Abstract
Fe-N-C catalysts were prepared by impregnating FeCl3 within two kinds of activated carbon (Kuraray GC and Nuchar) that had been previously burned-off at 500oC in air to vary their pore sizes in a controlled way. The impregnated samples were subsequently heated at 850oC in NH3. The average pore size of the samples was determined by small-angle X-Ray scattering (SAXS) measurements and quantified by the radius of gyration (Rg) of the pores. The catalytic activities of the samples vary with the pore size of the activated carbon, which depends on the burn-off time. The results support suggestions from the Dodelet group about the importance of the pore size in determining catalytic activity.