Reversible electrochemical intercalation of Li into the Equation or symbol description not availableLi1−xTiyV1−yS2 dichalcogenides, which was frustrated in the 1970s by the use of Equation or symbol description not available1M Equation or symbol description not availableLiClO4 in propylene carbonate as the electrolyte, is reinvestigated with Equation or symbol description not available1M Equation or symbol description not availableLiPF6 in ethylene carbonate:diethyl carbonate (1:1). The choice of the electrolyte allows full electrochemical cycling between Equation or symbol description not availableMS2 and Equation or symbol description not availableLiMS2 (Equation or symbol description not availableM=V or Equation or symbol description not availableTi0.3V0.7). The as-prepared Equation or symbol description not availableLizMS2 Equation or symbol description not available(z≈0.9) samples were fully lithiated after the first discharge, and from a subsequent charge of Equation or symbol description not availableLiVS2 to Equation or symbol description not availableVS2, the room-temperature solubility limits of the parent 3S phase, the Li-rich hexagonal phase, the intermediate α and β phases, and the hexagonal Li-poor hexagonal phase have been determined. Introduction of Ti in Equation or symbol description not availableLiTi0.3V0.7S2 remarkably improves the capacity at high cycling rates and increases the voltage by about Equation or symbol description not available0.2V.