Carbothermal reduction and nitridation method was used to prepare Equation or symbol description not availableCa-α-SiAlON:Eu2+ phosphor Equation or symbol description not available(Ca1−xEuxAl2Si10N16) from Equation or symbol description not availableCaCO3, Equation or symbol description not availableEu2O3, Equation or symbol description not availableAl2O3, and Equation or symbol description not availableSi3N4. The as-prepared samples were heated again at Equation or symbol description not available1600°C in a carbon-free atmosphere (high-purity Equation or symbol description not availableN2) to decrease the residual carbon content. The resulting Equation or symbol description not availableCa-α-SiAlON:Eu2+ phosphors with lowered carbon impurity showed the yellow emission band peaking at Equation or symbol description not available585–605nm as intensified 2–3 times more by the above heat-treatment. A white light-emitting diode (LED) with a Commission Internationale de l'Eclairage (CIE) chromaticity coordinate (Equation or symbol description not availablex=0.35, Equation or symbol description not availabley=0.32) was fabricated by using a blue LED chip Equation or symbol description not available(460nm) together with Equation or symbol description not availableCa-α-SiAlON:Eu2+ and Equation or symbol description not availableYAG:Ce3+ phosphors.