A study of the effect of varying the forming temperature, on both the composition of the positive plate active material and the self‐discharge of the positive plates, shows that between + 70° C. and approximately −2° C. a decrease in the forming temperature is accompanied by a decrease in the percentage of indicated Equation or symbol description not availablePbO2 and by an increase in the percentage of an as yet unidentified compound which has been designated “apparent Equation or symbol description not availablePbO.” The color of the active material also varies with the forming temperature, as does the rate of anodic local action of the freshly prepared positive plates. The principal anodic self‐discharge reactions are discussed. Other pertinent information is given.