Extended microtunnels with triangular cross sections in thick GaN films were demonstrated using wet chemical etching on specially designed epitaxial lateral overgrowth structures. For tunnels along the Equation or symbol description not available⟨11¯00⟩ and Equation or symbol description not available⟨112¯0⟩ directions of GaN, the Equation or symbol description not available{1122¯} and Equation or symbol description not available{101¯1¯} facets are the etch stop planes with activation energies of 23 kcal/mol determined by wet chemical etching. The axial etching rate of the tunnels in the Equation or symbol description not available⟨11¯00⟩ direction is twice as large than that along the Equation or symbol description not available⟨112¯0⟩ direction. The highest etching rate of the tunnels in the axial direction is Equation or symbol description not available1000μm/h.