The preparation of Equation or symbol description not availableY2O2S:Eu phosphor in sodium‐sulfide flux was studied as a means of obtaining different particle sizes (3–50 μm). Atmospheric control is absolutely necessary above 1050°C to prevent oxidation of both Equation or symbol description not availableY2O2Sand the flux. It is found that the particle size distribution of the raw materialEquation or symbol description not available(Y2O3) is reproduced in the starting particle of growth Equation or symbol description not availableY2O2S. The growth rate of small and nonaggregated single crystals of Equation or symbol description not availableY2O2S:Eu can be expressed by the equation, Equation or symbol description not availabledφ/dt=Aexp(−ΔE/kT).