Abstract
Tantalum nitride
atomic layer deposition (ALD) was performed using sequential exposures of (tert-butylimido)tris(diethylamido) tantalum (TBTDET) and either hydrazine
or ammonia
. X-ray reflectivity studies demonstrated that hydrazine consistently yielded
films with larger growth rates and higher densities than the
films grown using ammonia. The
ALD growth rate of
using hydrazine was higher than the growth rate obtained using ammonia over the temperature range from
. Quartz crystal microbalance measurements were also used to confirm the
ALD growth rates and to verify the self-limiting behavior of each reactant. Hydrazine yielded a
density of
at
that was significantly greater than the highest density of
obtained at
with ammonia. In situ resistivity measurements on the
ALD films grown using hydrazine at
obtained resistivities of
at
and
after annealing to
. The surface species and reaction products during the sequential exposures of TBTDET and hydrazine at
were examined using Fourier transform infrared spectroscopy and quadrupole mass spectrometry. These studies allowed a growth mechanism to be proposed for
ALD using TBTDET and hydrazine.