We develop a new photoresist etch mask process to etch (001) Equation or symbol description not availableInP wafers to obtain (111) B‐faceted v‐grooves for channeled substrate laser applications. We investigate the use of Equation or symbol description not availableHCl and Equation or symbol description not availableHF solutions to remove native oxide layers prior to v‐groove etching. We also study the relationship between the photoresist mask undercutting and the bath temperature used for native oxide removal. The degree of undercutting in photoresist mask can be reduced about two times by increasing the Equation or symbol description not availableHF bath temperature from room temperature to 48°C during the oxide removal process. We also identify two important factors that control the mask undercutting rates as (i) the thickness of native oxide on Equation or symbol description not availableInP surface and (ii) the chemical reaction between Equation or symbol description not availableInP and the oxide removal bath solution.