RAPID COMMUNICATIONS
082001
Jie Yang, Zheng-Cai Li, Wei Lu, Wei Yi, Xiao-Li Shen, Zhi-An Ren, Guang-Can Che, Xiao-Li Dong, Li-Ling Sun, Fang Zhou et al
Here we report the fabrication and superconductivity of the iron-based arsenic oxide
GdFeAsO1−δ
compound with oxygen-deficiency, which has an onset resistivity transition temperature
at 53.5 K. This material has the same crystal structure as the newly discovered
high-Tc ReFeAsO1−δ
family (Re = rare
earth metal) and a further reduced crystal lattice, while the
Tc starts to decrease
compared with the SmFeAsO1−δ
system.
082002
C G Zhuang, S Meng, H Yang, Y Jia, H H Wen, X X Xi, Q R Feng and Z Z Gan
We report a significant enhancement in upper critical field
Hc2 and irreversibility
field Hirr in
carbon-doped MgB2
films fabricated by hot-filament-assisted hybrid physical–chemical vapor deposition
(HFA-HPCVD) using methane as the doping source. For the parallel field, a very
large temperature derivative
value of 3 T K−1 near
Tc was achieved in a
heavily doped film with Tc
near 28 K. Carbon doping also enhanced flux pinning, resulting
in a much higher critical current density in a magnetic field
Jc(H)
than in undoped samples. The result suggests a more effective doping of carbon into the
MgB2
structure and a better connectivity between the carbon-doped
MgB2 grains
than in previous reports. A clear correlation between the decrease in grain size and the enhancement
of Hc2
was observed.
082003
Ruslan Prozorov
The superconducting gap and the superfluid density are calculated for the
extended d-wave gap suggested by angle-resolved photoemission spectroscopy
(ARPES) measurements in electron-doped superconductors as well as underdoped
Bi2Sr2CaCu2O8+x
(BSCCO2212). It is shown that experimental superfluid density may agree with such a gap,
but full-temperature range analysis is required. With additional information on the
Δ(0)/Tc
ratio, this opens up the possibility of deciding whether a non-monotonic or higher harmonic
spectral gap, as seen by ARPES, is a superposition of a regular d-wave gap and an
unrelated pseudogap that does not contribute to superconductivity or that the extended
gap is a real superconducting gap. This paper is also an erratum to earlier calculations
published in Prozorov and Giannetta (2006 Supercond. Sci. Technol.19 R41–67) where the
wrong sign was used for the non-monotonic gap, altering the conclusions rather drastically.
082004
Dmytro Abraimov, Alex Gurevich, Anatolii Polyanskii, X Y Cai, Aixia Xu, Sastry Pamidi, David Larbalestier and C L H Thieme
We report on a first implementation of a design which provides a significant reduction of AC losses
in YB2Cu3O7−δ
(YBCO) coated conductors (CCs) without mechanical twisting. The conductor is composed
of two diffusively bonded silver clad commercial CCs with zigzag patterned filaments
partially separated by a dielectric layer. We produced three fully bonded samples with
500 µm
wide filaments using three-stage photolithography and wet chemical etching. A tenfold
reduction of AC losses at frequencies between 20 and 400 Hz was observed, while
transport measurements and magneto-optical imaging showed no degradation of
Tc
and a low contact resistance of
between Ag and YB2Cu3O7−δ.
PAPERS
085001
Tomoyuki Naito, Hiroyuki Fujishiro, Kazumasa Iida, Shinya Nariki and Masato Murakami
We have measured the temperature dependence of the in-plane thermal conductivity,
κab(T), for both Er–Ba–Cu–O and Ho–Ba–Cu–O superconducting bulks. The absolute values of
κab(T)
for both bulks are smaller than that of Y–Ba–Cu–O bulk, but are larger than
that of Dy–Ba–Cu–O bulk, which is known to show an anomalous small
κab.
κab(T) for Ho–Ba–Cu–O
shows a positive slope (dκab/dT>0) in the normal state, similarly to that for Dy–Ba–Cu–O. On the other hand, a slightly negative slope
(dκab/dT<0) is found for Er–Ba–Cu–O. The out-of-plane thermal conductivity,
κc, was also measured for Er–Ba–Cu–O bulk, and the anisotropy in the thermal conductivity,
(κab/κc), was estimated to be about 2.
085002
W M Woch, R Zalecki, A Kołodziejczyk, H Sudra and G Gritzner
Bulk (Tl0.5Pb0.5)Sr2(Ca1−xGdx)Cu2Oz
superconductors with x = 0.1,0.2
and 0.3 were prepared by a wet chemical gel technique followed by a
special heat-treatment procedure. X-ray diffraction analysis revealed
practically phase-pure samples with tetragonal structure (space group
P/4mmm). The temperature dependence of the real and imaginary parts of the ac
susceptibility and the dependence on the ac applied magnetic field were
investigated to learn about the superconducting and magnetic properties of bulk
(Tl0.5Pb0.5)Sr2(Ca1−xGdx)Cu2Oz
superconductors. The critical current densities of the samples were derived from Bean’s
model. The temperature dependence of the critical current was successfully fitted based
on a power law from the thermally activated magnetic flux creep model. From
magneto-resistance measurements the temperature dependences of the transport critical
currents and the irreversibility fields were found. The dc magnetic field dependence of the
width of superconducting transitions and the critical currents was also obtained. These
properties of the superconductors were analyzed within available theoretical models.
085003
R Zeng, L Lu and S X Dou
We report a systematic study of the effects of polymer addition on the
lattice parameters, microstructure and superconducting properties of
MgB2. Polyvinyl
alcohol [−C2H4O−]n
(PVA) as a typical polymer was used as an additive to
MgB2. It was found that PVA additions have the following features: (1) the polymer can have a
very low oxygen (O) content or even none at all, and PVA has a low O content
(C:O = 2:1), which reduces the impurities brought into
MgB2
from the doping, and (2) PVA decomposes at a temperature of
400–650 °C, which means that the reaction occurs in the same temperature range as
MgB2
formation, providing highly reactive C, which homogeneously substitutes for B at this
low-temperature range. The above considerations significantly enhance the critical current,
Jc, the irreversibility
field, Hirr, and the
upper critical field, Hc2, of MgB2
compared to un-doped samples or those doped with other carbon sources. In this work,
suitable PVA doping levels improved both the connectivity and flux pinning, so that the
Jc of
PVA-doped MgB2
was improved over the whole field range.
085004
I M Obaidat, U Al Khawaja and M Benkraouda
We have investigated the role of pinning strength and density on the equilibrium
vortex-lattice to vortex-liquid phase transition under several applied magnetic fields. This
study was conducted using a series of molecular dynamic simulations on several samples
with different strengths and densities of pinning sites which are arranged in periodic square
arrays. We have found a single solid–liquid vortex transition when the vortex filling factor
n>1. We have found that, for fixed pinning densities and strengths, the melting temperature,
Tm, decreases almost linearly with increasing magnetic field. Our results provide direct
numerical evidence for the significant role of both the strength and density of pinning
centers on the position of the melting line. We have found that the vortex-lattice to
vortex-liquid melting line shifts up as the pinning strength or the pinning density was
increased. The effect on the melting line was found to be more pronounced at small values
of strength and density of pinning sites.
085005
Y F Chen, J Li, X P Xu, R L Wang, S L Li, F R Hu, C H Yi and D N Zheng
Superconducting Tl2Ba2CaCu2O8
thin films (Tl-2212) have been reproducibly fabricated on both sides of 2 inch
LaAlO3(001)
substrates by using a so-called two-step process. A simple and flexible horizontal
arrangement inside the crucible during thallination has been proposed, to
ensure a good convection of thallous oxide vapor around the film surface, and
thus a high film quality on both sides. A good uniformity over the whole
area of the films has been realized. The films are strongly textured, with the
c-axis perpendicular to the substrate surface, and they show the fourfold symmetry of the tetragonal
crystal structure. The full width at half maximum of the (002) peak for both films on the best sample
is 0.43°
and 0.55°
respectively. The films exhibit flat terraces with particles and shallow
holes, but free of microcracks. The superconducting critical temperatures
fall in the range 105–108.5 K. The critical current densities are between
1.0 × 106
and 4.8 × 106 A cm−2
at 77 K. The microwave surface resistances at the central area of the films are around
500 μΩ
at 77 K and 10 GHz. These films are suitable for microwave applications.
085006
T Nakamura, K Nagao, T Nishimura, Y Ogama, M Kawamoto, T Okazaki, N Ayai and H Oyama
We report on the direct relationship between output power and the current carrying
capability of a squirrel-cage HTS induction/synchronous motor based on experiment. The
secondary windings are fabricated by use of so-called DI-BSCCO tapes, and the
conventional (normal conducting) stator, three-phase and four-pole, is utilized. The tests
are carried out in liquid nitrogen for two kinds of HTS windings, in which the
number of HTS rotor bars is varied. It is directly shown that the output power
is proportional to the rotor bars’ critical current at 77 K. In other words, the
torque can be enlarged by increasing the critical current of the HTS rotor bars.
085007
S L Samal, S E Lofland, K V Ramanujachary, N Sarkar, S Ghosh and A K Ganguli
The effect of disorder on the suppression of superconductivity has been
studied in two series of high temperature superconducting oxides of the type
Ln1.2Ba1.2Ca0.6Cu3O7+δ
(Ln = La, Nd, Sm)
and La1.2−xNdxBa1.2Ca0.6Cu3O7+δ
(x = 0.3, 0.6, 0.9). These oxides crystallize in the tetragonal structure related to
the 1113-type superconductors. It has been shown that considerable cation
disorder exists at the Ln and Ba crystallographic sites in these oxides.
Furthermore, it has been shown that Ln and Ca ions occupy both the 1d- and the
2h-crystallographic sites whereas Ba ions only occupy the 2h-crystallographic site.
La1.2Ba1.2Ca0.6Cu3O7+δ shows a superconducting
transition with Tc
of 65 K while the Sm analog shows semiconducting behavior. A broad metal–semiconductor transition is
observed in Nd1.2Ba1.2Ca0.6Cu3O7+δ. It has also been shown that the gradual suppression of
Tc in
La1.2−xNdxBa1.2Ca0.6Cu3O7+δ,
as x
increases, is related to disorder which could be related to the variance
(σ2)
of the average ionic radii of the ions at the 2h site.
085008
R L S Emergo, J Z Wu, T J Haugan and P N Barnes
The anisotropy of electrical transport properties of
YBa2Cu3O7−δ
(YBCO) films containing high density nanopores grown on
5°,
10°
and 20°
vicinal substrates was investigated. For porous films in the normal state, the resistivity in the
longitudinal direction is comparable to that of reference YBCO films without nanopores. In addition,
the ρc/ρab
ratios derived from the resistivities in longitudinal and transverse directions of the
porous samples fall in the same range as that of twinned single crystal YBCO. For
the superconducting state, the pore surfaces provide strong magnetic pins to
magnetic vortices, which leads to significantly increased critical current density
Jc
along the longitudinal direction as compared to that of the reference
YBCO films. This strong isotropic pore surface pinning also increased the
Jc
along the transverse direction as compared to that of nonporous vicinal YBCO films. This
result suggests that the effect of nanopores on the electronic structure of YBCO is minimal
and the strong pore surface pinning may provide an effective way to enhance
Jc
after optimization.
085009
Y Shen, R Gandikota, R K Singh, F L Hunte, J Jaroszynski, D C Larbalestier, J M Rowell and N Newman
We report a new method for synthesizing magnesium diboride
(MgB2) thin films which exhibit a steep increase in the slope of the upper critical field
Hc2 versus decreasing
temperature (i.e. |dHc2/dT|Tc|≈2.5 T K−1). An Hc2
of 38.4 T at 4.2 K and an extrapolated value of
Hc2(0)
above 43 T at 0 K are reported. Films of magnesium plus boron were deposited on unheated
c-plane sapphire substrates by co-evaporation, and were subsequently
annealed in a reducing atmosphere at temperatures below
600 °C. The use of a combination of a magnesium-rich stoichiometry
(Mg/B>1/2) for
the as-deposited film and a two-step annealing process was found to be critical in obtaining these high
values of Hc2
and |dHc2/dT|Tc|.
085010
S Vinu, P M Sarun, R Shabna, A Biju and U Syamaprasad
The effect of sintering temperature on the microstructure and superconducting properties of
Bi1.7Pb0.4Sr1.8Nd0.2Ca1.1Cu2.1O8+δ
has been investigated. The samples are prepared by the solid-state
route. Remarkable variations in microstructure, critical current density
(JC)
and flux pinning properties have been observed for Nd-substituted
samples, sintered at different temperatures in the range
846–852 °C. The flux pinning
force (FP) calculated from
the field-dependent JC
values show that the irreversibility lines (IL) of Nd-substituted samples shift towards higher
fields to different extents depending on the sintering temperature. The samples sintered at
846 °C show maximum
flux pinning force (FP) of 631 kN m−3 and the
peak position of FP
shifts to higher fields (0.8 T) as against
262 kN m−3 and 0.44 T for the
samples sintered at 852 °C
and 18 kN m−3 and
0.08 T for the undoped sample sintered at its optimum sintering temperature, respectively. But the self-field
JC value of the
samples sintered at 846 °C
is lower than that of the samples sintered at
852 °C. The samples
sintered at 852 °C show
maximum self-field JC
due to improved microstructure. The changes in microstructure followed by very high enhancement of
self-field JC, JC–B characteristic and
pinning force density (FP) due to Nd substitution within a narrow temperature range, is of great scientific and
technological significance.
085011
Y Tanaka, D D Shivagan, A Crisan, A Iyo, P M Shirage, K Tokiwa, T Watanabe and N Terada
The Abrikosov lattice in the multilayer cuprate superconductor
CuBa2Ca3Cu3Oy
(Cu-1223) has been experimentally and theoretically demonstrated to be composed of
vortex molecules. Cu-1223 is considered to be a typical multicomponent superconductor.
We show that in such a system the rotational freedom around the axis of the vortex
molecular tube generates orientational disorder and the orientational glass (or
crystal) phase, which is never present in conventional vortex lattices consisting
of axisymmetric vortices. The emergence of the orientational glass phase and
orientational order phase with orthorhombic distortion is a general property of
vortex molecule lattices of the multiband type of multicomponent superconductors.
085012
Hua Zhao, Xiang Wang and Judy Z Wu
Third-order intermodulation has been studied in two-pole X-band microstrip
filters made of three high-temperature superconductors (HTS), including
HgBa2CaCu2O6+δ (Hg-1212),
Tl2Ba2CaCu2Oy (Tl-2212)
and YBa2Cu3O7−δ
(YBCO) at ≥77 K. In addition, the dc critical current density
Jc was
investigated in these three types of HTS films in the same temperature range. Interestingly, the dc
Jc and the rf critical
current density JIP3
derived from the third-order intercept (IP3) have a similar dependence on the reduced
temperature, suggesting that the magnetic vortex depinning in HTS materials dominates the
microwave nonlinearity at elevated temperatures. This observation agrees with the recent
theoretical discussion on the origin of the microwave nonlinearity. Disagreement between
Jc and
JIP3, however, has been
observed in the trilayer YBCO/CeO2/YBCO
filters. Although magnetic flux pinning and hence
Jc
were improved by the insertion of a 20 nm thin
CeO2 layer, the
reduced JIP3
is attributed to the high power loss from the extra interfaces between YBCO and
CeO2.
085013
D-X Chen, A Sanchez, C Navau, Y-H Shi and D A Cardwell
The field amplitude and frequency dependent complex ac susceptibility
χ(Hm,f)
of three Y–Ba–Cu–O disks made by a top-seeded melt growth
technique has been measured at 77 K with the ac field applied along the
c-axis of the samples (parallel to their thickness). A procedure based on the
Bean model has been developed to calculate the critical-current density
Jc
near the surface of the sample from the measured
χ(Hm)
for the case where the maximum imaginary component
χ′′
is not reached.
085014
S Mikusu, S Takami, K Tokiwa, K Takeuchi, A Iyo, Y Tanaka and T Watanabe
The crystal structure of the
high-TC superconductor
TlBa2Ca2Cu3O8+δ with different
maximum TC
values (∼132, 126 and 120 K) is investigated by neutron powder diffraction
measurements. The refined values of occupancy for the excess
oxygen(δ) located in interstitial positions on the Tl–O layer, O(4), are
0.775(6), 0.751(16) and 0.813(25) for the samples with a maximum
TC of
∼132,
126 and 120 K, respectively. It is found that the Cu(2)–O(3) bond lengths of samples with higher
TC
are shorter, and the value of this bond length for the Tl-1223 sample with a
TC of
∼132 K is almost equal to that for Hg-1223 with a maximum
TC of
∼135 K. It is also found that the flatness of the
CuO2 planes increases
with increasing TC. It appears that the structural features of the
CuO5
pyramids are among the factors contributing to the higher value of
TC
in cuprate superconductors.
085015
M I Petrov, Yu S Gokhfeld, D A Balaev, S I Popkov, A A Dubrovskiy, D M Gokhfeld and K A Shaykhutdinov
The intragrain pinning in high-Tc
superconductor compounds Y1−xRExBa2Cu3O7−δ
with low concentration of RE (La, Ce, Pr) was investigated. Magnetic and transport
measurements reveal that the pinning is maximal for the concentration of heterovalent RE
such that the average distance between the impurity ions in the plane of rare-earth
elements is close to the diameter of Abrikosov vortices in YBCO.
085016
R Biswal, J John, D Behera, P Mallick, Sandeep Kumar, D Kanjilal, T Mohanty, P Raychaudhuri and N C Mishra
The effect of 200 MeV Ag ion irradiation on the superconducting and normal state properties of the
high-Tc
superconductor YBa2Cu3O7−y
(YBCO) is studied by in situ temperature-dependent resistance
measurements. We show that irradiating YBCO thin films
(∼150 nm) at low temperature result in a softly defected region of about 85 nm radius due to swift
heavy ion-induced secondary electrons around the highly amorphized latent tracks of
∼5 nm radius. This
leads to a decrease of Tc
at fluences three orders of magnitude less than the threshold fluence, where overlapping of
tracks block the supercurrent path. Due to their low energy (4.1 keV for 200 MeV Ag ions),
the secondary electrons can induce point defects by inelastic processes rather than by direct
elastic collision.
085017
Soon-Gil Jung, N H Lee, W K Seong, W N Kang, Eun-Mi Choi and Sung-Ik Lee
We have successfully fabricated
c-axis-oriented MgB2
thin films by using a laser-assisted chemical vapor deposition (LACVD) technique.
Mg and B sources were supplied by pulsed laser ablation and a mixture of
B2H6 gas in
H2, respectively.
The MgB2 thin films
grown on Al2O3(0001)
substrates at 400 °C
showed a superconducting transition temperature of 40.2 K with a sharp
transition width of 0.2 K and a high critical current density of about
107 A cm−2
at 20 K and zero field, suggesting that this low-temperature process would be a
promising technique for electronic devices operating at high temperatures above
20 K.
085018
C H Sun, H S Yang, L Cheng, J B Wang and L Z Cao
The in-plane resistivity (ρ) and thermopower (S) were measured on Nd1.86Ce0.14CuO4+δ
single crystal after different annealing times. Both
S and
ρ can
be described in terms of a two-band model with an electron broad band and a hole-like narrow band.
From ρ
and S
data, we found that the hole component increases with the annealing
time before the optimal superconductivity is achieved, while
S and
ρ reach saturation after
further annealing in N2. So the annealing process has the same effect as Ce doping just before the sample is
optimally annealed, while after that they are not equal to each other. Furthermore, we also
argue that the holes may be responsible for the superconductivity in the electron-doped
cuprates.
085019
S F Wang, Ke Chen, C-H Lee, A Soukiassian, D R Lamborn, R DeFrain, J M Redwing, Qi Li, D G Schlom and X X Xi
A hybrid physical–chemical vapor deposition process using a pocket
heater was developed for the growth of high quality epitaxial large-area
MgB2 thin films
and c-axis
textured MgB2
thick films. This technique is able to independently control the substrate and Mg source temperatures
and maintain sufficient Mg overpressure to ensure phase stability. The two-inch large-area
MgB2 thin
films showed uniform superconducting properties with the superconducting transition temperature
Tc
of about 40 K, residual resistivity ratio (RRR) of about 10, and critical current density
Jc of about
107 A cm−2 (0 T, 5 K). The
thick films (∼10 µm) on sapphire substrates showed a maximum
Tc of 40 K and RRR
of 15, and a Jc
of 1.6 × 106 A cm−2
at low applied magnetic fields even at 20 K. High quality thick films also have been
obtained on metal substrates.
085020
Jaeun Yoo, SangMoo Lee, YeHyun Jung, Jaeyoung Lee, Dzung Nguyen Xuan, Dojun Youm, Hosup Kim, Hongsoo Ha, KyuJeong Song, SangSoo Oh et al
We calculated the current distribution in a coated conductor (CC) from magnetic induction
profiles measured using the scanning Hall probe method. An external magnetic field was applied
in the normal direction with respect to the tape surface and was decreased stepwise from
Hpeak to
−Hpeak. From the hysteretic behavior of the current distributions, the energy loss,
QM, was calculated for
various values of Hpeak. Comparison of the present results with Brandt’s theoretical calculations revealed that his
formula is still valid if one substitutes the magnetic field dependent critical current density
into his equation. The theoretical results obtained were consistent with the experimental
QM
values obtained.
085021
U Sinha, A Sinha and E J Tarte
In this paper, we study transmission line resonances in high
TC
dc SQUIDs (superconducting quantum interference devices). These resonances are exhibited in
the characteristics of SQUIDs which are fabricated on substrates with high dielectric constant,
such as strontium titanate. The power balance equation is analytically derived both for
symmetric and for asymmetric SQUIDs. Using this, we investigate SQUID current–voltage
I(V), voltage–flux
V (Φ) and voltage
modulation ΔV
characteristics.