Single crystals of Equation or symbol description not availableCdF2 doubly doped with Equation or symbol description not availableYbF3 and Equation or symbol description not availableErF3 efficiently convert infrared radiation (∼0.93 μm) from a Equation or symbol description not availableSi:GaAs diode to red and green light. By varying the Yb concentration, phosphors have been made which produce a red or green visual response. For the series of crystal samples ofEquation or symbol description not availableCdF2:1%ErF3:1–10%YbF3 studied: at Equation or symbol description not availableYbF3 concentrations below 3%, only red Er3+ emission peaks were observed (6450–6800Å); at 3% Equation or symbol description not availableYbF3, red and green spectra (5300–5700Å) were observed, the green bands being much less intense; the most intense phosphor contained 10 mole percent (m/o) Yb3+, and the green intensity was an order of magnitude higher than the red. Charge compensation by Equation or symbol description not availableNaF of the rare earth ions in Equation or symbol description not availableCdF2:1%ErF3:10%YbF3greatly reduces the intensity of emission bands, as well as the intensity of the absorption band at 976 nm, in agreement with previous studies of the absorption spectra properties of the Equation or symbol description not availableYbF3:CdF2 system (1). Recent results of 19F NMR of single crystals of Equation or symbol description not availableCdF2 containing high concentrations of Equation or symbol description not availableYbF3 andEquation or symbol description not availableErF3, respectively, indicate that most of the rare earth ions and their associated interstitial fluorides are found in Equation or symbol description not available(M3+‐F−)2 dimers in the crystal (2). The intense absorption band observed at 976 nm in Yb3+‐doped Equation or symbol description not availableCdF2 can be assigned to this dimer, which is destroyed by the use of Na+ as a charge compensator in place of interstitial fluoride, the native charge compensating defect. Similarly, as the accepted mechanism of the infrared‐to‐visible conversion in the Yb3+ sensitized Er3+ activated systems involves the transfer of two infrared photons from Yb3+ to Er3+, phosphor emission by diode excitation will decrease when the Equation or symbol description not available(M3+‐F−)2 complex is destroyed by Equation or symbol description not availableNaFsubstitution. The 976 nm strong absorption band was also observed in samples (10% Yb, 1% Er) prepared with Equation or symbol description not available1–50 m/o of CaF2 substituted for Equation or symbol description not availableCdF2without appreciable decrease in the intensity; however the emission intensities of both green and red bands were significantly enhanced for all of the samples codoped with Equation or symbol description not availableCaF2. There appears to be a plateau for the compositions 1.5–3%Equation or symbol description not availableCaF2 and a decrease in the 4.5 and 10% Equation or symbol description not availableCaF2 samples. Of all the materials investigated to date, Equation or symbol description not availableYF3 and Equation or symbol description not availableBaYF5 codoped with Yb3+ and Er3+ are reported to be the most efficient upconverting systems with a quantum efficiency between 10−4 and 10−3 Equation or symbol description not available(λ=0.97 μm). The quantum efficiency of Equation or symbol description not availableCdF2:10%YbF3:1%ErF3 is found to be 0.23% and that of Equation or symbol description not availableCdF2:10%YbF3:1%ErF3:2.5%CaF2, 0.70%. These values were obtained under intense excitation with a Equation or symbol description not availableGaAsdiode. Lower values might be found at lower excitation densities.