The effects of current density (54–865 mA/cm2), temperature (330°–355°C), and discharge depth (Equation or symbol description not availableNa2S3 to Equation or symbol description not availableNa2S2.4) on sodium‐sulfur cell efficiency, resistance, capacity, and longevity are presented. Equal discharge and charge cycle times obtained on 16 Ah laboratory cells at 865 mA/cm2 and 335°C demonstrated the resistive layer effectiveness in preventing sulfur passivation of the beta″‐alumina electrolyte surface during cell charging. Elevated temperatures increased cell efficiency ∼3%/10°C, decreased resistance, and increased capacity. A group of cells operating at 216 mA/cm2, twice the standard current density, and 330°C have obtained ∼700 cycles, ∼900 Ah/cm2, with little performance deterioration. The cells are ∼82% efficient and display ∼80% of theoretical capacity. Alternating current resistance analysis of typical laboratory cells revealed an increase in discharge resistance occurred when cells were cycled between Equation or symbol description not availableNa2S3 and Equation or symbol description not availableNa2S2. Correlations with the sodium‐sulfur phase diagram indicate the resistance rise was due to precipitation of Equation or symbol description not availableNa2S2. Upon subsequent charge inception, the ac resistance dropped. However, an increased two‐phase charge resistance was recorded. This suggested that Equation or symbol description not availableNa2S2 deposition occurred at the resistive‐mat/conductive‐mat interface.