A process was developed for low-temperature thermal chemical vapor deposition (CVD) of silicon dioxide Equation or symbol description not available(SiO2) in a single-wafer chamber utilizing disilane Equation or symbol description not available(Si2H6) and nitrous oxide Equation or symbol description not available(N2O) gaseous precursors. Deposition rate and refractive index (RI) were measured as a function of temperature, pressure, and gas flow rates. Additionally, film composition analysis and wet etch rates are provided. At Equation or symbol description not available550°C the deposition rate exceeds a Equation or symbol description not available700°C silane-based Equation or symbol description not available(SiH4) benchmark process. Deposition rates as high as Equation or symbol description not available90Å∕min were measured at Equation or symbol description not available470°C. It is proposed that Equation or symbol description not availableSi2H6 can be utilized in semiconductor manufacturing to achieve a lower thermal budget than existing Equation or symbol description not availableSiH4-based processes.