By electrochemical oxidation of Equation or symbol description not availableNaCrS2 in Li cells, phases of the typeEquation or symbol description not availableNaxCrS2 Equation or symbol description not available(x≥0.1) have been prepared, which provide host structures for Li+ intercalation. More than 1 eq. Li+/mole Equation or symbol description not availableNaCrS2 may be reversibly intercalated at sufficiently high rates. The three‐dimensional layered structure of these phases proves to be particularly rugged, thus allowing repeated cycling with minor performance losses. The high potentials of Equation or symbol description not availableLi/NaxCrS2couples allow high energy densities to be obtained. Starting from a theoretical value of 518 W‐hr/kg, a calculation based on the performance at 1.0 mA/cm2 and on the real battery weight still gives a value of 142 W‐hr/kg for an 8 hr discharge rate. Values of the Li+ chemical potential in Equation or symbol description not availableNaxCrS2 and of the free energy of intercalation have large negative values typical of efficient chalcogenide cathodes. Nonlinearly and continuously decreasing Equation or symbol description not availableE‐xplots seem to indicate the formation of a single phase through Li+ occupation of energetically different lattice sites.