Layers of mixed platinum and silicon were formed on p+‐n junction silicon single crystal wafers (hereafter abbreviated as p+n‐Si) by depositing Pt on the p+‐Si surface, followed by heating at 320°–350°C. ESCA studies showed that Pt silicide (Equation or symbol description not availablePtSi, or in some cases a mixture of Equation or symbol description not availablePtSi and Equation or symbol description not availablePt2Si) was formed when a 3–5 nm‐thick Pt layer on Si was heated, whereas a nonstoichiometric, Si‐rich Pt‐Si intermixed layer was formed when an ultrathin Pt layer (1.0 nm thick) on Si was heated. It was also confirmed that, in the former case, a majority of the deposited Pt remained in the form of pure metal when Pt‐deposited silicon was exposed to air for ca. one day before heating. The p+n‐Si photoanode covered with Pt silicide gave photocurrent‐voltage characteristics nearly the same as the previously reported Pt‐coated p+n‐Si photoanode in a hydrogen iodide/iodine solution, indicating that Pt silicide formation does not affect the photovoltage at the p+‐n junction. The photocurrent of ca. 14 mAcm−2 at the maximum power point was maintained for 400h under continued illumination and only slightly reduced after 4500h (∼6.3 months). The p+n‐Si electrode covered with the Pt‐Si intermixed layer gave a short‐circuit photocurrent higher than that covered with Pt silicide by virtue of the higher light transmittance in the layer, but was somewhat inferior in photocurrent stability. ESCA studies of the electrodes after long‐term stability tests revealed that some platinum was lost in the outermost layer, suggesting that the decay of the fill factor is mainly due to the chemical change at the top surface in both the case of Pt silicide and of the Pt‐Si intermixed layer.