Abstract
Both work function and interfacial oxide thickness control were attempted using
bilayered metal electrode on
. The flatband voltage, directly related to the work function, with an approximate span of
could be controlled by changing the Hf thickness. The interfacial oxide thickness was decreased with increasing the Hf thickness due to the high reducing capability of the Hf film, and the interface state density was reduced. However, Hf films thinner than
were needed to avoid the leakage current degradation caused by the diffusion of metallic Hf into the
during postdeposition annealing.