Abstract
The oxidation of In‐48Sn was investigated at partial pressures between 10−8 and 10+4 Pa over the temperature range from 22 to 250°C with different analytical methods. The oxide film contains a mixture of several oxides, although indium oxide forms preferentially. The measurements show at the surface an excess of indium compared to the eutectic composition. Below the melting point, a logarithmic growth, and above this point, a parabolic growth of the oxide film was observed. The oxide film formed in air at 250°C does not exceed about 50 nm in the first 5 min of oxidation.