This paper reports on metal–insulator–metal (MIM) capacitors comprised of Equation or symbol description not availableAl2O3∕TiO2∕Al2O3 laminate structure with postmetallization-annealing (PMA) treatment. By applying the laminate structure to Equation or symbol description not availableTiO2 capacitors, deposition of the Equation or symbol description not availableAl2O3 layer enables significant leakage current reduction while maintaining good electrical performance. For an Equation or symbol description not availableAl2O3∕TiO2∕Al2O3 film with PMA treatment, the electrical characteristics can be further improved, which is mostly due to the passivation of the dielectric interface charges. We have achieved low leakage current of Equation or symbol description not available6.4×10−9A∕cm2 at Equation or symbol description not available1V for Equation or symbol description not available18.3fF∕μm2 density Equation or symbol description not availableAl2O3∕TiO2∕Al2O3 MIM capacitors. These results meet the International Technology Roadmap for Semiconductors requirements (year 2018) of Equation or symbol description not available10fF∕μm2 density and Equation or symbol description not availableJ∕(CV)<7fA∕(pFV).