Etching kinetics for several silicon dioxide films in various hydrofluoric acid solutions have been studied. The low temperature silicon dioxide films were deposited at 450°C and 300 mTorr in Equation or symbol description not availableSiH4, Equation or symbol description not availableO2, and Equation or symbol description not availablePH3 and annealed at 950°C for 1 h. The thermal oxides were grown at 1100°C in Equation or symbol description not availableH2O and Equation or symbol description not availableO2. Four hydrofluoric acid solutions were used: dilutions of 49 weight percent Equation or symbol description not availableHF with deionized water, buffered hydrofluoric acid, surfactant‐buffered hydrofluoric acid, and hydrofluoric acid/hydrochloric acid mixtures. Expressions for etch rate as a function of hydrofluoric acid concentration are presented. Notably, the etching of the low temperature oxides was of the order 1.6–2.0 in Equation or symbol description not availableHF solutions and of the order 0.5–1.0 in buffered Equation or symbol description not availableHF solutions. The etching of the thermal oxide was of the order 1.37–1.5 in Equation or symbol description not availableHF and of the order 0.75–1.07 in buffered Equation or symbol description not availableHF solutions. The results for the Equation or symbol description not availableHF solutions provide evidence of a two‐part etching mechanism: first, the acidity causes the formation of the silanol bonds on the silicon dioxide surface and, then, the fluorine species react with the silicon to form Equation or symbol description not availableSiF4(g) which is soluble in water and forms Equation or symbol description not availableH2SiF6(aq). Significant enhancement (as much as 600%) in the etch rate was observed when hydrochloric acid was added to the Equation or symbol description not availableHF solutions.