It is demonstrated that an oxide layer can be formed on the Equation or symbol description not availableGaAs surface using the photoelectrochemical (PEC) method when the pH value of the electrolyte solution of Equation or symbol description not availableHCl is Equation or symbol description not available∼3.5. To study the effect of thermal treatment on the resulted Equation or symbol description not availableGaAs oxide films, the as-grown samples were thermally treated at 200, 300, and Equation or symbol description not available400°C in Equation or symbol description not availableO2 ambiance for 10, 20, 30, and Equation or symbol description not available40min. The Auger electron spectroscopy measurement indicated that the resulted layers were composed of O, Ga, and As, and the elements ratio of Equation or symbol description not availableO∕(Ga+As) of the as-grown layer and the layers annealed at 200, 300, and Equation or symbol description not available400°C in Equation or symbol description not availableO2 ambience were 1.39, 1.43, 1.51, and 1.52, respectively, being close to the value for Equation or symbol description not availableGa2O3 and Equation or symbol description not availableAs2O3. The X-ray photoelectron spectroscopy analysis showed that the bonding structure in the layer is Equation or symbol description not availableGa–O or Equation or symbol description not availableAs–O. These results confirmed that the layer could be identified as Equation or symbol description not availableGa2O3 and Equation or symbol description not availableAs2O3, mainly the former. It is also demonstrated that when the oxide layers were thermally treated in Equation or symbol description not availableO2 ambiance, the Equation or symbol description not availableGaAs oxide films became denser, the microstructure of the oxide changed from an amorphous to a polycrystalline structure, and the surface roughness of the oxide layer also changed. It is expected that the oxide Equation or symbol description not availableGaAs layer grown by the PEC method would replace the externally deposited oxide layers to avoid the influence of surface contaminates and to be used as an insulating layer in various devices.