Abstract
A negative electrode consisting of Laves-phase alloy particles with a composition of
requires more than 20 activation cycles to attain a nominal discharge capacity (ca.
). The activation cycles could be reduced to several times only by mechanical modification with planetary ballmilling and further shortened by mechanochemical modification using a small amount of Al or Mg powder as a modifier. Such mechanical and mechanochemical modifications are also effective for improving high-rate dischargeability. The best result was obtained by grinding the Laves-phase alloy with
modifier for
at
. The reason for quick activation and improved high-rate dischargeability is discussed on the basis of electrochemical impedance, crystallographic structure, particle size, and specific surface area.
Access this article