M C2H5OH electrolyte was measured, whereas the shift for a 20% Pt/C electrocatalyst was of 398 mV in the same solution. Similar high tolerances were established at increasing C2H5OH concentrations for Pd/C.
769
Gen Inoue, Yosuke Matsukuma and Masaki Minemoto
It is important to investigate the two-phase condition in PEFC gas diffusion layer (GDL) to improve mass transfer rate. In order to calculate liquid and heat transfer in heterogeneous GDL, the multi-calculation network model which consists of pore section and fiber section was developed on the basis of the structure of simulated GDL. And the influence of the temperature distribution on the condition of staying liquid water was examined by this model for internal condensation. As a result, it was found that the nonisothermal calculation was indispensable to examine the condition of liquid water in detail. In addition, the conditions of staying liquid water and the cell voltage were differed by each contact angle, and it was found that the performance of mass transfer was affected by not only the value of saturation but also the effective pore structure formed by staying liquid water.
779
Koichi Asano, Yoshiriho Mugikura and Takao Watanabe
The degradation of the Pt catalyst layer of polymer electrolyte fuel cells was studied for pressurized conditions. The cell performance loss under pressurized conditions was observed to be smaller than that under normal pressure conditions. A clear loss of Pt was observed at the cathode at the point of contact with the electrolyte and a Pt band was conspicuously formed in the membrane under pressurized conditions. Thus, a serious degradation was found to occur in the Pt catalyst layer under pressurized conditions.
787
Masakazu Yoneda, Masato Takimoto, Eiji Ejiri and Sheiichi Koshizuka
The behavior of liquid water transport process into the GDL is investigated by direct numerical simulation as well as experiment using X-ray computed tomography. As a result, it is possible that liquid water adjacent to the MPL is transported as mist which can pass through the small-pores by Brownian motion. Furthermore, the effect of the MPL on a PEFC performance under both dry-out and flooding condition could be elucidated by a hypothesis about the water transport mechanism involving the Kelvin effect inside the hydrophobic mesopore inside it.
795
Jae-Hyuk Lee, DongHyun Peck, Sang-Kyung Kim, Seong-Yop Lim, Doo-Hwan Jung, Sung-Hyeon Baeck and Jae-Hyuk Jang
Membrane electrode assemblies (MEA) for direct methanol fuel cell (DMFC) were prepared using PtRu/C (70 % Pt alloy base) and Pt/C (75 % Pt alloy base) as their anode and cathode catalysts, respectively. The anode and cathode catalyst layer were coated by using semi-automatic bar-coating method, which can prepare the catalyst layer with uniform thickness. To study the effect of Nafion contents on performance, MEA in which Nafion ionomer contents were used (20 wt.%, 35 wt.%, 40 wt.%) was fabricated. And surface and cross-section morphologies of the catalyst layers were observed by SEM. The performances and resistance of the MEAs were investigated through a single cell evaluation.
801
Young-Chul Park, DongHyun Peck, Doo-Hwan Jung, SangKyung Kim, Seong-Yop Lim, Bong-Do Lee, Jae-Hyuk Jang and Dokyol Lee
We have developed very small direct methanol fuel cell stack for mobile devices. The stack was designed with the total size of 48 mm × 50 mm × 17 mm (volume: ~ 40.8 cc) and it consisted of 6 cells and each cell has an active area of 13.7 cm2. The maximum power output of the stack is 7.63W (1.81V @ 4.22A) and the nominal power output of the stack was 5.49W (2.4V @ 2.29A) at 2.4V (0.4 V/cell). In this work, we studied starting characteristics of 5W class small DMFC stack and effects of methanol/air stoichiometry on the stack performance at constant current.
807
Daichi Imamura
The Pt/C catalyst of polymer electrolyte membrane fuel cell (PEMFC) was poisoned by 5 ppm of hydrogen sulfide for 5 hours at potentials of 0V, 0.3V, 0.6V and 0.9V vs. RHE, and the catalyst was characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and X-ray absorption spectroscopy (XAS) analysis. Only diffraction peaks of Pt, carbon and ionomer were observed in all samples, and the crystallite size of Pt was about the same after poisoning. In the XPS and XAFS analyses, accumulation of sulfur species on Pt/C catalyst and oxidation of Pt were observed in the samples poisoned at 0.3V and 0.6V.
817
Hiroshi Fukunaga, Y. Kabaya, T Tatatsuka and K. Yamada
The microstructure and the elementary steps of the direct methanol fuel cell (DMFC) anode are investigated using an advanced equivalent circuit. A serial circuit of two parallel circuits of resistance and capacitance, which is in parallel with a Faradaic impedance, is introduced to simulate the anodic reaction. Three processes with different anode polarization dependencies are clearly reproduced by the simulation using this equivalent circuit, and they are considered to be interfacial resistance representing the transport of ions through the electrode pores, electrooxidation reaction of the anode, and another process parallel to the reaction intermediate. The anode polarization dependence of the interfacial resistance and the change in the distortion was better explained by the modified equivalent circuit than by the conventional equivalent circuit using a constant phase element (CPE) with unfixed exponent. The relationship of the interfacial resistance with catalyst loading or electrode thickness was clarified using this equivalent circuit.
825
Kwan Soo Lee, Yu Seung Kim, Bryan Pivovar and Jae-Suk Lee
Partially fluorinated poly(arylene ether) copolymer having reactive functional group are used to fabricate the MEA to improve the interfacial adhesion between membrane and electrode. The optimum MEA processing procedure was studied using different hot pressing temperature and crosslinking. Good interfacial adhesion between hydrocarbon membrane and Nafion bonded electrode produced excellent fuel cell performance which was comparable to the MEA using Nafion 212.
831
Krzysztof A. Lewinski, Andrew J. Steinbach, Susan M. Hendricks and Darren R. Miller
The fuel cell community has by now wholeheartedly accepted the notion of matched MEA components as necessary ingredients of fuel cell performance and durability equation. Considerable research has been conducted on optimizing the combined properties of the gas diffusion layer backing and microporous layer, catalyst and ionomer. The same logic seems to be quite universally applied to interplay between stack components and MEAs, but direct evidence as to why this would be so has not been researched or publicized widely. In this work we attempt to show such link does indeed exist, and to back up our claims with experimental data.
841
Hisatoshi Fukumoto, Shoji Yoshioka and Shuichi Matsumoto
In-plane induction currents in electrodes and bipolar plates by reactant fed into a PEFC were evaluated using a 20-segmented cell. When hydrogen was fed into anode in the condition of anode (negative electrode) and cathode (positive electrode) exposed air, in-plane currents were detected in both electrodes in spite of the open-circuit condition. In-plane currents of anode and cathode in each segment had each other opposite direction and nearly equal quantity. Simultaneously, carbon dioxide and oxygen were also detected in the cathode exhaust.
849
Hidemitsu Aoki, Tomohiro Nitta, Susumu Kuwabata, Chiharu Kimura and Takashi Sugino
We attempt to develop high-performance and safe fuel cells using ammonium formate (HCOONH4) as a solid (powder) fuel. The ammonium formate with high deliquescence can be easily supplied as a fuel through a porous film in high humidity. This solid fuel has the potential to realize safe portability compared with liquid fuels such as methanol from the viewpoint of toxicity and flammability. We have found that oxidation of ammonium formate can be improved by the addition of Palladium (Pd) catalysts to Pt catalysts. There is a high potential for the use of ammonium formate as a solid (powder) fuel for polymer electrolyte membrane (PEM) fuel cells.
855
Yang-Chih Hsueh, Chia-Te Hu, Chih-Chieh Wang, Chueh Liu and Tsong-Pyng Perng
Platinum nanoparticles were formed on oxygen plasma treated carbon nanotubes by atomic layer deposition (ALD). The treatment time of oxygen plasma generated by a microwave plasma enhanced chemical deposition system varied at 5 s to 20 s under a power of 600 W. The reaction cycle number was controlled at 50-125 and the length of pulse time for Pt precursor, O2 and N2 were set at 1 s, 5 s and 20 s, respectively. It was observed that formation of uniform and well distributed Pt nanoparticles was achieved. Furthermore, the growth rate of Pt nanoparticles could be controlled by altering the reaction cycle number and oxygen plasma treatment time. X-ray photoelectron spectroscopic analysis indicated that oxygen plasma could graft oxygen-containing functional groups to the CNTs surface, to act as the nucleation sites for growth of Pt nanoparticles.
863
Dongsoo Ko, Cheoreon Moon, Jangsik Yang, Jihwan Jeong, Gyungmim Choi and Duckjool Kim
In this study, local temperature in a membrane electrode assembly (MEA) and performance of a proton exchange membrane fuel cell (PEMFC) are investigated by numerical studies and experiments. The performance of a lab-scale PEMFC is measured with the load changes for three different cell temperatures (40°, 50°, and 60°) at a relative humidity of 100%. In order to observe the local temperature in the MEA and analyze the performance of the PEMFC, the numerical studies using the CFD module of STAR-CD, which are based on experimental data, are conducted. The results show that the cell condition at a cell temperature of 50° gives the highest performance and the maximum temperature in the MEA dramatically increases with increasing cell temperature and current density. These results might be used to design the PEMFC system and channel flow-field.
873
Yunfeng Zhai, Guido Bender, Susanne Dorn, Michael Angelo, Keith Bethune and Rick Rocheleau
In this paper, we report on the effects of 1, 2, and 10 ppm SO2 injected into the cathode feed stream of a PEMFC that was operated at a constant current of 0.6 A/cm2. All experiments showed significant performance degradation before concentration dependent steady state poisoning conditions were reached. The poisoning process was identified as a 2-step process, indicated by an inflection of the voltage degradation. Cell voltage recovery by neat H2/air operation was incomplete, but independent on contaminant concentration. Subsequent CV stripping indicated that sulfur species remained on the catalyst surface during the self-induced recovery. The CV scans also showed features which developed due to SO2 exposure that were reported for Pt/Pt systems in sulfuric acid solution.
881
Yuichi Takamura, Eiji Nakashima, Hirohisa Yamada, Akimasa Tasaka and Minoru Inaba
Oxygen permeation in Nafion®117 and sulfonated poly(arylene ether sulfone) (BPSH-50) were investigated at different temperatures and relative humidities by a potential step method using a Pt microelectrode. The diffusion coefficient increased, while the solubility decreased with an increased in temperature and relative humidity for both samples. Consequently, the permeability increased with an increased in temperature and relative humidity for both samples. The permeability in BPSH-50 was approximately four times lower than that in Nafion®117, due to a smaller diffusion coefficient and a lower solubility in BPSH-50 than those in Nafion®117. Mass transport of oxygen in these membranes was correlated with microstructural changes of the membranes.
891
Morihiro Saito, Yoshinobu Saito, Takayuki Konishi, Hideki Kawai, Jun Kuwano, Hidenobu Shiroishi and Yoshiharu Uchimoto
To explore new electrocatalysts for alkaline DAFCs, oxygen reduction reaction (ORR) activity of the pyrochlores Ln2Ru2O7-d(LnR, Ln=Pr,Nd,Sm,Gd,Dy,Yb) and Ln2Ru2-xMnxO7-d(LnRMnx, Ln=Pr,Nd) were examined in 0.1 M KOH at 70oC. The onset potential (Eon) of the ORR current and the efficiency (Eff4) of 4-electron ORR were evaluated by semi-steady state voltammetry with rotating ring-disk electrodes. In the LnR series, PrR with the highest ORR activity showed Eon = 0.85 V vs. RHE and Eff4 above 90 %. Their Eon and Eff4 values revealed that LnR with a smaller atomic number had a higher ORR activity. In addition, effects of Mn substitution for the Ru-site were confirmed in both PrRMnx and NdRMnx series. The NdRMn0.25 exhibited the highest ORR activity (Eon = 0.95 V and Eff4 above 90%) in the pyrochlore single phase. The Eon value kept unchanged even in 0.1 KOH containing 1 M methanol, ethanol, ethylene glycol and 2-propernol.
901
Yu-Fan Chiu, Li-Chung Chang, Pu-Wei Wu and Yu-Chi Hsieh
Fabrication of PtRu nanoparticles was conducted by a galvanostatic pulse electrodeposition technique. We studied various deposition parameters including current on-time and off-time, current density, as well as concentrations for the Pt and Ru precursors in the plating bath in order to determine the optimized process condition for the highest methanol oxidation ability. Cyclic voltammetric profiles were obtained in electrolytes of 0.5 M H2SO4, and mixture of 0.5 M H2SO4 and 1.0 M CH3OH to determine characteristics in the hydrogen absorption/desorption and peak currents in the anodic/cathodic scans. We observed that a shorter current off-time resulted in better catalytic abilities when the Pt precursor concentration was increased. Partial dissolution of Ru in the as-deposited PtRu nanoparticles during the current off-time might be responsible.
913
Xu Zhang, Datong Song, Qianpu Wang, Cheng Huang and Zhong-Sheng Liu
A two-dimensional, non-isothermal two-phase model, which includes the full anisotropy of GDL, was developed to investigate the effect of anisotropic ratios on cell performance. Among the four anisotropic ratios, the anisotropic ratio of diffusivity,γD, is the most sensitive parameter to cell performance. The present study demonstrated the possibility of improving cell performance by using innovated GDL porous materials with higher anisotropic ratios, especially higher γD
925
Shin-ichiro Imabayashi, Yoko Kondo, Ryotaro Komori, Akihiko Kawano and Takashi Ohsaka
The effects of the atmospheric trace species (SO2, Cl-, NH3) on the formation of H2O2 accompanying the O2 reduction reaction (ORR) have been elucidated in 0.1 M HClO4 using rotating ring-disk Pt electrode methodology. The potential at which the ORR starts shifts to the negative direction and the amount of formed H2O2 increases concomitantly as the amount of added SO2 or Cl- increases, although Cl- less affects. The extent of the H2O2 formation is correlated to the coverage of SO2 or Cl- which was estimated from the decrease in the area of a hydrogen desorption peaks. This suggests that the adsorption of SO2 or Cl- on Pt reduces the number of the adjacent adsorption sites necessary for breaking of the O-O bond and then enhances the production of. No effect on the ORR activity and the H2O2 formation was observed for NH3.
931
In Dae Choi and Donggeun Lee
Carbon black, activated carbon and carbon nanotube have been used as supporting materials for precious metal catalysts used in fuel cell electrodes. One-step flame synthesis method is used to coat 2-5nm Pt dots on flame-generated carbon particles. By adjusting flame temperature, gas flow rates and resident time of particles in flame, we can obtain Pt/C nano catalyst-support composite particles. Additional injection of hydrogen gas facilitates pyrolysis of Pt precursor in flame. The size of as-incepted Pt dots increases along the flame due to longer resident time and sintering in high temperature flame. Surface coverage and dispersion of the Pt dots is varied at different sampling heights and confirmed by Transmission electron microscopy (TEM), Energy-dispersive spectra (EDS) and X-ray diffraction (XRD). Crystalline and surface bonding groups of carbon are investigated through X-ray photoelectron spectroscopy (XPS) and Raman spectroscopy. The electro-catalytic property of Pt/C composites for the application to catalytic electrode PEMFC are also investigated by Cyclic voltammetry (CV).
937
Atsuko Y. Nosaka and Yoshio Nosaka
Water molecules confined in perfluorinated ionomer membranes which are extensively used for polymer electrolyte fuel cells, presented characteristic 1H NMR spectra reflecting the difference in the morphology. For the hydrated membrane the water molecules at the distinct segments of the polymer undergo rapid exchange to give an apparent single signal. The signal shifts to the higher field with increasing the water content due to the increase of the fraction of the bulk water molecules. On shortage of bulk water the morphological conversion takes place. The membrane of such morphology exhibits a spectrum with separated regions at room temperature regardless of the water content, since the morphology prohibit the rapid exchange among the water molecules localized at the distinct segments. The characteristic spectral changes of water molecules associated with the chemical exchange among the water molecules in the different water domains and the change of the polymer morphology were demonstrated
945
L. Kim, Chul Goo Chung, Young Wook Sung and Jong Shik Chung
In order to verify the dissolution mechanism of Pt in the electrode of proton-exchange membrane fuel cell (PEMFC), the distributions of migrated platinum particles in the electrolyte membrane were investigated. The migrated platinum was observed by transmission electron microscope (TEM) after long-term operations under various conditions. Experimental results show that a large amount of Pt can be dissolved from cathode by chemical oxidation under excess O2. The distribution and particle size of migrated Pt are strongly dependant on H2 and O2 partial pressures. Possibility of Pt dissolution from anode is also appeared from observation of the MEA operated under lean H2 condition.
955
Takuro Iwanaga, Satoko Takase and Youichi Shimizu
Electrocatalytic properties of various pyrochlore-type oxides (A2-xA'xB2O7−Z: A = Pb, A' = Pb, Bi, Sb, In; B = Ru) synthesized by a co-precipitation method were systematically investigated for oxygen reduction, hydrogen oxidation and tolerance of CO poisoning for the electrocatalyst of the polymer electrolyte fuel cell. Most of the pyrochlore-type oxides could be synthesized by the co-precipitation method at 380 - 600oC in aqueous solutions. The electrode containing Pb1.9In0.1Ru2O7-Z prepared at 380oC indicated high oxygen reduction activity, 181mA/cm2 at +0.4 V vs. RHE in 2N H2SO4. In addition, hydrogen oxidation current density of Pb2Ru2O7-Z was 117mA/cm2 at 0.2V vs. RHE in same solution. Pb1.9M0.1Ru2O7-z (M = In, Sb, Bi, Pb) oxides indicated rather high oxygen reduction activity in the order of M= In > Sb > Bi > Pb.
961
Jutae Kim, Junhee Lee, Gibaek Lee and Yongsug Tak
Fuel starvation during start-up and shut-down processes affected the performance of proton exchange membrane fuel cell significantly. Fuel starvation was intentionally made by supplying hydrogen and air into anode side alternatively and the individual electrode potential was in-situ measured with dynamic hydrogen electrode (DHE). Cathode potential was raised up to 1.6 V when air / hydrogen boundary developed on anode side. The development of high cathode potential caused the oxidation of carbon support and the amount of CO2 evolution is proportional to the cathode potential above 1.0 V. Above ~1.2 V, CO was electrochemically generated and a small amount of SO2 was formed above ~1.3 V. Although higher cathode potential was induced irrespective of cell temperature, the oxidation of carbon support is remarkably retarded at low temperature.
969
Ion C. Halalay, Belabbes Merzougui and Andrew Mance
The performance of the perfluorinated sulfonic acid polymer electrolyte membrane in PEM fuel cells degrades through a multi-step process: (i) hydroxyl radicals attack on the fluorinated polymer with the release of fluoride ions; (ii) corrosion of the plates and alloy catalysts by the fluoride anions, with the release of base metal cations; (iii) generation of more hydroxyl radicals through Fenton's reaction catalyzed by the metal ions. While fluoride ion release can be greatly reduced through the inclusion of cerium, manganese or sodium ions into the PFSA polymer membrane, we present here an alternative approach for mitigating the membrane degradation. We propose three chemical methods for increasing the overall durability of the fuel cell by interfering with each step of this degradation cycle: the uses of (i) hydroquinones, to neutralize hydroxyl radicals, (ii) aza-crowns for sequestering fluoride anions, and (iii) crown ethers to sequester base metal cations.
A2.1: Diagnostics
985
Xiao Zi Yuan, Elton Gu, Colin Sun, Haijiang Wang, Jinfeng Wu and Jonathan Martin
In this work, local current distribution was investigated by temperature mapping without disturbing the operation of a diagnostic modeling cell. A temperature mapping ramp was measured using micro-thermocouples embedded into the anode plate of the modeling cell. Then, the current distribution was calculated based on the relation between current and heat generated from the reaction, and the assumption of the adiabatic condition. The effects of different operation conditions on current distribution were also investigated. The results show that the temperature derivative tends to increase along the flow field from the inlet to close to the outlet and then decrease under various conditions. This trend is exactly opposite to that of the local voltage distribution. We conclude that local current distribution depends on not only the flow field design but also the local voltage distribution.
995
Wei Zhu, Zachary W. Dunbar and Richard I. Masel
Micro CT was used to look through the graphite flow channels to provide accurate pictures of water inside of an operating PEM fuel cell. Water was observed emerging as water droplets on the surface of gas diffusion layer. Drops in both hydrophobic and hydrophilic flow channels were found to distort from the expected spherical shape before they started to move. However, drops in hydrophobic flow fields did not detach from the diffusion layer before moving, whereas water in the hydrophilic channel formed a thin water layer at the bottom of the channel. This is believed to be due to the role of the channel side walls, as well as possible non-uniformities in the flow channel surface.
1001
Zachary W. Dunbar and Richard I. Masel
Water management remains a significant challenge for the commercialization of PEM fuel cells. Many mathematical models have been created to gain insight into the effects of water distribution on cell performance. However, model verification remains difficult due to the challenging nature of acquiring relevant experimental data about water generation and movement inside an operating fuel cell. In this work, magnetic resonance imaging (MRI) is demonstrated as a strong diagnostic tool to gather information about water generation and transport inside an operating PEM fuel cell. The MRI technique is used to gather quantitative water distribution data in three dimensions. Acquisition times are as fast as 8 seconds, allowing observation of dynamic processes within the flow channels. Flow channel depth, geometry and hydrophobicity are varied, and the effect on water distribution and overall cell performance measured.
1009
Tetsuya Mashio, Atsushi Ohma and Kazuhiko Shinohara
An advanced in-situ analysis technique for evaluating the reactant gas partial pressure at the catalyst layer/polymer electrolyte membrane (CL/PEM) interfaces has been developed using a Pt probe inserted into the PEM. The results showed that the H2 partial pressure drop through the anode diffusion electrodes was significant and was affected by the relative humidity of the reactant gases. The O2 partial pressure drop through the cathode diffusion electrodes was affected by both the relative humidity of the reactant gases and the O2 partial pressure in the gas flow channels. The effect of the O2 partial pressure at the cathode CL/PEM interfaces on performance was also investigated. The results suggest that IR loss due to proton transport in the cathode might dominate performance under high O2 concentration conditions. On the other hand, the O2 partial pressure might dominate performance under low O2 partial pressure.
1019
Minoru Okamiya, Takashi Yamamoto, Seiji Sano and Takashi Kajiwara
Pressure Sensitive Paint (PSP) is useful measuring method to analyze oxygen distribution underneath a rib in a fuel cell. High spatial resolution of the PSP measurement is made by creating the uniformly thin PSP film. By using spin coating, which is effective implement to make a thin film, the spatial resolution is improved to 150 µm. PSP phosphorescence intensity depends on oxygen partial pressure. An accurate image of oxygen partial pressure is obtained from calibration curve of each pixel of a PSP image, which is captured by a CCD camera. By calculating each oxygen partial pressure from each calibration curve of its pixels, the error of oxygen partial pressure is decreased to 10%.
1027
Partha P. Mukherjee, Thomas Springer, R. Mukundan, Daniel S. Hussey, David Jacobson, Muhammad Arif and Rodney L. Borup
Water transport in the ionomeric membrane, typically Nafion®, has profound influence on the performance of the polymer electrolyte fuel cell, in terms of internal resistance and overall water balance. In this work, the response of Nafion® membrane water content and the resulting water gradient to fuel cell operational variability are investigated and the results from a theoretical modeling study are furnished along with reference to neutron imaging observations.
1035
Tomofumi Ikeda, Tetsuya Koido, Shohji Tsushima and Shuichiro Hirai
An environmentally controlled MRI technique was used to investigate the effect of relative humidity and current density on the transverse water content profile in a membrane under fuel cell operation at elevated temperature. MRI visualization revealed that, in the dry condition (40% RH), the water content in the membrane was around 3 and the water content profile was flat. In the wet condition (92% RH), a higher water content of around λ=15 was observed than that at 80% RH, suggesting that the generated water in the cathode catalyst layer was transported to the membrane at 92% RH. A larger water concentration gradient was observed at 0.1A/cm2 with 92% RH than that at 80% RH, suggesting that the larger water content in the membrane induced greater electro-osmotic drag, since the electro-osmosis coefficient was positively correlated with the water content.
B2.1: Catalyst Contamination II
1043
Shohji Tsushima, Hiroyuki Morioka, Keisuke Kaneko and Shuichiro Hirai
Catalyst poisoning by the SO2 supply to the PEMFC under OCV and load operational conditions was examined using simultaneous monitoring of cell voltage and SO2 emissions from the cathode exhaust. Results show that all supplied SO2 was readily absorbed in the cell during the initial period, thereby degrading cell voltage while poisoning of the catalyst proceeded more slowly in later periods. The relative humidity (RH) difference between the anode and the cathode brought considerable difference of the catalyst poisoning behaviors. Deteriorative poisoning was observed in the higher cathode RH with the lower anode RH because water transport from the cathode to the anode enhanced transport of contamination to the anode catalyst.
1051
Devina Pillay and Michelle D. Johannes
Interactions between sulfur dioxide, SO2, and hydrogen on two different surfaces of Pt3Co(111) were investigated using density functional theory. The two surfaces considered were a Pt-skin and Ll2 Pt3Co(111) surface. SO2 adsorption was found to be more favorable on the Ll2 surface owing to its d-band center being closer to the Fermi energy. However, both surfaces adsorbed SO2 more weakly in comparison to Pt(111). The adsorption energies of H follow the same adsorption energy trends as SO2 on the different surfaces and show a preference for the three fold-hollow sites similar to other fcc metal (111) surfaces. The weaker adsorption of SO2 on the alloy Pt3Co(111) surfaces agree well with experimental observations that removal of sulfur to attain the initial mass of activity of the catalysts prior to sulfur adsorption requires less cleaning cycles for the alloy. Additionally, our results indicate that less hydrogen adsorbs to alloy surfaces than to pure Pt(111), also in agreement with experiment. SO2 adsorption trends across the three surfaces closely mirror those of atomic sulfur, indicating that surface sulfur tolerance does not depend on the specific oxidation species.
1059
Hui Li, Jianlu Zhang, Khalid Fatih, Zheng Shi, Shaohong Wu, Datong Song, Jiujun J. Zhang, Nengyou Jia, Silvia Wessel, Rami Abouatallah et al
The effects of toluene contamination on the performance of polymer electrolyte membrane fuel cells (PEMFCs) were studied. The severity of the contamination effect increased with increases in the current density, the toluene concentration and air stoichiometry, but decreased with an increase in the back pressure. The effect of toluene contamination on current dynamic operation was also studied by cycling the current density from 0.0 to 0.2, and then to 1.0 A cm-2 at the presence of toluene. The degradation of the fuel cell performance during the current dynamic operation was accelerated by the presence of toluene.
1069
Brian Kienitz, Thomas Zawodzinski, Bryan Pivovar and Fernando H. Garzon
Cationic contamination of polymer electrolyte fuel cells has been shown to cause serious performance degradation but the exact mechanisms of this degradation are not fully understood. A strip cell configuration was devised to study the mechanisms of performance degradation due to cationic contamination by changing the time and length scales of traditional fuel cells while providing a suitable reference electrode. This "strip cell" configuration utilizes traditional Nafion® membranes in an in-plane configuration with electrodes painted on each end. Using this cell it was determined that cationic contaminants collect near the cathode of the fuel cell under load and that this profile leads to increased losses primarily in the cathode region. These results can be directly related to performance losses in a typical PEMFC contaminated by foreign cations.
C2–1.1: Pt Catalyst II
1081
Terry L. Payne, Thomas Benjamin, Nancy Garland and John Kopasz
The current electrocatalyst formulation for the polymer electrolyte membrane fuel cell (PEMFC), platinum supported on carbon (Pt/C), is known to be an effective promoter of redox reactions in fuel cells. However, the cost of Pt (currently ~$2,000/troy ounce) hinders its use as a practical catalyst in commercial fuel cell-powered vehicles at current platinum loading. Another issue with respect to adoption of any electrocatalyst for vehicle applications is durability, especially in light of transportation drive cycle operation with start/stop, start-up/shut-down, and transient requirements. Thus, a robust alternative to current Pt/C technology is needed as the PEMFC electrocatalyst for the oxygen reduction reaction (ORR) on the cathode. The U.S. Department of Energy is funding cathode catalyst research on low-platinum group metal (PGM) catalysts, including alloys and core-shell systems, and on non-PGM catalysts. This paper provides an overview of the issues, approaches, and status of the research.
1093
Shirlaine Koh, Nathan Hahn, Chengfei Yu and Peter Strasser
Dealloyed Pt25Cu75 bimetallic nanoparticle electrocatalysts exhibit up to 6 times higher oxygen reduction reaction activities than Pt-C catalysts. The effects of annealing temperature and duration on the catalyst activity are studied, with annealing temperature varied from 600 {degree sign}C to 950 {degree sign}C and for 7h and 14 h. XRD and electrochemical analyses is used to obtain insight to the structural details of the catalyst samples. Information regarding extend of alloying, Pt and Cu compositions and distributions on the nanoparticles and particle (crystallite) sizes is correlated with the trends observed from mass and specific activities of the catalysts. It is found that annealing duration of 14 h offers little or no benefit to catalytic activities compared to 7 h. Pt25Cu75 annealed for 7 h, at 800 {degree sign}C was found as an optimal compromise between the extend of alloying and particle size growth to give the highest catalytic activity.
1105
Insoo Choi, Oh Joong Kwon and Jae Jeong Kim
Oxygen reduction reaction is one of two main reactions occurring when the fuel cell operates. Unfortunately, high over-potential induced by the irreversibility of such a reaction causes low performance of the fuel cell. In order to overcome the obstacle, researches on utilizing Pt have been extensively studied. Because of low economic efficiency of Pt it is difficult to commercialize synthesized catalysts or practice to them into other applications In this regards, the objectives of this study are to reduce the amount of Pt and promote the reduction reaction by synthesizing Ptshell-Pdcore electrocatalyst. The Pd/C nanoparticle was surrounded by Cu using electroless deposition then, Cu was displaced by Pt using galvanic displacement method. XPS, XRD were applied to identify metallic composition and its existence. And TEM was adopted to image the catalysts. The catalytic properties were investigated using rotating disk electrode.
1111
Sang Hyun Ahn, Soo-Kil Kim, Oh Joong Kwon, Sun-Mi Hwang and Jae Jeong Kim
The Pt-Ru-Co ternary catalyst was prepared on the carbon paper with electrodeposition and galvanic displacement. The carbon paper without PTFE (polytetrafluoroethylene) was used as the substrate for catalyst deposition. The catalyst was prepared with Co electrodeposition on carbon paper through the change of deposition potential and time. The Co nucleation on carbon paper was investigated by using the electrochemical techniques of linear sweep voltammetry (LSV), cyclic voltammetry (CV), chronoamperometry (CA) and field emission scanning electron microscopy (FESEM). Then Pt and Ru galvanic displacement were carried out by control of displacement time. Consequently, the Pt-Ru-Co ternary catalyst was successfully formed using electrodeposition and galvanic displacement, and it showed competitive catalytic activity compared to other reported results in electrochemical analysis.
1117
Ho-Young Jung, Sehkyu Park, Prabhu Ganesan and Branko N. Popov
The electrochemical characteristics of unsupported PtIr black catalysts with various compositions were investigated by CV, LSV, and polarization techniques. The catalyst composition of 85 wt. % Pt and 15 wt. % Ir shows higher oxygen evolution reactivity and comparable electrochemical activity to the unsupported Pt black catalyst. Based on the electrochemical characteristics, URFC using the 85Pt:15Ir catalyst shows higher round-trip efficiency than that of unsupported Pt black catalyst at different current densities.
1123
Di-Jia Liu, Junbing Yang, Nancy Kariuki, Gabriel Goenaga, Ann Call and Deborah J. Myers
A novel membrane electrode assembly (MEA) using aligned carbon nanotubes (ACNT) as the electrocatalyst support was developed for proton exchange membrane fuel cell (PEMFC) application. A multiple-step process of preparing ACNT-PEMFC including ACNT layer growth and catalyzing, MEA fabrication, and single cell packaging is reported. Single cell polarization studies demonstrated improved fuel utilization and higher power density in comparison with the conventional, ink based MEA.
1131
Abhishek Dhanda, Ryan O'Hayre and Heinz Pitsch
This paper presents a novel experimental setup for studying the ORR on well-defined single crystal Pt/Nafion interfaces. Low frequency inductive loops are observed in the impedance spectra that correspond to the dynamics of the adsorbed intermediates. An appropriate reaction mechanism is proposed and the kinetic parameters are derived using a combination of mathematical modeling and impedance analysis.
1143
Prabhu Ganesan, Shenyang Huang and Branko N. Popov
Nb-doped TiO2 support in pure rutile phase with high electrical conductivity (0.83 S cm-1) was synthesized by a simple hydrolysis method. The synthesized support showed disordered mesoporous structure with a surface area of 35 m2g-1. The support showed better stability than Vulcan carbon at more anodic potentials. Nanosized Pt particles were deposited by a borohydride reduction method. Pt/Nb-TiO2 catalyst showed comparable oxygen reduction reaction (ORR) activity and selectivity (> 95%) that of a conventional Pt/C catalyst when tested in rotating ring disk electrode (RRDE).
1151
Dusan Strmcnik, Dennis Van der Vliet, Chris Lucas, Goran Karapetrov, Nenad M. Markovic and Vojislav Stamenkovic
The ability to tune the electronic and structural properties of nanocatalysts can potentially lead towards their superior catalytic activity. This can be achieved by numerous ways such as controlling the size and shape of nanoparticles, the introduction of another metal into the bulk of the catalyst and tuning of the nanoscale surface morphology. The later has been in focus of this report and can be controlled by either preparation procedure or by in-situ electrochemical treatment.
C2@ndash;2.1: Perfluoro Membranes
1163
Nahid Mohajeri, Benjamin P. Pearman, Marianne Rodgers, Rohit Agarwal, Darlene Slattery, Leonard Bonville, H. R. Kunz and James M. Fenton
750 EW perfluorosulfonic acid composite membranes with 15% phosphotungstic acid (FSEC3) were prepared and characterized for high temperature/low relative humidity PEM fuel cell. The membranes at different stages of fabrication, i.e., as cast, Cs treated, and protonated were evaluated with FTIR, XRD, TGA, water uptake, TEM and SEM. By using a low relative humidity atmosphere during the fabrication process, particle sizes of ~20 nm for Cs-PTA within the membrane were achieved. At 30{degree sign}C and 80% relative humidity a conductivity of 80 mS/cm for FSEC3 membrane was measured, which is 2.5 times higher than Nafiona^ 112 conductivity at the same conditions and exceeds the current DOE milestone of 70mS/cm.
1173
Lu Zhang, Xuan Cheng, Ying Zhang and Qinbai Fan
The Nafion membrane was modified using chemical deposited Pd in an effort to reduce methanol crossover in DMFC. The surface morphology, crystal structure and chemical composition of the Pd-deposited membranes were characterized. The glass transition temperature (Tg), proton conductivity and methanol-inhibiting performance of the Pd deposited membranes were studied and compared with those of non-modified membranes. It was shown that Pd-modified membrane exhibited better performance in methanol inhibition and proton conductivity than the Nafion®112 membrane.
1183
Vito Di Noto, Matteo Piga, Giuseppe Pace, Enrico Negro and Sandra Lavina
The electrical performance of Nafion was investigated from -155 to 155 C in the frequency range from 10 mHz to 10 MHz and for two different hydration conditions. The electrical responses are mainly due to conductivity, electrode polarization and relaxation phenomena. These features were correlated to the molecular and nano-scale structure of the material and to the transition/relaxation phenomena observed in both DSC and DMA studies.
1195
Jun Lin, Pin-Han Wu, Ryszard Wycisk and Peter Pintauro
Pre-stretched recast Nafion is a new membrane material with many desirable properties for PEM fuel cells. It was previously shown that the proton conductivity of this membrane in room temperature water was identical to that of commercial Nafion but its permeability to methanol was significantly reduced. Consequently, the power output from a direct methanol fuel cell with pre-stretched recast Nafion (draw ratio of 4) was 50% higher than that with Nafion 117. In an effort to better characterize pre-stretched recast Nafion, additional property measurements were made and compared to those for commercial Nafion. There was a substantial increase in the polymer crystallinity with increasing draw ratio which translated into improved membrane mechanical properties (a higher storage modulus and ultimate tensile strength). There was also a modest increase in the α-transition temperature when the membrane was elongated, as determined from dynamic mechanical analysis. Preliminary results indicated that the proton conductivity of pre-stretched membranes at a sub-zero temperature (-20oC) was about 35% greater than that for Nafion 212 or Nafion 117. On the other hand, the proton conductivity of a water vapor equilibrated pre-stretched Nafion film (draw ratio 4) at 95% relative humidity was identical to that of Nafion 212 for temperatures in the 15-60oC range.
1205
Eric L. Brosha, Tommy Rockward, Francisco A. Uribe and Fernando H. Garzon
The H2S permeability through dry and humidified Nafion{trade mark, serif} PEMFC membranes was studied using ion probe techniques. A sulfide anti-oxidant buffer solution was used to trap and concentrate trace quantities of H2S that permeated through 50 cm2 samples of Nafion{trade mark, serif} 117 and 212 membranes using a partial pressure difference up to 1030ppm at room temperature. Experiments were conducted for up to 24 hours in order to achieve sulfide ion concentrations high enough to be precisely determined by subsequent titration with Pb(NO3)2. The rate of H2S crossover for dry 117 and 212 were identical at 1.2e-7 g/min. Humidification increased the crossover rate to 5.9e-7 g/min and 1.8e-6 g/min for 117 and 212 respectively. An accurate determination of permeation constants from this work was not possible because the H2S partial pressure was found to be not constant throughout the experiment.
1219
Naoto Miyake, Kohei Kita, Masatoshi Honda and Tsuneaki Tanabe
Asahi Kasei Chemicals Co. (AKC) has been developing and producing perfluorinated ionomer membrane for PEFC (PEM) to become new business as the core of membrane and energy business in the future. Recently we focus on R&D of PEM for both stationary and automotive application. In this paper, our latest achievement is summarized and elucidation of membrane degradation mechanism is also conducted.
1229
Eiji Endoh
The world's first highly durable PFSA membrane and MEA for PEMFC have been developed, which can operate for more than 6,000 hours at 120ºC and 50% relative humidity (RH). The MEA is comprised of a newly invented composite polymer (NPC polymer), which has exceptional chemical stability against degradation caused by the hydroxyl radical even at 120ºC. This achievement has opened up a new era of operating PEMFC in the temperature range of near freezing to120ºC under low humidity as well as under high humidity conditions for an extended period of time.
D2.1: Acidic Direct–Fuel FCs and Fuel Oxidation Products
1243
Zenonas Jusys and R. Juergen Behm
The electrooxidation of methanol, ethanol and ethylene glycol on a Pt/Vulcan catalyst was investigated over a wide temperature range [20 to 100oC] at 3 bar overpressure and under continuous electrolyte flow by differential electrochemical mass spectrometry [DEMS]. Oxidation of methanol, ethanol and ethylene glycol at 0.6 V at ambient temperatures yields CO2 current efficiencies of ~40, 5 and 4%, which increase to 100, 24 and 33% at 100oC, respectively. The apparent activation energies for the overall reaction and for oxidation to CO2 were found to be 58 and 64 kJ mol-1 for methanol oxidation, for ethanol / ethylene glycol they were 41 / 32 kJ mol-1 and 73 / 53 kJ mol-1, respectively. The mechanistic and kinetic implications of these data and the importance of model studies under realistic reaction conditions will be discussed.
1253
Shigenori Mitsushima, Tomoaki Takahashi, Azreena Ariffin, Koichi Matsuzawa, Akimitsu Ishihara and Ken-ichiro Ota
In order to clarify the electrooxidation reaction of ethanol, the current efficiency of CO2, CH3CHO, and CH3COOH generation has been determined on platinum of various roughness factors at 70oC in 0.1 mol dm-3 H2SO4 with 1 mol dm-3 C2H5OH. The oxidation current density based on geometrical surface area increased with the roughness factor. On the other hand, the oxidation current density based on a real platinum surface area decreased, and the CO2 generation current efficiency increased. The crystal structure of the platinum surface did not change with roughness factor, because the shape of hydrogen adsorption and desorption in cyclic voltammogram was independent of the roughness factor. Therefore, this behavior would be caused by the difference in the pore structure of Pt plated Pt with the potential distribution. The current efficiency of CO2 generation increased with the decrease of the potential, and became more than 50% at 0.4 V vs. RHE.
1263
Carsten Cremers, Domnik Bayer, Birgit Kintzel, Martin Joos, Florina Jung, Michael Krausa and Jens Tübke
The electro-oxidation reactions of methanol and ethanol were studied in sulfuric acid and potassium hydroxide solution. Different electrode materials were tested for this reaction including base metal electrodes in the alkaline case. Tests were performed using standard electrochemical techniques such as cyclic voltammetry, chronoamperometry and differential electrochemical mass spectrometry. Comparing both reactions it was found that in the acidic environment the methanol oxidation proceeds faster and is more complete than the ethanol oxidation. However, the situation changes in alkaline solution. Here, the kinetic enhancement of the ethanol oxidation reaction is in many cases so strong that the ethanol oxidation kinetics become faster than the methanol oxidation kinetics at the same metal and under the same conditions.
1275
Junichiro Otomo, Satoru Nishida, Hiroyuki Kato, Hidetoshi Nagamoto and Yoshito Oshima
Anodic reactions in a direct alcohol fuel cell (DAFC) at intermediate temperature (250 oC) were investigated from the standpoint of achieving high performance. In order to evaluate the temperature effect on the electro-oxidation of small alcohols in the intermediate temperature region, a kinetic study on the electro-oxidation of methanol and ethanol on Pt/C was conducted using a single cell fabricated with CsH2PO4 proton conducting solid electrolyte. At 250 oC, the current density of ethanol electro-oxidation is comparable to that of methanol electro-oxidation in a low potential region (< 400 mV vs. RHE). In addition, the analysis of reaction products suggests that C-C bond cleavage in ethanol electro-oxidation can proceed at the intermediate temperature. Through the electrochemical measurements, characteristic features in the alcohol electro-oxidation at the intermediate temperature were discussed.
1285
Andrew B. Bocarsly and Ellazar Niangar
Ethanol presents several advantages over other alternative fuels. Its volumetric energy density (23.4 MJ/L) is slightly lower than gasoline (33.4 MJ/L), but much better than available with either methanol or hydrogen. If an ethanol is used in a proton exchange membrane (PEM) fuel cell the lowered energy density compared to gasoline in an internal combustion engine can in theory be overcome. This assumes that an electrochemical system can be developed that carries out the complete 12-electron oxidation of ethanol. To reach this goal, new catalyst systems must be developed. It is found that multicomponent catalysts such as platinum tin oxide (Pt/SnO2) and platinum tin oxide titanium dioxide (Pt/SnO2/TiO2) improve the conversion of ethanol to its 12-electron oxidation products. Catalysts of this type can be quickly prepared usingamicrowave-assisted polyol procedure. Elevation of the operating temperature of a PEM fuel cell using the indicated catalysts to 130åC facilities production of CO2 and provides an improved current-voltage response.
1293
Yuta Katayanagi and Yohtaro Yamazaki
The effect of oxygen crossover in a direct ethanol fuel cell with acetaldehyde fuel was investigated. The cell was operated at a constant voltage of 0.2 V, and the fuel flow rate of the anode and the oxygen concentration in the cathode gas were varied. The reaction products in the anode were analyzed using gas chromatography. When the O2 concentration in the cathode gas increased and the fuel flow rate decreased, the amounts of the evolved CO2 gas increased.
B2.2: Catalyst Support Degradation I
1301
Axel Ofstad, John Davey, Svein Sunde and Rodney L. Borup
Carbon corrosion rates were measured for four types of polymer-electrolyte membrane (PEM) electrode assemblies (MEAs) during shut-down air purging and start-up. The corrosion rates were measured at different purge rates, temperatures, and relative humidities. The highest amount of carbon corrosion occurs when gases are humidified and when using low flow rates for the air purging during shut-down and low hydrogen flow during start-up. Dry conditions give the highest rates of corrosion during shut-down when comparing the same flow rates of hydrogen and air, while humid conditions gives the highest rate of corrosion during start-up when comparing the same flow rates of hydrogen and air.
1313
Jingwei Hu, Pang-Chieh Sui, Ned Djilali and Sanjiv Kumar
A two dimensional model is developed to simulate carbon corrosion reaction caused by local fuel starvation during the operation of a PEMFC. This work focuses on the evaluation of different mitigation techniques for carbon corrosion reactions, namely use of catalyst with high oxygen evolution reaction (OER) activity, membrane of low O2 diffusivity, corrosion-resistant carbon support and high proton conductivity in the catalyst layer. It is found that using the OER-favorable catalyst and low O2-diffusivity membrane are two effective techniques for mitigation of carbon corrosion reaction for local starvation.
1323
Kunal Jain, Ashok Gidwani, Sanjiv Kumar and James Vernon Cole
This paper addresses the durability and degradation of Proton Exchange Membrane (PEM) fuel cells with a focus on carbon corrosion at electrodes. To address this, detailed Butler-Volmer kinetics are implemented in a general purpose finite volume CFD code CFD-ACE+. The code was validated against experimental and model data from the literature showing excellent match with polarization data and partial current densities for individual reactions. Numerical calculations of fuel cell operation under different corrosion conditions were performed in two-dimensional and three-dimensional geometries. Results are presented in terms of distribution of fuel, potential and the current densities. The simulations and results indicate that advanced CFD with detailed Butler-Volmer kinetics can be used to identify the conditions leading to corrosion and guide development of operating conditions and materials to mitigate the electrode degradation and improve the fuel cell system durability.
A2.2: Diagnostics and Cell Stacks
1337
Shuichiro Hirai and Shohji Tsushima
Recent developments in MRI visualization for water transport and degradation analyses in PEMFC are presented. High-resolution MRI experiments were performed for a 117-μm-thick membrane. Partial dehydration of the membrane's anode side was visualized with the increase of current density. Nuclei-labeling MRI was also presented. Results demonstrated its unique potential for direct visualization of the water source on membrane hydration using D2 and D2O. Spatially-resolved NMR was also applied to a degraded membrane. The membrane's cathode side, as measured using 1H-NMR spectra, showed a greater chemical shift.
1345
Jacob Spendelow, R. Mukundan, John Davey, Tommy Rockward, Daniel S. Hussey, David Jacobson, Muhammad Arif and Rodney L. Borup
High resolution neutron radiography was used to image polymer electrolyte membrane fuel cells (PEMFCs) during operation under a variety of conditions. The effect of specific operating conditions, including flow direction (co-flow or counter-flow), orientation of the PEMFC with respect to gravity, and simulated anode recycle loop, were examined. Counter-flow operation was found to result in higher water content than co-flow operation, with more uniformly distributed water. Orientation with respect to gravity was also significant, with net water transport observed from the higher side of the cell to the lower side. The higher anode flow rate resulting from the simulated recycle loop facilitated convective removal of liquid water from the anode flow field, leading to lower overall levels of water in the PEMFC.
1357
Moon Jeong Park and Nitash P. Balsara
Ion conducting polymers containing sulfonic acid are of interest for the fuel cell applications. This study is based on sulfonated poly(styrene-b-methylbutylene) block copolymers. In dry state, these materials show remarkably rich sequence of phase transitions, i.e., lamellae, gyroid, hexagonally perforated lamellae, hexagonal cylinder, and disorder, depending on temperature, molecular weight, and fraction of sulfonated monomers. The effect of hydration on the dry morphologies is determined by a combination of in-situ neutron scattering and cryogenic electron microscopy.
1365
Yong-Sheen Hwang, Suk Won Cha, Seo-Young Kim, Sang-Hoon Ji, Daeheung Lee, Hoon Choi, Jong Won Choi, Jeong-Hoon Seo, Min Soo Kim and Dae-Young Lee
This study considers the feasibility of the concentration control of the fuel and vapor by oscillating flow in the channel of Polymer Electrolyte Membrane Fuel Cells(PEMFCs). PEMFC Stack performance is largely influenced by the fuel and vapor concentration. If the fuel concentration is lower than stoichiometry 1.25 of the hydrogen and 2.5 of the air or the flooding is happened by excess water, its performance deteriorates seriously because of the fuel and air starvation. In this respect the optimization of the fuel and vapor concentration is crucially important to maximize fuel cell stack performance. The objective of the current study is to apply the principle of the mass transfer being enhanced by the oscillating flow to the cathode channel.
1377
Michael Pien, Marvin Warshay, Stephen Lis and Radha Jalan
ElectroChem, Inc. has demonstrated a dead-ended fuel cell operating at very low excess oxygen requirement and maintaining very stable performance. The fuel cell not only showed significantly higher voltages at high current density but also demonstrated the gravity-independent operation. The dead-ended operation significantly enhances the fuel cell power density by creating self-humidification and obtaining high efficiency of gas utilization.
C2–1.2: In–situ Spectroscopy and Theory
1385
H. Ogasawara, L. A. Naslund, J. McNaughton, T. Anniyev and Anders Nilsson
Water is present during the normal operating condition of polymer electrolyte membrane fuel cells (PEMFCs) and we have, through model experiments on a platinum surface using x-ray photoelectron spectroscopy, investigated its role in two different stages in the oxygen reduction reaction (ORR). We found that the activation of oxygen to the adsorbed atomic phase occurs readily in the dry region, but not in the humid region process. In this case, water is acting to inhibit the active sites on the catalyst. On the contrary, water is found to promote the reduction of adsorbed atomic oxygen in the formation of a water-hydroxyl surface complex.
1395
Sarah L. Hudson, Sarah C. Ball, Katie B. Blaney, Gael H. Chouchelamane, Steven G. Fiddy, Ian Harvey, Prabalini Sivasubramaniamb, Béatrice C. Tessier, Brian R. Theobald, David Thompsett et al
A proton exchange membrane fuel cell has been designed to enable correlation of cathode catalytic activity with structural parameters determined by in situ XAS investigations in transmission mode. The cell design is described and validated for oxygen reduction activity measurement using both Pt and PtCo alloy catalysts. Findings from in situ XAS investigations at the Pt LIII edge are presented for a 60% Pt/C cathode catalyst operating at OCV, under load with oxygen feed, and during time resolved potential step experiments with oxygen and nitrogen feeds. In nitrogen XANES and EXAFS analysis show increasing oxide formation and particle disruption with increasing potential up to 1.0 V. In oxygen the catalyst structure remained unchanged irrespective of the applied potential and therefore load drawn from the cell. Differences in coordination number at the same applied potential in oxygen compared to nitrogen indicate that a particle morphology change occurs during the ORR.
1405
Chin-Hsien Cheng, Kourosh Malek and Ned Djilali
An equilibrium molecular dynamics simulation is employed to investigate the morphology changes inside the catalyst layer (CL) due to different sizes of Pt particles. The microstructure formed during the fabrication stage determines majority of the CL performance. Different sizes of the nano Pt particles are formed during the fabrication process. It is important to investigate the relation between the microstructure and the Pt cluster sizes. Different sizes (about 1, 2 and 3 nm) of Pt particles are considered in the present work. It was found that the small Pt particles (case of 1 nm) tend to merge to form a larger Pt cluster. This was not so in the case of lager Pt particles (2nm and 3nm). The microstructure formed at various Pt cluster sizes is shown to be quite different. Detailed information about the structure was obtained by carrying out structural analysis in view of radial distribution function (RDF)
C2–2.2: Composite Membranes
1415
Jennifer Peron, Feifei Ng, Elodie Ruiz, Deborah Jones and Jacques Roziere
A novel sulfonated polybenzimidazole has been prepared by solution copolycondensation of diaminobenzidine, 5-sulfobenzene-1,3-dicarboxylic acid and 4,4'-(hexafluoropropylidene) bis(benzoic acid) in various stoichiometric ratios using polyphosphoric acid as solvent. The resulting polymers, characterized by 1H NMR spectroscopy, are soluble in polar aprotic solvents and show excellent film-forming characteristics. Mechanically tough and flexible films are prepared by solution casting. The properties of the polymer and membranes have been characterized as a function of the degree of sulfonation, and compared with those of sulfonated poly-[(1-(4,4'-diphenylether)-5-oxybenzimidazole)-benzimidazole] prepared by direct sulfonation. The hexafluoropropyl group imparts flexibility and favours clustering of sulfonic acid rich domains that are favourable for proton transport.
1423
Bo Li, Pyoungho Choi, Benjamin P. Pearman, Marianne Rodgers, Rohit Agarwal, Nahid Mohajeri, Clovis A. Linkous, Wonseok Yoon, Xinyu Huang, Darlene Slattery et al
Two different fabrication procedures of catalyst coated membranes (CCMs) using 750 EW poly [perfluorosulfonic acid] ionomer composite membranes that contain phosphotungstic acid are discussed in this study. Cell polarization was obtained at three operating conditions: 80/100/75, 100/70/70, and 120/35/35 (cell temperature {degree sign}C/anode %RH/cathode %RH), and ambient pressure. Hydrogen/air cell performances at 120/35/35 and 400 mA/cm2 varied with the procedure from 0.39V to 0.64 V. Utilization of different fabrication procedures has a significant effect on electrode structure and thus relative overpotential, but little influence on membrane resistance and related ohmic loss. Although much higher performance occurred with the non-heat treatment process, durability issues require heat treatment for stabilization. Further study on the physical and chemical properties of the fabrication process of 750EW poly [perfluorosulfonic acid] ionomers/phosphotungstic acid CCMs is necessary to optimize both the performance and durability of elevated temperature and low relative humidity CCMs.
1433
Jonghyun Choi, Kyung Min Lee, Ryszard Wycisk, Peter Pintauro and Patrick Mather
A new class of proton-exchange membranes has been developed and characterized, where an interconnected network of proton conducting polymer nanofibers is embedded in an inert (non-conducting) polymer matrix. In the present study the nanofiber network membrane contained electrospun fibers from sulfonated poly(arylene ether sulfone) solutions (with/without sulfonated polyhedral oligomeric silsesquioxane, sPOSS). The membranes were characterized in terms of morphology, proton conductivity, and water uptake. In-plane proton conductivity was measured using a BekkTech cell that was placed in a controlled temperature/humidity chamber. The data show: (1) There was a modest increase in nanofiber > 50%.membrane conductivity when the IEC of the fibers was increased from 2.1 to 2.6 mmol/g (in the absence of sPOSS), (2) There was a substantial increase in membrane conductivity when sPOSS was added to the fibers, and (3) The proton conductivity of the sPOSS-loaded membranes was significantly higher than that for a commercial Nafion 212 sample at 30oC for a relative humidity
1443
Keiji Sasajima, Hirokazu Munakata and Kiyoshi Kanamura
Three-dimensionally ordered macroporous (3DOM) silica composite membrane including a binary polymer consisting of sulfonated poly (ether ether sulfone and poly styrene (SPEES-PS) was fabricated by stepwise filling method. In the SPEES-PS composite, SPEES coated 3DOM-silica surface and PS occupied a vacancy of remaining pore of SPEES composite. Therefore, the structure of SPEES-PS composite were core-shell like structure. Water uptake and methanol permeability of SPEES-PS composite was greatly suppressed. However SPEES-PS composite exhibited relatively high proton conductivity.
1451
Chunmei Wang, Elena Chalkova, Christopher Lute, Mark Fedkin, Sridhar Komarneni, T.C. Mike Chung and Serguei Lvov
The main objective of this study is to synthesize new membrane materials in which inorganic proton conductors are deposited within a functionalized and cross-linkable Teflon-type polymer. These new composite membranes are aimed to efficiently conduct protons at temperatures above 100 oC and relative humidity (RH) down to 25% in proton exchange membrane (PEM) fuel cells. To effectively choose inorganic proton conductors, the conductivity studies of different materials are performed in our lab. An experimental system was developed and Gamry Electrochemical Impedance Spectroscopy (EIS) was applied to measure the proton conductivity of inorganic materials. Alpha zirconium phosphate was used as a standard to check the accuracy of the present experimental approach. The conductivity of the solid acid sulfated zirconia (S-ZrO2) was studied. The proton transport mechanisms in inorganic proton conductors were discussed.
1461
Stephen L. Rhoden and Clovis A. Linkous
As pollution and climate change continues to affect the world renewable, non-polluting sources of fuel are vital. Hydrogen fuel cells have been shown to be very effective in converting fuel to usable energy, with water being the only product. Sulfonated poly aryl compounds such as sulfonated poly(etheretherketone) (SPEEK) are oxygen-containing organic polymers, which when hydrated exhibit proton-conducting properties. The use of solid inorganic fillers such as phosphotungstic acid (PTA) to increase proton conductivities at high temperatures is of much interest to MEA fabricators. Previously we showed that SPEEK membranes doped with 15 wt% PTA that had been treated with a 0.1 M cesium carbonate solution to render the it insoluble, increased the conductivity by over one order of magnitude over a range of relative humidities. The optimal loading of PTA into the membrane, plus conditions for PTA and SPEEK membrane co-precipitation are both of much interest.
1471
Vivek S. Murthi, Joseph Dura, Sushil Satija and Charles Majkrzak
Nafion thin films (~500 Aå) spin coated onto the Pt and Au layers on Si are investigated for water uptake and swelling. Neutron Reflectometry data demonstrate that these structures are composed of nafion layers which differ from their bulk properties in terms of their scattering length density and water uptake. However, as the relative humidity is increased, the amount of water in the layers increases for a Nafion on Au and is comparable to that observed on bulk nafion membranes only up to 80 % RH. However, the Nafion on Pt reaches complete hydration at 96% RH. Although, a single layer model was able to fit the NR data obtained on nafion under vapor conditions, only a bilayer model, with an outer less hydrated nafion and an inner more hydrated nafion layer, was able to fit the data in liquid water.
1487
Patrick Mangiagli, Chrostopher Ewing, Kui Xu, Qing Wang and Michael A. Hickner
Gravimetric analysis was performed during a step change in relative humidity for a series of sulfonated polymers to determine their dynamic water uptake characteristics. The mass change was recorded as a function of time for both stiff-backboned and flexible-backboned polymers when the humidity was instantaneously increased from 40 to 50 %. The observed water uptake profiles were distinctly different based on the inferred stiffness of the sulfonated polymer backbone. A sulfonated poly(sulfone)-based membrane had a slower mass uptake than more flexible Nafion with time constants of 307 s and 150 s for the sulfonated poly(sulfone) and NRE212, respectively. The dynamic water absorption properties were measured for a series of sulfonated poly(styrene)-b-poly(vinylidene fluoride)-b-sulfonated poly(styrene) membranes. The backbone flexibility of these polymers was intermediate to that of the poly(sulfone) and Nafion membranes and could be tuned based on the molecular weight of the poly(styrene) blocks and sulfonation level.
D2.2: DMFC Systems and Operation
1495
Jianyu Cao, Ting Yuan, Qinghong Huang, Zhiqing Zou, Baojia Xia, Hui Yang and Songlin Feng
To meet the demands for high power microelectronic devices, research efforts at SIMIT have involved the optimization of Si based flow fields using the MEMS technology, the development of key components for the air-breathing micro direct methanol fuel cells (µDMFCs), the assembly of µDMFC stacks and the integration of micro energy systems. We found that the microstructure of both the anodic and cathodic flow fields has a significant influence on the performance of the µDMFCs. By adjusting the microstructure of the flow field plates, it is possible to obtain the better performance of a µDMFC with Si based flow field plates than that using traditional flow field plates. Recent research results including the fabrication of the membrane electrode assembly with improved performance and the water management under the air-breathing mode will be presented. Integrated µDMFC systems and their possible applications will be discussed.
1507
Christian E. Shaffer and Chao-Yang Wang
A low water crossover from anode to cathode in a direct methanol fuel cell (DMFC) must be realized if highly concentrated methanol fuel is to be used. The use of a low-α membrane electrode assembly (MEA) is vitally important in achieving this goal. The low rate of water crossover for a low-α MEA has traditionally been attributed to the hydrophobic cathode micro-porous layer (MPL), thin membrane combination, but it has recently been discovered that a hydrophobic anode MPL is also effective in reducing water crossover. In this paper we demonstrate that a hydrophobic anode MPL may play an even more significant role than cathode MPL in reducing water crossover, and we embark on developing anode-controlled water management strategies for DMFCs. As a first step in this process, we show that a thicker, more hydrophobic anode MPL with lower permeability is more effective in reducing water crossover.
1519
Young-Soo Chang, Changhwan Cho and Youngchan Kim
We have developed an electro-chemical model of a stack to analyze its performance. The model includes methanol solution at the anode to "cross over" to the cathode through, which reduces the system efficiency and increases fuel consumption. BOP (Balance of plants) system - condenser, cooler, and methanol solution tank - was modeled. Dynamic simulation was performed to evaluate and develop a control algorithm of the fuel cell system for an efficient operation of DMFC. We simulated the effects of the varying total UA (overall heat transfer coefficient), and proposed minimum UA of the condenser and cooler. When the volume of the methanol solution tank decreases below a certain level, ON/OFF based control algorithm leads to an unstable fuel cell operation. By adopting PID based control algorithm, the system has better controllability of methanol concentration and power generation in response to load change under the same methanol solution tank volume.
1525
Cullen Buie and Juan Santiago
Controlled experiments on a direct methanol fuel cell (DMFC) elucidate the effects of methanol flow rate and current density on pressure drop across the DMFC anode. A novel experimental technique is developed to measure void fraction, liquid slug length, and velocity of the slug/annular two phase flow exiting a DMFC anode. For the explored channel geometry, hydraulic diameter (Dh) of 600 microns, pressure drop scales with the number of slug/bubble interfaces, surface tension, and Dh. We present an empirical correlation of more than 160 measurements to aid in predicting pressure drop for DMFCs of similar scale. This work will aid in the design of fuel pumps for miniature DMFC systems.
1539
Seungbum Ha, Ikwhang Chang and Suk Won Cha
The transient behavior of a passive air breathing direct methanol fuel cell (DMFC) operated on vapor-feeding mode is studied in this paper. As a result of experiment, the output performance is sometimes unstable and there are some overshoots. A mathematical dynamic one-dimensional model for simulating transient response of the DMFC is presented. In this model a DMFC is decomposed into its subsystems using lumped model. A one-dimensional, non-isothermal, combined heat and mass transport model is developed that captures the coupling among water generation and transport, oxygen consumption, self-heating and natural convection. For validation, similar experiments were carried out. As a result of simulation and experiments, strong effects of feeding methanol concentration and water transport were found out. The model and experiment analysis provides several conclusions. The performance drop after peak point is caused by insufficiency of water at the anode. The excess water at the cathode makes performance recovery impossible.
1549
Alan B. Ilicic, David P. Wilkinson, Khalid Fatih and Francois Girard
A unique approach which facilitates the use of high fuel concentrations in Direct Liquid Fuel Cells (DLFCs) is reported. By substituting the air cathode of a conventional DLFC with a redox couple cathode, a 3D carbon-based electrode can be employed to achieve cathode selectivity. This configuration not only eliminates cathode depolarization, but also enhances the cell design flexibility, allows for a Pt-free cathode and precludes cathode flooding as it is an all-liquid system. Methanol and formic acid are used as model fuels with the Fe2+/Fe3+ redox couple in cyclic voltammetry and fuel cell performance tests to demonstrate the positive attributes of this system. Fuel cell tests include the use of Nafion® 112 or Nafion® 117 as the membrane and fuel concentrations approaching that of pure fuel.
B2.3: Catalyst Support Degradation II and Membrane Mechanical Durability
1563
Norimitsu Takeuchi and Thomas F. Fuller
Carbon loss phenomena, such as partial hydrogen starvation and startup, have been investigated in previous works. Even for short times, these situations can be fatal and some mitigation were suggested to improve PEMFC durability. Small carbon loss occurs under ordinary PEMFC operation. Although this impact is less than for hydrogen starvation and startup, it is still large enough to cause the degradation of PEMFC cell performance after long-term operation. Carbon loss under PEMFC operation is investigated in this work with a physical model. These results suggest that high cell potential, high humidity, and imbalance of water vapor pressure in the cell affect carbon loss. Oxygen reduction promoted carbon loss due to a reduced solution potential at the fuel-cell cathode-membrane interface.
1573
Xinyu Huang, Marianne Rodgers, Wonseok Yoon, Bo Li and Nahid Mohajeri
The authors report the mechanical degradation behavior of perfluorosulfonic acid (PFSA) membranes under open circuit voltage hold condition. The degradation behavior of an ePTFE reinforced PFSA membrane impregnated with phosphotungstic acid (PTA) in cesium form was compared with that of an extruded Nafion® N-112 membrane. Membrane electrode assemblies were fabricated by spraying carbon supported platinum catalysts on either side of the membrane. Diagnostic tests were conducted before and after 100 hours of OCV hold period. Mechanical tests were performed on as-fabricated MEAs and MEAs after OCV hold test. The PTA additive was found to be very effective in reducing fluoride emission rates. However, the mechanical strength decay for both type of membranes remains significant. The composite membrane retained a comparatively higher level of residual toughness than the N112 membrane. SEM analysis revealed localized cracks form inside the membranes as a result of OCV hold.
C2–1.3: Pt Catalysts III
1583
Patrick Pietrasz, R. M. Sankaran and Thomas Zawodzinski
Pulse voltammetry as a technique was used to explore the conditions under which platinum oxides form in an operating fuel cell. The technique is shown to have much slower reaction times due to the high surface area of the fuel cell electrodes.
1591
Ram Subbaraman, Thomas Zawodzinski and Jay A. Mann
The structure of supported nanocatalysts plays a significant role in the kinetics of fuel cell reactions. A molecular dynamics (MD) approach to understanding the structure based on the interaction energy between atoms in the nanoparticle and support is presented. The effect of particle size on the "strain," as represented by the displacement field, is determined for nanoparticles of platinum and various alloys. Effects of alloying elements and the nature of the support are discussed.
A3.1: Gas Diffusion Media
1603
Tatsumi Kitahara, Toshiaki Konomi, Hironori Nakajima, Yoshinobu Tateishi, Makoto Murata, Nico Haak and Peter Wilde
The present study was carried out to find out the best combination of gas diffusion layers (GDLs) for a polymer electrolyte fuel cell (PEFC) operated under very low-humidity conditions at the cathode and high-humidity conditions at the anode using a test apparatus in which the clamp pressure on the cell could be accurately controlled. For cathode GDLs, it is important to maintain humidity and prevent dehydration of the MEA. A microporous layer (MPL) coating on the low-porosity carbon paper substrate is effective for enhancing PEFC performance. For anode GDLs, however, it is important to increase water transport from the humidified hydrogen gas to the MEA. An anode GDL with the MPL reduces PEFC performance. Hydrophobic treatment by PTFE (polytetrafluoroethylene) loading in the anode GDL is effective for performance enhancement. However, when the PTFE content becomes too high, the water transport properties are reduced, thereby lowering PEFC performance.
1615
Wei Zhu, Jim P. Zheng, R. Liang, Ben Wang, Chun Zhang, Shawn Walsh, George Au and Edward J. Plichta
The Pt catalytic electrode was developed using carbon nanotube film (buckypaper) as a supporting medium through use of the electrodeposition method. Buckypapers are free-standing thin films consisting of single-walled carbon nanotubes (SWNT), multi-walled carbon nanotubes (MWNT) or carbon nanofibers (CNF) held together by van der Waals forces without any chemical binders. Mixed buckypapers may be developed by layered microstructures with a dense and high-conducting SWNT networks at the surface, as well as large porous structures of MWNT or CNF networks as supports. This unique microstructure may improve Pt catalyst accessibility and the mass exchange properties. Pt particles were uniformly deposited in porous buckypaper and had an average particle size of about 6 nm. A promising electrochemical surface area of about 40 m2 g-1 was obtained from these electrodes. A Pt utilization of as low as 0.5 g kW-1 was achieved for the cathode electrode at 80 oC. Pt utilization efficiency may be further improved by optimization of the electrodeposition condition in order to reduce the Pt particle size.
1627
Sehkyu Park and Branko N. Popov
The effect of hydrophobic and structural properties of the cathode gas diffusion layer on mass transport in PEM fuel cells was examined experimentally and theoretically. The results indicated that liquid water transport at the cathode is controlled by the interplay between fraction of hydrophilic surface and average pore diameter in the cathode gas diffusion layer.
1635
Yoshinobu Fujii, Shohji Tsushima, Katsuhiko Fukuzato and Shuichiro Hirai
An effect of a micro porous layer (MPL) on water transport under a low-humidity condition was examined in a PEMFC with a single straight channel using a tunable diode laser absorption spectroscopy (TDLAS) measurement system, which can measure local through-plane water transport based on measurement of the distribution of water vapor concentration along the channel. The TDLAS results showed that the MPL imparts mass transport resistance at the cathode side under low-humidity conditions with co-flow and counter-flow modes and enhanced back-diffusion of the generated water to the anode side. The MPL at the cathode side strongly affected through-plane water transport and is therefore effective for membrane hydration under low-humidity conditions.
1643
Perry Cheung, Joseph D. Fairweather and Daniel T. Schwartz
The relationship between capillary pressure (PC) and liquid saturation (SL) in gas diffusion layers (GDLs) is an important feature of water management in polymer electrolyte membrane fuel cells (PEMFCs) (1). Experimentally measured PC vs. SL data (3-7) have emerged as an important way to characterize this key water management-related property, but a theoretical framework for analyzing PC vs. SL data to understand fundamental structure/property relationships is lacking. We present here a bundle of capillaries model capable of analyzing experimental PC vs. SL data that deconvolute the effect of pore structure and surface properties on GDLs in PEMFCs.
1651
Vladimir Gurau, Thomas Zawodzinski and Ryan Wayne
Single cell testing is carried out using a sensitivity testing approach to evaluate the performance of GRAFCELL® materials used as macro-porous substrate for cathode GDLs under a range of flow, pressure, temperature and humidity conditions. Polarization curves and electrochemical impedance spectroscopy data are used to establish a correlation between the processing factors and the in-situ fuel cell performance, to identify the key characteristics required to optimize the fuel cell performance and to downselect the specimens with the best combination of properties.
1661
Gen Inoue, Yosuke Matsukuma and Masaki Minemoto
It is important to investigate the two-phase condition in PEFC gas diffusion layer (GDL) to improve mass transfer rate. The structure of simulated GDL made of layered carbon fibers was produced by the numerical analysis in this study, and the structural properties of various simulated GDL were investigated, for example pore distribution, permeability and tortuosity. With these structures, the two-phase analysis model in GDL was developed with a 3-dimensional network model converted from simulated GDL directly, and the two-phase condition in GDL was calculated on various conditions of GDL structure and hydrophilicity. And the influences of multi-layer GDL structure were evaluated. As a result, it was confirmed that the liquid water distribution was affected by multi-layer structure and that optimizing the connection of pore-pore and changing the contact angle along the direction of water flowing out lead to decrease the amount of water and increase O2 diffusivity.
1673
Satheesh Sambandam and V. Ramani
The ionomer/binder type and composition can influence both ionic and mass transport in a PEFC electrode. For an electrode to have minimum resistance to O2, proton and electron transport, the ionomer composition has to be optimized for its EW and volume fraction. An optimum ionomer composition in the electrode results in higher Pt utilization and hence better MEA performance. Ion and species transport characteristics of electrode layers containing PFSA ionomers with different EWs are examined in this study by analysis of MEA polarization data at different relative humidities. Steady state polarization curves were obtained with air and oxygen. The polarization data for MEAs was analyzed to determine the relative contributions of the different sources of polarization, namely activation losses, membrane resistance losses, ohmic losses in the electrode, and mass transport losses in the GDL and electrode.
B3.1: Membrane Degradation
1687
Thor Anders Aarhaug, Ann Mari Svensson, Axel Baumann Ofstad, Jan Gregor Ho̸ydahl So̸rli and Héloi¨se Couvert
Experimental design has been applied to study PEMFC performance and durability as a function of operating conditions. Two levels of relative humidity, clamping pressure and back pressure have been systematically applied to an ON/OFF load cycle. Effluent analysis of fluoride and sulfate has been performed to correlate the emission rates to the durability observed. Background effluent levels for fuel cell test rigs were also assessed. Fluoride emission rates increases with time. The rates are higher for the experiments with back pressure, but they do not correlate well with voltage losses. High initial emission rates of sulfur are observed. After flushing with humidified inert gas, the emission rates decline but are sustained at high rates compared to fluoride. Sulfate emission rates are higher for experiments with high humidification levels. The total mass of sulfur released is higher than expected from the ionomer equivalent weight.
1697
Xinyu Huang, Xiaofeng Wang, Joshua Preston, Leonard Bonville, H. R. Kunz, Michael Perry and David Condit
The authors report the degradation behavior of polymer-electrolyte membrane fuel cells tested under two types of water-management schemes: the solid plate (SP) cells that mange water via flow and dew point control of the reactant gases, and water transport plate (WTP) cells that actively remove liquid through micro-porous bipolar plates. Comparative experiments were conducted. Cell performance degradation was tracked by periodic diagnostic testing. After cell testing, the residual mechanical strength of the membrane electrode assemblies was characterized. It was found that both water management schemes led to cell performance reduction via the loss of the electrochemical active area. However, the SP cell led to rapid reduction of membrane toughness. The WTP cell tended to preserve the membrane mechanical toughness better. Post-analysis found localized membrane failure in SP cell test during which a step change in performance occurred. Abrupt performance degradation was not observed for either of the WTP cell tests.
1705
Jae Young Shim, Shohji Tsushima and Shuichiro Hirai
Membrane degradation was investigated by accelerated membrane degradation tests in various gas-supply conditions. Results show that the anode side of the membrane was more deteriorated under H2-O2 supply conditions. However, the cathode side of the membrane was more deteriorated under H2-air supply conditions. Quantitative examination of the oxygen crossover by direct gas mass spectroscopy (DGMS) elucidated that the oxygen crossover depends on the oxygen partial pressure and relative humidity of the supplying gas. Based on membrane degradation and oxygen crossover, we modeled membrane thinning with a simple rate equation with the effect of partial pressure. Calculated values of membrane thinning were consistent with the experimental values.
1713
Naoki Hasegawa, Takashi Asano, Tatsuya Hatanaka, Masaya Kawasumi and Yu Morimoto
Open-circuit durability tests are carried out for intentionally Pt-precipitated membranes with and without electrodes to clarify the roles of Pt-band and the electrodes. The Pt-precipitated membrane without electrodes gives a small but non-zero fluoride emission rate (FER). The Pt-precipitated membrane with electrodes gives the highest FER, which is much higher than that of membrane with electrodes (conventional MEA). Chemically aggressive species are produced on both Pt-band and electrodes. Pt band, without electrodes, is only slightly detrimental for the membrane but, with electrodes, it significantly accelerates membrane degradation.
1717
Yoji Nakamori, Naotoshi Suzuki, Kazuhisa Tanaka and Tsutomu Aoki
H2O2 formation on Pt/C catalyst and Pt1Run/C (n = 1/3, 1/2, 1, 3/2, 2) catalysts was studied with rotating ring-disk electrode (RRDE) in 0.5 M H2SO4. H2O2 formation on Pt/C catalyst and Pt1Run/C catalysts with smaller Ru content increased sharply below 0.1 V vs. RHE. On the other hand, for larger Ru content catalysts, Pt1Run/C (n = 1, 3/2, 2), their H2O2 formation was lower than that of smaller Ru content catalysts below 0.1 V vs. RHE. Pt1Run/C catalysts with larger Ru content prevented H2O2 formation in anode catalyst layer and mitigated membrane degradation in PEFC. Potential cycles between 0.1 V and 1.0 V and between 0.1 V and 1.2 V vs. RHE were applied for Pt1Ru2/C catalyst. H2O2 formation below 0.1 V vs. RHE increased after potential cycles. Ru dissolution from Pt1Ru2/C catalyst was considered to promote H2O2 formation.
1725
Panagiotis Trogadas, Javier Parrondo and V. Ramani
The efficacy of CeO2 nanoparticles in mitigating free radical induced PEM degradation is investigated. Commercially obtained CeO2 and nanoparticles synthesized in-house were incorporated within a recast Nafion® membrane. MEAs were prepared using Nafion® and Nafion®-CeO2 composite membranes (0.5wt%, 1wt%, and 3wt% CeO2). The composite membranes exhibited very similar proton conductivities (~35mS/cm) and hydrogen crossover (~1 mA/cm2) as Nafion®. However, the fluoride emission rate (estimated from accelerated tests) was lowered by more than one order of magnitude upon addition of CeO2 into the Nafion® membrane, suggesting that CeO2 nanoparticles have potential to enhance membrane durability.
1735
Frank D. Coms, Han Liu and Jeanette E. Owejan
Cerium and manganese ions are very effective reversible scavengers of •OH in an operating PFSA-based PEM fuel cell. The use of these ions in very small quantities can reduce the fluoride release rate by up to three orders of magnitude relative to an unmitigated sample and thereby afford extremely durable membranes. A chemically rational mechanism that accounts for the remarkable effectiveness of these chemical mitigants is presented.
C3.1: Electrode Materials and Processes I
1751
Hiroshi Iden, Atsushi Ohma and Kazuhiko Shinohara
Analytical techniques were investigated for examining the influence of the ionomer network structure on proton transport in the catalyst layers of a polymer electrolyte fuel cell. It was verified that the proton transport resistance of a pseudo catalyst layer consisting of a carbon black support and ionomer between two membranes as an intermediate layer (IL) was estimated by a hydrogen pump technique. Using the technique, the effective proton conductivity of ILs with different carbon supports was investigated. It was found that the effective proton conductivities differed. An analysis of the difference revealed the following two possible causes. One is that the Bruggeman factor of the samples might have been affected by the state of ionomer coverage. Another is that the proton conductivities of the ionomer as bulk differed, which might have been due to a difference in water content attributable to the carbon supports.
1763
Dzmitry Malevich, Ela Halliop, Brant Peppley, Jon Pharoah and Kunal Karan
The influence of humidity of supplied gases on on electrochemically active surface area and charge transfer resistance in cathode process of PEM fuel cell was studied. Impedance spectra for cells operated with various gas stream combinations - H2/Air, H2/O2, H2/H2 and H2/N2 - was analyzed to determine the physical/chemical origin of the spectra features. Cathode charge transfer resistance increased with a decrease in the humidity of supplied gases. As well, a reduction in the electrochemically active surface area with a decrease in relative humidity was observed.
1775
Yuxiu Liu, Chunxin Ji, Daniel Baker, Wenbin Gu, Jacob Jorne and H. A. Gasteiger
Dependence of electrode proton resistivity on electrode thickness, Pt-loading, and ionomer equivalent weight (EW) was investigated using Pt/Vulcan catalyst. The proton resistivity, an intrinsic electrode property, is independent of the electrode thickness and Pt-loading, but depends on the ionomer EW.
1787
Alex Bauer, David P. Wilkinson, Elod Gyenge, Dan Bizzotto and Siyu Ye
The potentiostatic electrodeposition of platinum onto gold coated Si wafers and a gold rotating disk electrode (RDE) was carried out with non-ionic surfactants that functioned as templating agents to obtain mesoporous deposits with size features in the nanometer range. The particle size and morphology were studied by surface analysis (SEM and AFM). The electrochemically active surface area of Pt electrodeposited onto the RDE by using a mixture of Brij 56 and n-heptane was increased by a factor of ~2 compared to Pt deposited without structure directing additives. Corresponding oxygen reduction tests at 2500 rpm revealed an improvement of about 14 % (from 5.9 to 7.2 x 10-4 A cm-2) for the cathodic current density at 0.9 V vs. RHE while the mass transfer limited current density was increased by ~25 % from 4.4 to 5.5 x 10-3 A cm-2.
1795
Phillip Baker, Robert P. Brooker, H. R. Kunz, Leonard Bonville and Richard Parnas
Silicotungstic acid (STA), a heteropolyacid, was added to the electrode of polymer electrolyte membrane fuel cells (PEMFCs) and evaluated for increased performance at high temperature and low relative humidity (RHs). Activity was shown to increase for cells containing STA by as much as 35% at 118{degree sign}C/40%RH compared to the cells at 78{degree sign}C/100%RH. Additionally, STA was shown to decrease the fluoride emission rate (FER) by an order of magnitude compared to cells with no additive.
1801
Jack R. Ferrell, John A. Turner and Andrew M. Herring
In this study, polarization experiments were performed on a direct dimethyl ether fuel cell (DMEFC). The experimental setup allowed for independent control of water and DME flow rates. Thus the DME flow rate, backpressure, and water flow rate were optimized. Three heteropoly acids, phosphomolybdic acid (PMA), phosphotungstic acid (PTA), and silicotungstic acid (STA) were incorporated into the anode catalyst layer in combination with Pt/C. Both PTA-Pt and STA-Pt showed higher performance than the Pt control at 30 psig of backpressure. Anodic polarizations were also performed, and Tafel slopes were extracted from the data. The trends in the Tafel slope values are in agreement with the polarization data. The addition of phosphotungstic acid more than doubled the power density of the fuel cell, compared to the Pt control.
1811
Zhong Xie, Titichai Navessin, Xinsheng Zhao, Makoto Adachi, Steven Holdcroft, Tetsuya Mashio, Atsushi Ohma and Kazuhiko Shinohara
Aggregation of Nafion in water and in n-propyl alcohol (NPA)/water and its influence on the size of Pt/C agglomerates in catalyst inks has been studied by Dynamic Light Scattering (DLS). DLS shows that Nafion more strongly aggregates in water than in NPA/water. This is believed to be responsible for differences found in FC performance for catalyst layers prepared from these two different dispersion media.
D3.1: Anion–Exchange Membrane Fuel Cells
1819
John R. Varcoe, Marion Beillard, Dost M. Halepoto, Jamie P. Kizewski, Simon Poynton and Robert C. T. Slade
This paper and the associated presentation will describe the latest developments regarding alkaline anion-exchange membrane (AAEM) fuel cells at Surrey. The program of work conducted has been targeted at the materials development of both membranes and electrodes containing alkaline ionomers and as such has focused on H2/O2 fuel cell testing. Radiation-grafted AAEMs can be made with fully hydrated thicknesses between 18 - 80 μm with conductivities in water of up to 0.06 S cm-2 at 60oC. A peak power density of 230 mW cmgeo -2 and a maximum current density at full discharge of 1.3 A cmgeo -2 have been obtained in a H2/O2 fuel cell at 50oC with a 18 μm AAEM and Toray carbon paper based electrodes (Pt/C(20%mass), 0.5 mgPt cmgeo -2 loading) that were treated with Surrey's first generation alkaline ionomer. A future priority is the development of the next generation alkaline ionomer.
1835
Antonio Filpi, Massimiliano Boccia and H. A. Gasteiger
H2/O2 AMFCs enable the use of Platinum Group Metal (PGM) free Membrane Electrode Assemblies (MEAs), especially for the Oxygen Reduction Reaction (ORR). A promising catalysts for the ORR (Acta's "K14"), has been developed and tested using Rotating Disk Electrode (RDE) analysis, showing promising performance. In this paper we characterize current Anion-Exchange Membranes (AMs), show the fuel cell activity of AM-based MEAs prepared with K14 ORR catalyst, and compare their performance with the kinetic and ohmic limits projected from the membrane and catalyst properties. The data and projections show promising results for this technology.
1847
Steven R. Ragsdale and Chris B. Ashfield
The oxidation of caustic, crude glycerin in a passive direct-fuel cell using an alkaline anion-exchange membrane (AAEM) at ambient temperature is reported. Glycerin is a byproduct of the biodiesel production process and the recent surge in biodiesel production has resulted in increased and underutilized glycerin supplies. The described AAEM fuel cell uses crude glycerin directly and eliminates the need for costly neutralization, distillation and purification procedures. The AAEM fuel cell using crude glycerin demonstrated five times greater energy density than a comparable direct-methanol fuel cell. The enhanced energy density is attributed to the AAEM and glycerin fuel combination, which allows for significantly higher fuel concentrations to be used, a consequence of the AAEM reducing fuel-crossover and preventing water-management problems at the cathode. The described fuel cell performance and demonstrated energy densities could facilitate the use of fuel cells in portable power applications, particularly for low-watt, hand-held mobile electronic devices.
1855
Diogo M. Santos and Cesar A. Sequeira
Potential step experiments were carried out with a Au disc electrode in alkaline sodium borohydride solutions of varying concentrations and temperatures. Analysis of the current transients for the full timescale enabled the delimitation of the domains where diffusion, electron transfer, and mixed control prevail. Chronoamperometric measurements in the diffusion controlled region led to current transients exhibiting Cottrellian behaviour, from which accurate diffusion coefficients, D, were estimated. Arrhenius plots of D allowed determination of the diffusion activation energies, Ed, and maximum diffusion coefficients, D0. Chronocoulometric measurements generated Anson plots from which the kinetic rate constants, k, and charge transfer activation energies, Ect, were calculated. Analysis of the current densities in conditions of infinite mass transfer led to Tafel plots from which exchange current densities, i0, transfer coefficients, α, standard rate constants, ks, and standard activation energies for charge transfer, Ect0, were determined. Purely charge transfer regimes were never observed for the studied applied potentials.
1869
Gholamreza Rostamikia and Michael J. Janik
Direct Borohydride Fuel Cells (DBFCs) have the potential to generate high power densities for use in portable power applications. Despite the potential of DBFC's, current applications are limited in part, by the lack of an effective anode electrocatalyst. Though a number of pure metals and alloys have been tested as anodes, gold and silver electrodes are uniquely capable of completing direct oxidation at near 100% coulombic efficiency. Overpotentials on Au anodes, however, limit the overall cell efficiency and little is known of the elementary electrocatalytic mechanisms, reaction intermediates, or limiting elementary steps . In this study, we apply density functional theory (DFT) calculations to examine borohydride electro-oxidation over the Au(111), and compare with Pt(111) surfaces for which non-selective hydrolysis paths compete with direct oxidation. Possible stable surface intermediates and limiting elementary steps are identified and results are discussed in comparison with experimental data from the literature.
A3.2: Bipolar Plates
1879
Heli Wang and John A. Turner
Duplex 2205 stainless steel was deposited with ˜0.6 µm thick SnO2:F coating; coated steel was characterized for PEMFC bipolar plate application. Compared with bare alloy, interfacial contact resistance (ICR) values of the coated 2205 steel are higher. SnO2:F coating adds its own resistance to the air-formed film on the steel. In a PEMFC anode environment, a current peak of ca. 25 µA/cm2 registered at ca. 30 min for coated 2205 steel. It stabilized at ca. 2.0~-1.0 µA/cm2. This peak is related to the complicated process of coating dissolution and oxide-layer formation. Anodic-cathodic current transfer occurred at ca. 200 min polarization. In a PEMFC cathode environment, current was stable immediately after polari¬zation. The stable current was ca. 0.5~2.0 µA/cm2 during the entire polarization period. AES depth profiles with tested samples and ICP analysis with the tested solutions confirmed the excellent corrosion resistance of the SnO2:F coated 2205 alloy in simulated PEMFC environments.
1891
Cortney K. Mittelsteadt and William Braff
An advanced composite bipolar plate is described for a unitized regenerative fuel cell and electrolyzer system that operates on pure feed streams (H2/O2 and water, respectively). The composite bipolar plate can greatly simplify "closed-loop" unitized fuel cell/electrolyzer power systems, as it eliminates the need for saturators, a second stack, and water/gas phase separation equipment. It provides a substantial system improvement over presently used alkaline systems in that it allows for simple high pressure electrolyzer operation with a high differential pressure. Additionally, it allows for dead-ended H2 and O2 feed during fuel cell operation, eliminating parasitic pumping losses required for water removal in a conventional fuel cell. Results from a 50 cm2 bench design are presented. Additionally, the composite bipolar plate has been used to deliver methanol vapor to a direct methanol fuel cell, resulting in a lower methanol concentration at the catalyst/membrane interface and reduced methanol cross-over.
1901
Katsuhide Kikuchi, Ikuyasu Kato, Makoto Yoshida, Mikio Wada and Seiji Mizuno
The commercialization of metal bipolar plates for polymer electrolyte fuel cells (PEFCs) requires excellent corrosion resistance, and low costs are also demanded. It is thus important to have an accurate grasp of the corrosive environment. In this study, we developed equipment that measures potential and pH around the surface of a bipolar plate during power generation in real time. The corrosive environment revealed that the cathode side at the time of Open Circuit (OC) is the severest. Moreover, it became clear that due to differences in pH the potential on the surface of a bipolar plate is relatively low compared with that of a catalyst layer.
1907
Rachid Zaffou, Robert P. Brooker, H. R. Kunz, Leonard Bonville and Richard Parnas
Light-weight, porous bipolar plates were developed that are ideally suited for use with phosphoric acid-doped polybenzimidazole membrane fuel cells. The porous nature of the bipolar plates allows for a reservoir of acid to remain in intimate contact with the MEA to replenish lost acid. Single-cell and 4-cell stack data show good repeatability, both in flow distribution and performance scans. Over 1000 hour endurance data show performance losses are due to MEA decay, and not bipolar plate corrosion.
1915
Omar E. Herrera, Walter Merida and David P. Wilkinson
We report on the separation of anodic and cathodic potentials in a working fuel cell via reference electrodes at constant conditions. The reference electrodes consisted of four platinized platinum electrode wires and two patches of the same catalyst layer used in the anode. All the reference electrodes were unaffected by the operating conditions of the fuel cell and those with patches provided the most stable potentials. Additional sensing electrodes were placed at the fuel and oxidant inlet and outlet to provide localized information on the operating conditions and the state of the membrane electrode assembly (MEA). Our results show that this type of sensing electrode system can be used to detect flooding, dehydration, and low stoichiometry events, while the reference electrodes provide detailed behavior of the anode and cathode potentials.
1927
Bien H. Chiem, Paul Beattie and Kevin Colbow
Ballard's Technology "Road Map" (TRM) highlighted the automotive fuel cell performance targets Ballard planned to meet on an annual basis, as the company progressed toward its goal of developing commercially viable fuel cell stack technology. These evaluation activities culminated in the most recent demonstration of a stack design in 2007 that met the cost (< US$57/kWnet), power density (>1900 Watts/Litre), durability (>5000 hours under a dynamic load profile and freeze-start capability (from -30C to 50% power in <130 seconds) targets that were on the path to satisfy the 2010 interim objectives. The stack technologies developed as part of the TRM initiative were leveraged into other product areas such as materials handling. Ballard recently completed the sale of its automotive fuel cell assets. As a result, the company is now shifting focus to the development of stack technology for non-automotive applications.
B3.2: MEA Degradation
1939
R. Mukundan, John Davey, Roger Lujan, Jacob Spendelow, Yu Seung Kim, Daniel S. Hussey, David Jacobson, Muhammad Arif and Rodney L. Borup
The effect of MEA preparation on the performance of single-PEM fuel cells operated at sub-freezing temperatures is presented. The cell performance and durability are dependent on the MEA and are probably influenced by the porosity of the catalyst layers. When a cell is operated isothermally at -10 oC in constant current mode, the voltage gradually decreases over time and eventually drops to zero. AC impedance analysis indicated that the rate of voltage loss is initially due to an increase in the charge transfer resistance and is gradual. After a period, the rate of decay accelerates rapidly due to mass transport limitations at the catalyst and/or gas diffusion layers. The high frequency resistance also increases over time during the isothermal operation at sub-freezing temperatures and was a function of the initial membrane water content. LANL prepared MEAs showed very little loss in the catalyst surface area with multiple sub-freezing operations, whereas the commercial MEAs exhibited significant loss in cathode surface area with the anode being unaffected. These results indicate that catalyst layer ice formation is influenced strongly by the MEA and is responsible for the long-term degradation of fuel cells operated at sub-freezing temperatures. This ice formation was monitored using neutron radiography and was found to be concentrated near cell edges at the flow field turns. The water distribution also indicated that ice may be forming mainly in the GDLs at -10 oC and could be concentrated in the catalyst layer at -20 oC.
1951
Marianne Rodgers, Rohit Agarwal, Benjamin P. Pearman, Bo Li, Darlene Slattery, Pyoungho Choi, Nahid Mohajeri, Leonard Bonville, H. R. Kunz and James M. Fenton
Durability studies were carried out on membrane electrode assemblies (MEA)s containing commercial Nafion® and perfluorinated ionomer/PTFE composite membranes that include the incorporation of phosphotungstic acid (PTA). Fuel cells were run for 100 hours at 30% relative humidity, 90 and 100 oC, and open circuit voltage. The voltage was monitored during the durability test, as was the condensate water for presence of fluoride ions. Crossover current, electrochemical active areas, and polarization curves were evaluated pre- and post- test. Improved degradation behavior was observed for the perfluorinated ionomer/PTA/PTFE composite membranes compared to the commercial Nafion® membranes under both testing conditions. Knowledge of the effect of operating conditions on the properties of a MEA over time provides important degradation information that can be used in the design of long-lasting MEAs.
1961
Tatsuya Hatanaka, Tomohiro Takeshita, Hajime Murata, Naoki Hasegawa, Takashi Asano, Masaya Kawasumi and Yu Morimoto
Our approach focusing on Pt catalyst degradation, carbon corrosion and membrane degradation is reviewed in this paper. For Pt catalyst degradation in potential cycle test, the quantitative TEM image analysis and 1-D chemical engineering model was applied. The Pt particle distribution after the durability test could be explained by the Pt ion diffusion model. For carbon corrosion mitigation, vertically aligned carbon nanotube electrodes were applied. For membrane degradation understanding, membranes with intentionally introduced Pt-band was applied and revealed their higher fluoride emission rate. These results and further efforts would lead us to develop more durable PEFC system.
1967
Osamu Yamazaki, Hideki Shintaku, Yasuharu Oomori and Takeshi Tabata
Long-term continuous operation test under the actual operation condition in the system was carried out for more than 24,000 hrs using full-size cell stack manufactured by Sanyo Electric Corp.. Degradation tendencies of CO tolerance of anode and gas diffusivity of cathode were evaluated quantitatively by measuring the voltage drop by high concentration CO poisoning and air utilization dependence on the voltage. Accelerated degradation method concerning the gas diffusivity of cathode developed by Sanyo was verified. Accelerated magnifying power of gas diffusivity was calculated as about 2,100.
1977
Soowhan Kim, Manish Khandelwal, Charles Chacko and Matthew Mench
Performance loss can result from local or partial interfacial delamination between the catalyst layer and diffusion media, or peeling of the catalyst layer from the membrane. Under frozen conditions, experimental freeze/thaw testing of a polymer electrolyte fuel cell (PEFC) has revealed damage due to a local delamination in the soft goods, resulting in an increase of ohmic resistance. To study the impact of local delamination on performance, a two-dimensional anisotropic model was developed. To identify key parameters independently of particular material properties, a dimensionless ratio approach was taken. The model was then validated with experimental results from a model cell designed to simulate a gap between diffusion media and catalyst layers. Localized interfacial delamination of the polymer electrolyte membrane (PEM)|catalyst layer(CL) and CL|diffusion media were found to increase ohmic resistance significantly. The main engineering parameters which control the extent of damage when anomalous delamination occurs were determined with parametric study.
1987
Cheng Huang, Zhong-Sheng Liu and Deqiang Mu
The purpose of this work is to establish a theoretical framework for modeling of the interface changes between the MEA components of PEM fuel cells due to load cycles. A 2D finite element model with the cohesive zone model and the fractional contact model is proposed to simulate the interface changes due to hydrothermal cycles. The material properties as functions of temperature, humidity and strain rate are applied here. The stress-strain simulations show stress and strain distributions inside the MEA, how and where, the interface changes take place during the load cycle and the cause of membrane thinning.
1997
Masahiro Ide, Yutaka Suzuki and Hironosuke Ikeda
The analysis and the clarification of the deterioration phenomena of MEA for the practical use of PEFC are important. For this purpose, we carried out the investigation of MEA which was made of well-defined materials throughout well-defined process of manufacturing. The long term durability test was conducted for the improvement of cell operations. Various performances were measured periodically by electrochemical measurements. The cells were disassembled periodically to observe the change of materials that composed MEA. The deterioration phenomena of the cells were revealed.
C3.2: Electrode Materials and Processes II
2009
Ingo A. Schneider, Michael Bayer, Pierre Boillat, Alexander Wokaun and Guenther G. Scherer
In this talk, we present key results obtained in our laboratory using local electrochemical impedance spectroscopy (EIS), local cyclic voltammetry (CV) and current step technique as well as through plane and in plane neutron radiography in PEFCs. It is shown that processes along the gas flow channels have a tremendous impact on the local and the overall transient response of technical PEFCs. Their identification and consideration is crucial for a meaningful interpretation of results.
2021
Roland Friedmann and Trung V. Nguyen
For optimal performance and high durability PEM fuel cells run at high water saturation levels. Excess liquid water can block pores in both the gas diffusion layer and the catalyst layer and reactant gasses can't access the active catalyst sites. Thus, to prevent electrode flooding the catalyst layer structure has to provide pathways for both gas and liquid water transport as well as high ionic and electronic conductivity. This study presents a 2-step preparation method for such a catalyst layer and also gives an optimal composition of the catalyst ink resulting in high fuel cell performance. Teflon® has been incorporated into the catalyst layer to provide a hydrophobic pathway without blocking active catalyst sites. In general, less Nafion® content needed more Teflon® in the catalyst ink. The optimal ratio was found to be C:Nafion®:Teflon® = 1:0.875:0.875.
2031
Bruno G. Pollet
A novel Sonoelectrochemical method for preparing catalyst layers for Proton Exchange Membrane Fuel Cell (PEMFC) is described. In order to optimize the system, initial studies focused on potentiostatic platinum electrodeposition on glassy carbon (GC) disc electrodes in the absence and presence of ultrasound (20 kHz, up to 29 W.cm-2) and at (313 {plus minus} 1) K. It was found that ultrasound affects significantly the electrodeposition process of Pt on GC electrodes, i.e. increased limiting currents were observed compared to those obtained under 'silent' conditions (no agitation). Platinum loaded on Nafion-bonded carbon anodes were prepared in K2PtCl4 aqueous solutions by galvanostatic pulse electrodeposition in the absence and presence of low-frequency high-power ultrasound; and MEAs were fabricated by conventional method. It was found that electrodes prepared sonoelectrochemically showed better performance compared to those prepared by (i) galvanostatic pulse method only (i.e. in the absence of ultrasound) and (ii) conventional method.
D3.2: Alkaline Membrane Fuel Cell Catalysts
2045
Michele Piana, Stefano Catanorchi and H. A. Gasteiger
Working in the area of alkaline fuel cell and electrolyzer technology, Acta S.p.A. developed over the past two years catalysts without Platinum Group Metals (PGM), named K14 and K18, with high activity for the oxygen reduction reaction (ORR) in alkaline medium. The comparison of the ORR activity between K14, K18 and commercial 10 wt% Pt on Vulcan XC-72R at 0.9 V vs. RHE (Reversible Hydrogen Electrode) has been carried out using Rotating Disk Electrode (RDE) analysis in 0.1 M KOH, showing how K14 has an activity close to Pt/C while the ORR activity of K18 is significantly higher. An important advantage of this catalysts is the absence of any oxidation reaction with fuels like alcohols. We used the Rotating Ring-Disk Electrode (RRDE) to detect the peroxide production and to demonstrate for K14 and, most of all, for K18 the almost complete conversion of oxygen via the 4 electrons mechanism.
2057
Dane C. Hansen, Gerald Watt, Joey Nichols, Merrit B. Andrus, Dean R. Wheeler and Sang H. Choi
Investigation of viologen-based organic catalysts has shown them to be capable of directly oxidizing various sugars. Methyl viologen has been studied using oxygen uptake vial experiments, NMR analysis, and electrochemical methods. We have found that under appropriate conditions this catalyst is capable of completely oxidizing glucose to form carbonate. The preliminary performance of this catalyst in an alkaline fuel cell is also demonstrated.
D3.3: Anion–and Cation–Exchange Membranes for Direct–Fuel Fuel Cells
2067
Takuro Hirakimoto, Kazuaki Fukushima, Yongming Li, Shuichi Takizawa, Koichiro Hinokuma and Tadashi Senoo
A fullerene-based compound with proton-conductive functional groups was synthesized and characterized for fuel cell applications. The fullerene-based proton conductor was mixed with polyvinylidene difluoride (PVdF) as a binder to form the electrolyte membranes. The film property can be tuned by changing the ratio of the fullerene derivatives. The proton conductivity of the electrolyte membranes with 67 wt % fullerene derivative was higher than 4.5 × 10-3 S cm-1 at 25 {degree sign}C under relative humidity (RH) of 70%. The membrane-electrolyte assemblies with these materials showed high DMFC performance under ambient conditions.
2073
Dai Yamamoto, Keiji Sasajima, Hirokazu Munakata and Kiyoshi Kanamura
Three kinds of proton conducting composite electrolyte membranes with three-dimensionally ordered macroporous (3DOM) polyimide were fabricated. Their performances for direct methanol fuel cells were compared. Poly (2-acrylamido-2-methylpropane sulfonic acid) (PAMPS), sulfonated poly (1,4-phenylene ether ether sulfone) (SPEES), and sulfonated poly (1,4-phenilene ether ether ketone) (SPEEK) were employed as filling electrolytes. No swelling was observed in any composite membrane. The highest proton conductivity of 7.4 x 10-2 S cm-1 was obtained for composite membrane with PAMPS having the highest ion exchange capacity. On the other hand, the lowest methanol permeability of 1.3 x 10-6 cm2 s-1 was obtained for composite membrane with SPEEK having the lowest water uptake. The contribution of 3DOM polyimide to the methanol permeability was larger than to the proton conductivity. Thus, two orders of magnitude larger proton transfer selectivity of 1.1 x 106 S cm3 s-1 compared to Nafion membrane was obtained in the SPEEK composite membrane.
C3.3: Supports
2083
Natalia P. Lebedeva, Arend S. Booij and Gaby J. Janssen
Electrodes for the PEMFC were made from 40 wt% Pt on ordered mesoporous carbon (OMC) and their performance as cathodes in PEMFC fuel cells was evaluated. Good activity for the oxygen reduction reaction was found resulting in mass activities better than observed with commercial catalysts. The mesopores in the OMC were in the order of 3.6 nm, which did not prevent a high utilization of the Pt. However, the oxygen transport was very poor in these electrodes, suggesting the mesopores are easily blocked by ionomer and water.
2093
Amar P. Yadav, Yuu Sugawara, Atsushi Nishikata and Tooru Tsuru
The oxidation behavior of a sputtered carbon electrode has been investigated in 0.5 M H2SO4 solution with the help of an electrochemical quartz crystal microbalance (EQCM). The mass change response of the carbon coated Au-QCM during potential cycling showed an increase of mass due to adsorption of water or bisulfate ion just after observation of an anodic peak for the oxidation of hydroquinone. A mass loss due probably to the evolution of CO2 gas was observed at potential above 1.3 V vs. SHE during anodic scan. During cathodic scan, a loss of mass due to release of water or bisulfate ion was accompanied by the reduction of quinone to hydroquinone. By comparing the result of carbon coated QCM with that of highly ordered pyrolytic graphite (HOPG), the mechanism for the oxidation of carbon in acidic medium is discussed.
2101
Siyu Ye, Miho Hall and Ping He
Cost and durability are major challenges for the commercialization of polymer electrolyte membrane (PEM) fuel cells. Accordingly, there remains a need in the art to understand the degradation of fuel cell components and to develop design improvements to mitigate or eliminate such degradation. Carbon support corrosion and Pt dissolution/aggregation are considered as the major contributors to the degradation of the carbon-supported Pt or Pt alloy catalysts. This paper will provide recent advances at Ballard in the performance and stability improvement of the carbon supported Pt and Pt alloy catalysts in PEM fuel cells. An accelerated stress test (AST) has been developed and used to evaluate the degradation resistance of different cathode catalyst materials and structures. It is demonstrated that the morphology, physical and chemical characteristics of these carbon supports have significant effects on the performance and stability of the electrocatalysts.
A4.1: Water Management Misc.
2117
Takuya Hoshiko, Hironori Nakajima, Toshiaki Konomi, Tatsumi Kitahara and Shoichiro Kita
We have analyzed the impedance of the cathode of a polymer electrolyte fuel cell (PEFC) to estimate oxygen diffusion distance, d. Assuming planar oxygen diffusion in a thin liquid water layer at the cathode unconventionally, we can regard d as water layer thickness adjacent to the cathode catalyst layer. Calculated values of d agree well with our previous experimental result of liquid water accumulation amount at the cathode. Measurement of impedance variation with time reveals that d initially tends to be almost constant with time after start-up from dry condition, but that excessive water accumulation due to long time operation causes an increase in d. From the viewpoint of the diagnosis, an exceeding increase in d can be used to indicate the flooding at the catalyst layer.
2125
Partha P. Mukherjee and Chao-Yang Wang
A key performance limitation in polymer electrolyte fuel cells (PEFC), manifested in terms of mass transport loss, originates from liquid water transport and resulting flooding phenomena in the constituent components. Liquid water leads to the coverage of the electrochemically active sites in the catalyst layer (CL) rendering reduced catalytic activity and blockage of the available pore space in the porous CL and fibrous gas diffusion layer (GDL) resulting in hindered oxygen transport to the active reaction sites. The cathode CL and the GDL therefore play a major role in the mass transport loss and hence in the water management of a PEFC. In this article, we present the development of a mesoscopic modeling formalism coupled with realistic microstructural delineation to study the profound influence of the pore structure and surface wettability on liquid water transport and interfacial dynamics in the PEFC catalyst layer and gas diffusion layer.
2133
Jingwei Hu, Pang-Chieh Sui and Ned Djilali
The relationship between predicted cell performance and the microstructures of the porous components such as the gas diffusion layer (GDL) and catalyst layer (CL) is a challenge for proton exchange membrane fuel cell (PEMFC) modelling. In this study, the GDL and CL are reconstructed based on complicated structure generated software GeoDict. The effective transport properties are then derived from reconstructed structures. By incorporating the thus obtained effective transport properties, a two-dimensional, two-phase cathode model is developed to predict the cathodic polarization curve. This study offers a way to correlate microstructures of the GDL and the CL with cell performance.
2145
Vesna Stanic
Hydrogen production in the reactions of sodium brorhydride with various polyhyroxyl compounds was investigated. The reactions were carried out at room temperature and ambient pressure with glycol, glycerol, fructose, and sucrose. The volume of hydrogen was measured during the reactions and compared with the theoretically predicted values. The results show that the hydrogen yield in the reactions of glycol or glycerol is 100%; however, the reactions with fructose and sucrose generated 40% and 70%, respectively, of the expected hydrogen amount.
215
Tomoyuki Tada, Yumi Yamamoto, Koichi Matsutani, Katsuichiro Hayakawa and Tatsunori Namai
After optimization of the preparation procedure and the alloy composition of a PtCo catalyst, we found that MEA of the PtCo catalyst could show better I-V performance than that of a Pt catalyst. To improve the stability of a carbon support, we have evaluated various types of carbon, and we found a graphitized carbon could show better stability than a normal carbon. We also evaluated the PtCo catalyst on the graphitized carbon to achieve both better ORR activity and better stability of carbon, but the PtCo catalyst on the graphitized carbon could not show any ORR activity improvement due to the larger particle size of PtCo. After exploring new carbons, we could find a unique carbon which has higher surface area and better stability than a normal carbon. We prepared the PtCo catalyst on the carbon, and this catalyst could show good balance between the ORR activity and the carbon stability.
C4.1: High Temperature Materials
2157
Pyoungho Choi, Bo Li, Rohit Agarwal, Benjamin P. Pearman, Nahid Mohajeri, Marianne Rodgers, Darlene Slattery, Leonard Bonville, H. R. Kunz and James M. Fenton
Two types of composite membrane were prepared by incorporating phosphotungstic acid (PTA) into host NafionO` membranes; one with 1100 EW of NafionO` and 15% PTA, namely FSEC1, and the other with 750 EW of NafionO` and 15% PTA, namely FSEC3. Catalyst-coated membranes (CCMs) were made using the composite membranes with the 32 wt.% and 25 wt.% ionomer contents in the catalyst layer for FSEC1 and FSEC3 membranes, respectively. The composite membranes were tested in a 25 cm2 single cell at the temperature of 80 oC, 100 oC, and 120 oC and compared to NafionO`112. At 80 oC and 100 oC, the performance of FSEC1 membrane showed the highest and followed by NafionO`112 and FSEC3 membranes. However, both the composite membranes, FSEC1 and FSEC3, outperformed NafionO`112 at 120 oC, showing great potential for their application in the high temperature (~120 oC) operations. At 400 mA/cm2, the potentials maintained were 0.47V, 0.55V, and 0.51V for NafionO`, FSEC1 and FSEC3 membranes, respectively. The resistance of oxygen mass transfer in FSEC3 was pronounced at high temperature as evidenced by oxygen gain at the temperature.
2165
Melinda Einsla, R. Mukundan, Eric L. Brosha and Fernando H. Garzon
We have synthesized various indium-tin pyrophosphates using the traditional high-temperature method described in the literature as well as a novel solution-precipitation process developed in our laboratory. An ammonium-based precursor was used in an attempt to achieve a lower crystallization temperature. The use of this precursor in the solution-precipitation of indium-tin pyrophosphate gels resulted in precursors that could be crystallized at less than 600{degree sign}C. Inelastic neutron scattering studies indicate the presence of phosphate rich grain boundary phases that may be responsible for the high conductivity of the materials.
2171
S Shimpalee, Tao Gu and J. W. Van Zee
The objective of this study is to aid the development of an understanding of the mechanisms of H3PO4 loss and transport in PolyBenzImidazole (PBI)-type High Temperature Membranes (HTM) fuel cells. The isotherms for adsorption and desorption of water in PBI-type HTM are critical data and reported for the first time here for a commercially available membrane. Depending on their values, this adsorption/desorption could play an important role in the long-term dilution of acid and thereby affect (in the long-term) the transport of this acid and proton flux in the membrane. Inclusion of these data is necessary in the development of a mechanistic model that allows for design of new experiments and prediction of fuel cell performance.