Two different solder alloys, Equation or symbol description not availableSn–37Pb and Equation or symbol description not availableSn–4Ag–0.5Cu, were used to joint p- and n-type bismuth telluride-based thermoelements with copper. Equation or symbol description not availableSnTe and Equation or symbol description not availablePb1−xSnxTe were identified to be the major interfacial compounds for the Equation or symbol description not availableSn–Ag–Cu and Equation or symbol description not availableSn–Pb soldered junctions, respectively. The contact resistivity measured is around Equation or symbol description not available10−4to10−5Ωcm2, which depends on both the thickness and composition of interfacial compounds. The study shall lead to the effective strategy for choosing appropriate solder alloy systems to improve the contact property of bismuth telluride-based thermoelectric coolers.