The etch rate of a solid‐excitation‐based photochemical etching process for semiconductor materials is determined by the balance between recombination of photogenerated carriers and carrier participation in the surface etching reaction. Ion implantation‐induced damage of the semiconductor can shift the balance between recombination and reaction, permitting selective etching of undamaged regions of a semiconductor surface relative to ion‐implanted, damaged regions. Spatially selective photochemical dry etching of Equation or symbol description not availablen‐GaAs has been achieved by this approach.