The properties of phosphorus‐doped molybdenum silicide as a gate electrode, interconnecting material, and impurity diffusion source for LSI's have been studied. The phosphorus‐doped molybdenum silicide films were deposited by co‐sputtering using specially designed Mo and Si targets in a Equation or symbol description not availablePH3/Aratmosphere. Equation or symbol description not availablePH3 decomposed to P and Equation or symbol description not availableH2 during sputtering and the phosphorus combined with Mo and Si. Typically, a phosphorus concentration ofEquation or symbol description not available1.5×1021 cm−3 in the films was used. As‐deposited films Equation or symbol description not available(Mo/Si≤0.5)had amorphous structure and high resistivity. After the films were annealed at temperatures above 800°C, they became polycrystalline and resistivity was decreased. The resistivity of the film with a Mo/Si ratio of 2 to 1 wasEquation or symbol description not available7.5×10−5 Ω‐cm with annealing at 1000°C in Equation or symbol description not availableN2. Phosphorus was able to diffuse from the doped molybdenum silicide films to the Si substrate during annealing in Equation or symbol description not availableO2. After high temperature annealing up to 1100°C, the contact resistance between the molybdenum silicide and the silicon substrate was below Equation or symbol description not available2×10−6 Ω‐cm2. The reliability of doped molybdenum silicide gate MOSFET's is as good as polysilicon gates and the threshold voltage shift is within ±20 mV under stress conditions of 2.5 MV/cm for 1000 hr at 150°C.