The anodic formation of self-organized porous Equation or symbol description not availableTiO2 on titanium was investigated in 1 M Equation or symbol description not available(NH4)2SO4 electrolytes containing 0.5 wt % Equation or symbol description not availableNH4F by potential sweeps to Equation or symbol description not available20VSCE. By a combination of electrochemical, morphological, and compositional information we show that the sweep rate has a significant influence on the initiation and growth of the porous structures. In the first phase of the anodization process, a precursor barrier type of oxide film is formed; underneath this film pores then start growing first randomly and then self-organize. High-aspect-ratio Equation or symbol description not availableTiO2 nanostructures can be obtained under optimized electrochemical conditions. These nanotubular oxide layers have single-pore diameter ranging from 90 to 110 nm, average spacing of 150 nm, and porosity in the order of 37–42%. The current work indicates that the nature of the initial barrier-type layer has a strong influence on establishing optimized pore growth conditions.