The electrical conductivity of Equation or symbol description not availableSrTiO3 as a function of Equation or symbol description not availablepO2 was investigated in the two gaseous systems Equation or symbol description not availableH2–O2 and Equation or symbol description not availableCO–O2. The experimental results showed different conductivity values for these two different systems. The oxygen partial pressure was, therefore, checked carefully and it turned out that the control of Equation or symbol description not availablepO2 at reducing conditions is complicated by disequilibrium states when using Equation or symbol description not availableCO–CO2–O2 gas mixtures. A sample and an oxygen sensor that are positioned side by side may be exposed to Equation or symbol description not availablepO2 values that differ by up to 2 log units because of their different catalytic behavior with respect to the oxidation of CO. At intermediate Equation or symbol description not availablepO2 conditions, e.g., between Equation or symbol description not available10−5 and Equation or symbol description not available10−13bar at Equation or symbol description not availableT=973K, low concentrations of Equation or symbol description not availableH2 (CO) and Equation or symbol description not availableO2 may result in Equation or symbol description not availablepO2 gradients of up to 10 log units per centimeter in both Equation or symbol description not availableH2–O2 and Equation or symbol description not availableCO–O2 systems.