Abstract
Composition profiles of the boron distribution in borosilicate glasses are shown to be dependent on the mode of sample preparation. Surfaces prepared for analysis by either abrasive polishing or saw cutting exhibit a boron gradient, the boron concentration increasing gradually to a constant level at 1–2 μm, Conversely, profiles for surfaces prepared by impact fracture show no significant change with depth.