The continued need for reliability and quality is inherent in the building of semiconductor devices. Control and reproducibility of the breakdown strength and threshold voltage of the gate oxide insulator is a basic and necessary condition for achieving these results. Alkali ions have been found to be a major cause of surface potential instabilities, and the removal of these mobile ion species is very important in the building of strong silicon dioxide insulators. Equation or symbol description not availableHCl in particular has been found to be an effective gettering agent when used in small percentages during a thermally grown oxidation process. Further work has been done on the treatment of oxides with a high temperature anneal step using small percentages of Equation or symbol description not availableHCl andEquation or symbol description not availableO2 after an initial oxide has been grown. This leads to the two‐step Equation or symbol description not availableHCl treatment or dual Equation or symbol description not availableHCl cycle. Using the dual Equation or symbol description not availableHCl cycle a 56% increase in electric field breakdown has been achieved over a standard one‐step oxidation cycle in rupturing the thin oxide under a 20,000 square mil capacitor. Decreased defect density seen on large capacitors will result in a significant improvement in VLSI manufacturing.