Abstract
Passive films formed under strictly controlled conditions during anodic polarization of iron in borate buffer solution were reduced in the same solution with a constant cathodic current. The cathodic charge consumed for the reduction of passive film was greater than the theoretical value calculated under the assumption that
was reduced to Fe2+. The higher the oxidation potential was and the longer oxidation time was employed, the greater was the consumed charge found experimentally. At certain characteristic thicknesses of the passive film associated with changes in film growth during its formation, inflections of the
vs. time and
vs. film thickness were observed.