Degradation reactions of a nylon 6 battery separator material have been studied in 4–34% aqueous Equation or symbol description not availableKOH electrolytes at 35°–110°C. In a Ni/Cd cell, this degradation involves a slow hydrolysis reaction followed by fast electrochemical oxidations of the hydrolysis reaction products. Arrhenius activation energy of the hydrolysis reaction in 34% Equation or symbol description not availableKOH was Equation or symbol description not available20.0±0.3 kcal/mole. A plot of the hydrolysis rate at 100°C vs. hydroxyl ion concentration gave a rate maximum at about 16% Equation or symbol description not availableKOH, and the mechanism for this effect is discussed. Electrochemical oxidations of the hydrolysis product, 6‐aminocaproate ion, appear to proceed rapidly in several sequential steps at a nickel oxide electrode. In a Ni/Cd cell, the combination of nylon separator hydrolysis followed by electrochemical oxidation of the products can seriously degrade the battery life‐time. The rate of the hydrolysis of nylon 66 separator material was approximately one half of that of the nylon 6 material.