In this paper, we investigate the transformation of Equation or symbol description not availableTiSi2 from the high-resistivity C40 phase to the low-resistivity C54 phase. In particular, the effect of C40 film thickness on the transition temperature, which has not been studied in the literature, is scrutinized. Two types of laser, i.e., Equation or symbol description not availableNd:YAG (yttrium aluminum garnet) and excimer laser, were used to induce C40 Equation or symbol description not availableTiSi2 on samples of 350 Å of Ti deposited on (100) Si substrates. It was also found that the thicker C40 Equation or symbol description not availableTiSi2 (40 nm) induced by the Equation or symbol description not availableNd:YAG laser required a very high temperature of more than 1000°C and an activation energy of 6.5 eV for the formation of the stable C54 Equation or symbol description not availableTiSi2, whereas a thinner C40 Equation or symbol description not availableTiSi2 (15 nm) produced by the excimer laser required a low temperature of 700°C and an activation energy of 2.5 eV to transform into C54 Equation or symbol description not availableTiSi2. The much lower transition temperature for the thin samples is attributed to the compressive strain in these samples.