The reactions of tungsten hexafluoride Equation or symbol description not available(WF6) on stainless steel, tantalum, platinum, nickel, and Monel 400® were investigated using temperature‐programmed desorption and Auger electron spectroscopy in ultrahigh vacuum. The high reactivity of stainless steel and tantalum surfaces indicate that they are not suitable materials for tungsten chemical vapor deposition reactors. Nickel and Monel 400® are much less reactive and are suitable for use below 800K. Platinum does not react with Equation or symbol description not availableWF6 below 600K and may be suitable for use at higher temperatures. Mass spectrometer cracking patterns forEquation or symbol description not availableWF6, Equation or symbol description not availableWOF4, and Equation or symbol description not availableWO2F2 were measured.