The depth profile in nitrided Equation or symbol description not availableSiO2 films using Equation or symbol description not availableN2 remote radio frequency plasma was investigated. N was incorporated into the film at levels of up to 27 atom %, largely concentrated at the film surface, and not the film interface. The depth profiling data showed that the depth of incorporated N is dependant on film thickness, i.e., N is incorporated to a depth of about Equation or symbol description not available1.1nm in a Equation or symbol description not available1.5nm thick film, while the depth is significantly less to about Equation or symbol description not available0.7nm in the case of a Equation or symbol description not available4.0nm thick film. Moreover, under the same nitridation condition, more N content is concentrated nearer to the surface of a Equation or symbol description not available1.5nm thick oxide film than that of Equation or symbol description not available4.0nm thick film. Equation or symbol description not availableN2, generated in the molecule during the nitrogen process is almost completely concentrated at the film interface. After an additional annealing treatment, the molecular Equation or symbol description not availableN2 diffuses out extensively and N, which is chemically bonded to Equation or symbol description not availableSi3, is changed into a more stable state with different second-nearest neighbors, accompanied by reoxidation at the film interface of an ultrathin film.