Abstract
The effect of proportion of antimony in grid metal on the rate of self discharge of lead‐acid storage batteries was investigated over the range 0.5% to 12% Sb with the conventional type of cells, and also with the low discharge (LD) type of construction. As the proportion of antimony in the grid metal increases, the rate of self discharge increases. This rate is higher and accelerates upward more rapidly at 125° F (51.7° C) than at 80° F (26.7° C). To produce a cell really free from self discharge the use of pure lead metal for grids is required. Alloys with 1% to 2% Sb are difficult to cast into grids and therefore are not practical. Tellurium, where added to pure lead grid metal to the extent of 0.06%, does not markedly affect the self discharge of cells and does not contribute appreciably to the mechanical properties of the grid. Negative plates lose power on standing from 2 to 5 times faster than do the positive plates. As the concentration of electrolyte increases from 1.250 sp. gr. to 1.400 the rate of self discharge increases slowly for cells with pure lead grids and rapidly for those with antimonial lead grids. As the length of test on open circuit becomes longer the rate of self discharge decreases somewhat. Low discharge cells with pure lead grids were found to lose capacity so slowly at 80° F (26.7° C) that after a 35 month period of standing on open circuit they still had half of the original capacity left available. At 125° F (51.7° C) they lose capacity much more rapidly, but even then not materially exceeding the rate for the conventional batteries at 80° F (26.7° C). The material of separators, comparing treated wood with rubber, does not affect self discharge. Cell design, however, as it depends on the design of the grids, does affect the self discharge behavior of antimony.
Access this article
The computer you are using is not registered by an institution with a subscription to this article. Please choose one of the options below.