The oxidation of Si(100) in Equation or symbol description not availableN2O has been studied at temperatures in the range from 950 to 1200°C using secondary ion mass spectroscopy, Auger electron spectroscopy, and x‐ray photoelectron spectroscopy. During oxidation N became incorporated into the oxide film, the amount increasing with increasing temperature to 1100°C and then falling to a lower value at 1200°C. The N was concentrated as a thin N‐rich layer near the Equation or symbol description not availableSiO2‐Si interface inhibiting the influx of oxidant, leading to a reduction in the extent of oxidation compared with that in pure Equation or symbol description not availableO2. The oxidant species is believed to be NO, which is stable under the conditions of the experiments. The N‐rich phase was shown to have a composition of Equation or symbol description not availableSi3N4 surmounted by N‐rich oxynitride.