Si wafers covered with a sublimed Equation or symbol description not availableC60 layer have been directly bonded to bare or oxidized Si wafers at room temperature via Van der Waals attraction forces. The interface energies of the bonded pairs increase during storage in air at room temperature and approach saturated values after ∼200 h. The typical saturated interface energy of Equation or symbol description not availableC60/SiO2 (∼40 erg/cm2) is higher than that of Equation or symbol description not availableC60/Si (20–30 erg/cm2). Other material combinations having a Equation or symbol description not availableC60 buried layer may also be realized by wafer bonding for specific applications.