A number of batteries were made in which negative plates formed at 20° F. (−7° C.) were used with positive plates formed at 90° F. (32° C.). Batteries were made in which positive plates formed at 20° F. (−7° C.) were used with negative plates formed at 90° F. (32° C.) A comparison of these batteries showed that low temperature formation of the positive plates decreased their life but increased their initial capacity, while low temperature formation of the negative plates increased the life of the positive plates used with them and little affected the initial capacity. Batteries made with both the positive and negative plates formed at various temperatures showed that as the temperature of formation decreased the battery life decreased, and the initial capacity of the battery increased at most of the usual rates of discharge. The maximum temperature of formation used was 100° F. (38° C.) and the minimum temperature of formation was 20° F. (−7° C.) Many other interesting points about formation, initial capacity and life of the battery, as affected by the temperature of formation, are discussed.