The electrochemical reduction of molten Equation or symbol description not availableLiNO3 on platinum or nickel electrodes produces insoluble Equation or symbol description not availableLi2O that passivates the cathode at high current densities. The presence of small amounts of silver ions prevents this passivation by undergoing reduction to silver metal in the form of dendritic deposits that increase the effective area of the electrode. The deposited silver is unstable in molten Equation or symbol description not availableLiNO3 and reacts with the melt to regenerate silver ions. Corrosion studies of silver coupons gave a weight loss rate of 280 μg h−1cm−2 in molten Equation or symbol description not availableLiNO3 at 350°C, but of only 5 μg h−1cm−2 in Equation or symbol description not availableKNO3 at 375°C. The presence of water in the Equation or symbol description not availableLiNO3 melt increases the corrosion rate of silver. Additions of Equation or symbol description not availableLi2O, Equation or symbol description not availableLiNO2, Equation or symbol description not availableLiCl, orEquation or symbol description not availableAgNO3 to molten Equation or symbol description not availableLiNO3 significantly decreases the corrosion rate. The addition of oxide ions to a Equation or symbol description not availableAgNO3 containing melt produces a dark precipitate of Equation or symbol description not availableAg2O in Equation or symbol description not availableNaNO3 or Equation or symbol description not availableKNO3, but not in Equation or symbol description not availableLiNO3. The decomposition reaction of Equation or symbol description not availableAg2O into its elements is kinetically slow in molten nitrates with a rate similar to that observed in air.