Abstract
We investigated the effects of UV treatment on the device properties of a plasma-enhanced atomic layer deposition (PE-ALD) ZnO thin film transistor (TFT). Remote PE-ALD ZnO thin films were used as active layers for bottom-gate TFT devices. The as-deposited PE-ALD ZnO film at a growth temperature of
has an overly small carrier concentration, which produces a TFT device with no modulation by gate voltage sweep. However, after UV light exposure, the device shows proper TFT modulation by gate voltage. The threshold voltage
of the device can be controlled to the negative direction by increasing the UV exposure time.
moves from 17.8 to −6.5 V with an increase in UV exposure time from 3 to 120 min.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.