A new range of stable γ solid solutions has been found in the system Equation or symbol description not availableLi4SiO4‐Li3CrO4, of formula Equation or symbol description not availableLi3+xSixCr1−xO4:0.3< x<0.65. For compositions, Equation or symbol description not available0<x≤0.4, a range of solid solutions based on Equation or symbol description not availableβ‐Li3CrO4 also forms. At low Equation or symbol description not availablex,≤∼0.5, the solid solutions are predominantly electronic conductors but with increasing Equation or symbol description not availablex, the level of electronic conductivity decreases giving rise to materials that are either mixed conductors or ionic conductors, depending on composition. Thus, compositionEquation or symbol description not availablex=0.7 has good Li+ conductivity, Equation or symbol description not available1.7×10−6 Ω −1 cm−1 at 25°C where Equation or symbol description not availablex=0.5 is primarily an electronic conductor, Equation or symbol description not available2.3×10−5 Ω−1 cm−1 at 25°C. These materials provide the first example of mixed conduction in the LISICON‐related γ solid solution family. A new qualitative method for investigating transport numbers in mixed Equation or symbol description not availableLi+/e− conductors is proposed: dc polarization measurements are made using pelleted samples with Au electrodes and the amount of charge stored as a consequence of electrochemical decomposition of the pellet is estimated; results obtained from such charge/discharge experiments corroborate those obtained by low frequency ac impedance studies. Samples which are primarily electronic conductors give rise to significant Schottky barrier impedances at the sample‐electrode interface. These effects are also investigated by ac impedance by varying the nature of the electrode materials: In/Ga or Au.