Thin films of porous alumina were formed from an alumina sol which was cured at 500°C in either air or oxygen. We have determined, from a simple RBS marker experiment, that alumina films made from this sol have a volume porosity of about 50%, which is substantially different from bulk structures formed from this material. Ellipsometric measurements were also carried out to determine the porosity of these films. Our analysis shows an excellent agreement between the two measurements. No change in film porosity was found to occur after annealing at 900°C for 60 min in oxygen.