In this article we discuss the synthesis of nanoparticles and the preparation of dense nanoceramics of Y-doped Equation or symbol description not availableCeO2. We prepared the nanoparticles by combustion synthesis and characterized the nanopowders by X-ray diffraction, scanning electron microscopy (SEM), and transmission electron microscopy. The good sintering properties of these nanopowders allowed us to obtain very dense ceramics of Y-doped Equation or symbol description not availableCeO2 (Equation or symbol description not available90% theoretical density) and keep the grain size small, in some cases around Equation or symbol description not available100nm, by using sintering temperatures as low as Equation or symbol description not available1250°C and very short annealing times between 5 and Equation or symbol description not available60min. The microstructure of these nanoceramics was analyzed by atomic force microscopy and SEM. The most interesting feature of these nanoceramics is that the electrical measurements in Equation or symbol description not availableN2 Equation or symbol description not available(pO2=3.5×10−6atm) carried out by the four-point dc technique showed a considerable increase in total conductivity in comparison with the measurements in air or oxygen in the range Equation or symbol description not available700–900°C. This conductivity enhancement might be associated with the electronic contribution to the total conductivity and it is clearly higher than the ionic conductivity in the same temperature range.