The electrocrystallization process of Bi–Te films deposited from Equation or symbol description not availableBi3+ and Equation or symbol description not availableHTeO2+ nitric acidic solution was studied with an emphasis on the impact of electrochemical conditions on film microstructure. Equation or symbol description not availableBi2Te3 films with a (110) preferential orientation and platelet grain morphology were obtained at the concentration of Equation or symbol description not available7.5mM Equation or symbol description not availableBi3+ and Equation or symbol description not available10mM Equation or symbol description not availableHTeO2+. The grain morphology changed from single- to multiorder platelets, and the texture decreased when the deposition potential became more negative. This phenomenon was explained by considering geometrical selection growth and Equation or symbol description not available{11¯010̱} Equation or symbol description not available⟨1¯105⟩ twinning of Equation or symbol description not availableBi2Te3 crystals. However, when the concentration ratio of Equation or symbol description not available[Bi3+] to Equation or symbol description not available[HTeO2+] was increased to 1.25, the film composition was changed to BiTe, and its preferential orientation was (014). The grain morphology changed from irregular polyhedron to spherulite, and the texture intensity decreased with more negative potentials.