The characteristics of Equation or symbol description not availableCF4/O2 plasmas which are used to etch composite layers of sacrificial photoresist and underlyingEquation or symbol description not availableSiO2 have been examined with experimental design and modeled empirically by response‐surface methodology using a Lam Research Autoetch 480 single‐wafer system. The effects of variations of process gas flow rates for Equation or symbol description not availableCF4 (150–200 sccm) and Equation or symbol description not availableO2 (0–50 sccm), reactor pressure (900–2000 mtorr), and interelectrode spacing (4–6 mm) on the etch rates of Equation or symbol description not availableSiO2 and photoresist were explored at fixed radio frequency power (500W at 13.56 MHz) at Equation or symbol description not available22°±2°C. Variation in spacing shows different effects for these two materials; whereas the Equation or symbol description not availableSiO2 etch rates generally increase with increasing spacing as the other parameters are varied, the photoresist etch rates exhibit more complex behavior. At the lower spacing of 4 mm, neither film has a measurable etch rate for low settings of the other variables. The Equation or symbol description not availableSiO2 etch rates are virtually constant with increasing Equation or symbol description not availableO2 flow rate for low, middle, and high settings of the other variables. At low settings of the other variables, the photoresist etch rates are zero over the range of Equation or symbol description not availableO2 flow rates but increase with increasing Equation or symbol description not availableO2 flow rates for middle and high settings of the other variables. At a spacing of 4 mm, the etch rates of both films are negligible over the range of Equation or symbol description not availableCF4 flow rates and the range of reactor pressure. At larger spacings the etch rates of photoresist increase with increasing Equation or symbol description not availableCF4 flow rate, while the etch rates of Equation or symbol description not availableSiO2 are similar for middle and high settings of the other variables over the range of Equation or symbol description not availableCF4 flow rates. Process optimization using the empirical models to attain suitable etch rates for both films for planarization of a composite layer of photoresist and Equation or symbol description not availableSiO2 with high etch uniformity was achieved at 500W of RF power, 1450 mtorr, 150 sccm of Equation or symbol description not availableCF4, 0 sccm Equation or symbol description not availableO2, and a spacing of 5.5 mm. Hence, for a Equation or symbol description not availableCF4 plasma with this reactor adequate planarization is obtained without the use of Equation or symbol description not availableO2. The addition of small concentrations of Equation or symbol description not availableO2 to a Equation or symbol description not availableCF4 plasma resulted in increasingly higher etch rates for photoresist as the process progressed.