The performances of a novel Ru/WHfN barrier against Cu diffusion are compared with those of Ru and Ru/WN barriers by sheet resistance, X-ray diffraction, elemental depth profiles, and leakage–current measurement of metal-oxide-silicon capacitors. For the Cu/barrier/Si samples, both Equation or symbol description not availableRu(10nm) and Equation or symbol description not availableRu(5nm)∕WN(5nm) barriers fail after annealing at 500 and Equation or symbol description not available750°C, respectively. However, the Equation or symbol description not availableRu(5nm)∕WHfN(5nm) barrier can still maintain the perfect ability to prevent Cu penetration at the failure temperature of the Equation or symbol description not availableRu(5nm)∕WN(5nm) barrier. This could be attributed to the fact that the incorporation of Hf into WN greatly enhances the crystallization temperature of WHfN, whose amorphous texture can be maintained after Equation or symbol description not available800°C annealing. In contrast, the WN film begins to crystallize after Equation or symbol description not available700°C annealing, and many of the generated grain boundaries facilitate Cu diffusion through the barrier.